journal article·2026-01Open access

Subcritical crack growth in cold sintered ZnO ceramics

Abdullah Jabr, Peter Supancic, Raul Bermejo

Abstract

The long-term mechanical reliability of ceramic components is often compromised by the subcritical growth of defects (SCCG), especially under high relative humidity environments. In this study, structural degradation associated with SCCG is investigated for the first time in cold sintered ZnO and compared to counterparts of same density sintered at 1000°C. Constant stress rate experiments ranging between 0.001 MPa/s and 1000 MPa/s are performed in air and water for both samples. While both cold sintered and conventionally sintered ZnO ceramics are susceptible to SCCG in the same manner, the former exhibit a distinct threshold behaviour up to relatively high stress intensity levels (ca. 0.7 ∙ K Ic ). The effect of the nanoscale grain size and potential chemical effects associated with the cold sintering process on SCCG are discussed. The findings are supported by constant stress experiments and fractographic analyses, providing valuable insights for the mechanical design and lifetime assessment of cold sintered components.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Powder Metallurgy Techniques and Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (51)

Show source-provided references
1. M.N. Rahaman, Sintering of Ceramics, Taylor & Francis, 2008.10.1201/b15869 ↗
2. Fundamental aspects of hot isostatic pressing: an overview10.1007/s11661-000-0078-2 ↗
3. Field-assisted sintering technology/spark plasma sintering: mechanisms, materials, and technology developments10.1002/adem.201300409 ↗
4. Review: liquid phase sintering10.1007/s10853-008-3008-0 ↗
5. A review of ceramic sintering and suggestions on reducing sintering temperatures10.1023/A:1008621020555 ↗
6. Hydrothermal-assisted cold sintering process: a new guidance for low-temperature ceramic sintering10.1021/acsami.6b07481 ↗
7. Protocol for ultralow-temperature ceramic sintering: an integration of nanotechnology and the cold sintering process10.1021/acsnano.6b03800 ↗
8. A route towards fabrication of functional Ceramic/Polymer nanocomposite devices using the cold sintering process10.1021/acsaelm.0c00225 ↗
9. Fabrication of bimorph lead zirconate titanate thick films on metal substrates via the cold sintering-assisted process10.1016/j.actamat.2020.05.053 ↗
10. Sodium molybdate-hexagonal boron nitride composites enabled by cold sintering for microwave dielectric substrates10.1111/jace.19254 ↗
11. Using percolation to design ZnO composites with hBN modified grain boundaries to obtain varistor-like behavior
12. Enhanced high permittivity BaTiO 3 –polymer nanocomposites from the cold sintering process10.1063/5.0021040 ↗
13. Preparation of zinc oxide/poly-ether-ether-ketone (PEEK) composites via the cold sintering process10.1016/j.actamat.2021.117036 ↗
14. Highly reliable BaTiO3 -Polyphenylene oxide nanocomposite dielectrics via cold sintering10.1002/admi.202100963 ↗
15. Mechanical strength of cold-sintered zinc oxide under biaxial bending10.1007/s10853-018-3173-8 ↗
16. The effect of liquid phase chemistry on the densification and strength of cold sintered ZnO10.1016/j.jeurceramsoc.2022.11.071 ↗
17. Scaling up the cold sintering process of ceramics10.1016/j.jeurceramsoc.2023.04.061 ↗
18. Understanding the lower fracture resistance of cold sintered ceramics10.1016/j.jeurceramsoc.2024.116968 ↗
19. Nanocrystalline-Matrix ceramic composites for improved fracture toughness10.1557/mrs2004.12 ↗
20. Subcritical crack growth in ceramics
21. B. Lawn, Fracture of Brittle Solids, 2nd ed., Cambridge University Press, Cambridge, 1993. https://doi.org/10.1017/CBO9780511623127.10.1017/CBO9780511623127 ↗
22. Slow crack growth in brittle materials under dynamic loading conditions10.1007/BF00113930 ↗
23. Subcritical crack growth in low temperature Co-fired ceramics under biaxial loading10.1016/j.engfracmech.2012.12.004 ↗
24. Sub-Critical crack growth in alumina – a comparison of different measurement and evaluation methods10.1007/s00501-011-0035-y ↗
25. The phenomena of rupture and flow in solids10.1098/rsta.1921.0006 ↗
26. Tada · 2000
27. Ceramics: mechanical properties, failure behaviour
28. Morphological and chemical evolution of transient interfaces during zinc oxide cold sintering process
29. Room temperature ZnO ageing after cold sintering process: grain boundaries evolution characterization by in situ electrochemical impedance spectroscopy10.1016/j.jeurceramsoc.2024.02.014 ↗
30. The ball on three balls test for strength testing of brittle discs: stress distribution in the disc10.1016/S0955-2219(01)00458-7 ↗
31. The Ball-on-Three-Balls strength test for discs and plates: extending and simplifying stress evaluation10.1016/j.jeurceramsoc.2022.09.047 ↗
32. Mechanical properties and microstructure of zinc oxide varistor ceramics10.4028/www.scientific.net/MSF.530-531.408 ↗
33. Subcritical crack growth in multilayer low temperature Co-fired ceramics designed with surface compressive stresses10.1016/j.jeurceramsoc.2016.07.003 ↗
34. Effects of stress rate and calculation method on subcritical crack growth parameters deduced from constant stress-rate flexural testing10.1016/j.dental.2010.11.016 ↗
35. ASTM C1368-06, Standard Test Method for Determination of Slow Crack Growth Parameters of Advanced Ceramics by Constant Stress-Rate Flexural Testing at Ambient Temperature, (2008).
36. Subcritical crack propagation in 3Y-TZP ceramics: static and cyclic fatigue10.1111/j.1151-2916.1999.tb02213.x ↗
37. Analysis of subcritical crack growth in dental ceramics using fracture mechanics and fractography10.1016/j.dental.2007.08.001 ↗
38. Influence of the scatter of strength and of measurement uncertainties on the determination of the subcritical crack growth exponent in ceramics and glasses10.1016/j.jeurceramsoc.2016.11.043 ↗
39. Subcritical crack growth in Al2O3 with submicron grain size10.1016/S0955-2219(02)00072-9 ↗
40. Crack velocity functions and thresholds in brittle solids10.1016/0955-2219(90)90053-I ↗
41. Threshold intensity factors as lower boundaries for crack propagation in ceramics10.1186/1475-925X-3-41 ↗
42. Microcantilever investigation of slow crack growth and crack healing in aluminium oxide10.1016/j.actamat.2024.119914 ↗
43. Crack propagation and fatigue in zirconia-based composites10.1016/S1359-835X(98)00145-6 ↗
44. Jr., environmentally enhanced fracture of glass: a historical perspective10.1111/j.1551-2916.2009.03097.x ↗
45. Effect of surface stress on stress corrosion of silicate glass
46. Fracture toughness by the surface crack in flexure (SCF) method10.1002/9780470314555.ch29 ↗
47. J.J. Swab, G.D. Quinn, Effect of Precrack “Halos” on KIc Determined by the Surface Crack in Flexure Method, Defense Technical Information Center, Fort Belvoir, VA, 1997. https://doi.org/10.21236/ADA335068.10.21236/ADA335068 ↗
48. Intricacies involving the evaluation of fracture toughness obtained by the surface-crack-in-flexure method10.1111/jace.18667 ↗
49. R. Morrell, Fractography of brittle materials, National Physical Laboratory, Teddington, 2008. 〈http://eprintspublications.npl.co.uk/1571/〉.
50. G.D. Quinn, NIST Recommended Practice Guide Fractography of Ceramics and Glasses, National Institute of Standards and Technology, 2016. https://doi.org/10.6028/NIST.SP.960-16e2.10.6028/NIST.SP.960-16e2 ↗
51. Fracture of ceramics10.1002/adem.200700347 ↗