journal article·2025-08Open access

Evaluation of 1.5 mol% yttria – 1.5 mol% gadolinia stabilized tetragonal zirconia polycrystals derived from solid state synthesis and laser vaporation

Bettina Osswald, Lenka Müller, Janet Grabow, Frank A. Müller, Frank Kern

Abstract

Variation of stabilizer composition and amount offers the opportunity to tailor the mechanical properties of tetragonal zirconia polycrystals. In this study, zirconia stabilized with 1.5 mol% yttria and 1.5 mol% gadolinia was prepared by co-milling zirconia with yttria and gadolinia stabilizer oxides. A laser vaporized powder was derived from this starting powder. The two powders were subsequently consolidated into bulk ceramics by hot pressing at 1300–1450 °C sintering temperature and 60 MPa pressure. Tetragonal zirconia polycrystals obtained from the different powder technology processes differ considerably in phase composition, microstructure and mechanical properties. The laser vaporized derived materials are predominantly tetragonal, hard and combine high strength with a moderate toughness. The solid state synthesized materials show a transition to higher hardness and strength and lower fracture resistance with increasing sintering temperature, which can be correlated to the changes in phase composition and microstructure. • Synthesis route of YGd-TZP powder affects mechanical properties and microstructure
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Nuclear materials and radiation effects

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. Transformation toughening in zirconia-containing ceramics10.1111/j.1151-2916.2000.tb01221.x ↗
2. Stabilized zirconia as a structural ceramic: an overview10.1016/j.dental.2007.05.005 ↗
3. The mechanics of transformation toughening10.1098/rspa.1987.0084 ↗
4. Transformation toughening: Part 3 experimental observations in the ZrO2- Y203 system10.1007/BF00809059 ↗
5. Effect of heat treatment on grain size, phase assemblage, and mechanical properties of 3 mol% Y-TZP10.1111/j.1151-2916.1996.tb08980.x ↗
6. Compositional effects in nanostructured Yttria partially stabilized Zirconia10.1111/j.1744-7402.2010.02503.x ↗
7. Coprecipitation conditions and compaction behaviour of Y-TZP nanometric powders10.1016/0272-8842(94)90063-9 ↗
8. Phase-transformation and grain-growth kinetics in yttria-stabilized tetragonal zirconia polycrystal doped with a small amount of alumina10.1016/j.jeurceramsoc.2010.01.007 ↗
9. F. Lair, Critical effect of cubic phase on aging in 3mol% yttria-stabilized zirconia ceramics for hip replacement prosthesis10.1016/j.biomaterials.2004.01.002 ↗
10. Grain growth in ultrafine-grained Y-TZP ceramics10.1016/S0955-2219(96)00217-8 ↗
11. Hydrothermal synthesis of precursors for Y-TZP/α-Al2O3 composite10.1016/j.powtec.2004.09.012 ↗
12. Morphology and composition of spray-flame-made yttria-stabilized zirconia nanoparticles10.1088/0957-4484/16/7/039 ↗
13. Calado, J., Dos Santos, E., Nanocrystaline spherical ceramic oxides, process for the synthesis and use thereof. (2009) US patent 9249020 B2.
14. Preparation of Y2O3-coated ZrO2 powder by suspension drying10.1023/A:1006714032131 ↗
15. Evidence of phase transitions and their role in the transient behavior of mechanical properties and low temperature degradation of 3Y-TZP made from stabilizer-coated powder10.3390/ceramics2020022 ↗
16. Preparation of ceramic nanospheres by CO2 laser vaporization (LAVA)10.1016/j.jeurceramsoc.2011.01.010 ↗
17. Synthesis of ceramic nanoparticles by laser vaporization (LAVA)
18. Synthesis of Eu-doped SrAl2O4 nanophosphors by CO2 laser vaporization10.1016/j.actamat.2013.08.010 ↗
19. Preparation of SrTiO3 nanocubes by CO2 laser vaporization (LAVA) and hydrothermal maturation10.1039/D1NA00685A ↗
20. Gas phase condensation of superparamagnetic iron oxide-silica nanoparticles--control of the intraparticle phase distribution10.1039/C5NR00845J ↗
21. New ZrO2/Al2O3 nanocomposite fabricated from hybrid nanoparticles prepared by CO2 laser co-vaporization10.1038/srep20589 ↗
22. Microstructure, mechanical properties and low temperature degradation resistance of 2Y-TZP ceramic materials derived from nanopowders prepared by laser vaporization10.1016/j.jeurceramsoc.2015.03.006 ↗
23. Correlation of mechanical properties and composition in tetragonal CeO2-Y2O3-ZrO2 ceramic system10.1016/S0254-0584(02)00328-0 ↗
24. Phase stability of fine-grained (Mg,Y)-PSZ10.1111/j.1151-2916.1995.tb08928.x ↗
25. Preparation and conductivity of Yb2O3–Y2O3 and Gd2O3–Y2O3 co-doped zirconia ceramics10.1016/j.ssi.2008.03.003 ↗
26. Phase diagrams and thermodynamics of rare-earth-doped zirconia ceramics10.1351/pac200779101731 ↗
27. Pressureless sintering of yttria-gadolinia co-stabilized zirconia10.1016/j.jeurceramsoc.2022.08.046 ↗
28. Calibration curve for quantitative analysis of the monoclinic-tetragonal ZrO2 system by X-ray diffraction10.1111/j.1151-2916.1984.tb19614.x ↗
29. Mechanical properties of ytterbia stabilized zirconia ceramics (Yb-TZP) fabricated from powders prepared by co-precipitation method10.1016/S0272-8842(99)00042-5 ↗
30. Average grain size in polycrystalline ceramics10.1111/j.1151-2916.1969.tb11975.x ↗
31. A critical evaluation of indentation techniques for measuring fracture toughness: II, strength method10.1111/j.1151-2916.1981.tb10321.x ↗
32. Indentation studies on Y2O3-stabilized ZrO2: II, Toughness determination from stable growth of indentation-induced cracks10.1111/j.1151-2916.1994.tb05392.x ↗
33. A fracture mechanics analysis of indentation-induced Palmqvist crack in ceramics10.1007/BF00725625 ↗
34. Phase relationships in the zirconia-yttria system10.1007/BF01031853 ↗
35. Mechanical behaviour of extremely tough TZP bioceramics10.1016/j.jmbbm.2018.11.001 ↗
36. Ytterbia – praseodymia co-stabilized TZP with high toughness and transformation limited strength
37. New Y-TZP powders for medical grade zirconia10.1023/A:1018562917779 ↗