Corrosion of silicon nitride materials in acidic and basic solutions and under hydrothermal conditions

M Herrmann, J Schilm, G Michael, J Meinhardt, R Flegler

Publisher page

Abstract

Abstract Silicon nitride ceramics with different amounts and compositons of the grain boundary phases are produced by gas pressure sintering and the corrosion behaviour was analysed in acids, bases and under hydrothermal conditions. The investigation shows, that the corrosion is strongly affected by the SiO 2 content in the grain boundary and the amount of the additives. The results indicate that the grains and the thin films between the grains are very stable in acids and bases but solves partially under hydrothermal conditions. The corrosion behaviour of the investigated materials with a relatively stable grain boundary phase in acids can be described by the same kinetic laws as those used to describe the corrosion of glasses. An interfacial reaction is assumed to be rate-controlling. The less stable material with Y 2 O 3 /Al 2 O 3 additives can be described by the corrosion behaviour of oxide nitride glasses only at the beginning. For higher corrosion depths, the formation of protective barriers consisting of a hydrated SiO 2 network is assumed to occur.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · High-Temperature Coating Behaviors · Magnesium Oxide Properties and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (16)

Show source-provided references
1. Silicon nitride based hard materials
2. Corrosion resistance of silicon nitride ceramics
3. Mechanical degradation of silicon nitride ceramics in corrosive solutions of boiling sulphuric acid10.4028/www.scientific.net/KEM.113.227 ↗
4. Corrosion of silicon nitride in sulphuric acid aqueous solution10.1016/S0010-938X(00)00193-1 ↗
5. Theory of corrosion of glass and ceramics
6. Korrosionsstabile keramische Werkstoffe für Anwendungen in Wälzlagern und im Anlagenbau
7. Schilm, J., Herrmann, M., Michael, G., Kinetic study of corrosion of silicon nitride materials in acids. J. Eur. Cer. Soc., 2003, 23, 577–584.10.1016/S0955-2219(02)00375-8 ↗
8. The geometry of two phase aggregates in which the shape of the second phase is determined by its dihidral angle10.1016/0001-6160(76)90015-8 ↗
9. An inhomogeneous Grain Boundary Composition in Silicon Nitride10.1023/A:1022659412549 ↗
10. Bobeth · J. Am. Ceram. Soc. · 1999 · 82 · 153710.1111/j.1151-2916.1999.tb01952.x ↗
11. Corrosion behaviour of engineering ceramics in acids and basic solutions
12. Wötting, G., Herrmann, M., Michael, G., Siegel, S., Frassek, L., Sinteradditive und SiO2-enthaltende Siliciumnitridwerkstoffe, ein Verfahren zur Herstellung und deren Verwendung; patent DE 197 46 008.9 (1997) ;
13. WO 99/20579 (1999) patent.
14. Chemical Durability of glasses; a thermodynamic approach10.1007/BF00552247 ↗
15. Seipel, B., Nickel, K.G., J. Eur. Cer. Soc. (submitted for publication).
16. Herrmann, M., Schilm, J., Michael, G., Report of the DFG project (contract number HE 2471/1).