Surface strengthening of Ti3SiC2 through magnetron sputtering Cu and subsequent annealing
Source abstract
Abstract
Magnetron sputtering deposition Cu and subsequent annealing in the temperature range of 900-1100 degrees C for 30-60 min were conducted with the motivation to modify the surface hardness of Ti3SiC2. Owing to the formation of TiC following the reaction Ti3SiC2 + 3Cu -> 3TiC(0.67) + Cu3Si, the surface hardness was enhanced from 5.08 GPa to a maximum 9.65 GPa. In addition, the surface hardness was dependent on the relative amount of TiC, which was related to Cu film thickness, heat treatment temperatures and durations of annealing. Furthermore, after annealing at 1000 degrees C for 30 min the Cu-coated Ti3SiC2 has lower wear rate and lower COF at the running-in stage compared with Ti3SiC2 substrate. The reaction was triggered by the inward diffusion of Cu along the grain boundaries and defects of Ti3SiC2. At low temperature and short annealing time, i.e. 900 or 1000 degrees C for 30 min, Cu diffused inward Ti3SiC2 and accumulated at the trigonal junctions first. At higher temperature of 1100 degrees C or prolonging the annealing time to 60 min, considerable amount of Cu diffused to Ti3SiC2 and filled up the grain boundaries leaving a mesh structure. (c) 2008 Elsevier Ltd. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: MXene and MAX Phase Materials · Aluminum Alloys Composites Properties · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. Synthesis and characterization of a remarkable ceramic: Ti3SiC210.1111/j.1151-2916.1996.tb08018.x ↗
2. Damage mechanisms around hardness indentations in Ti3SiC210.1111/j.1151-2916.1997.tb02861.x ↗
3. In situ hot pressing/solid-liquid reaction synthesis of dense titanium silicon carbide bulk ceramics10.1007/s100190050076 ↗
4. The MN+1AXN phases: a new class of solids; thermodynamically stable nanolaminates10.1016/S0079-6786(00)00006-6 ↗
5. Diffusion kinetics of the carburization and silicidation of Ti3SiC210.1063/1.366707 ↗
6. Improving the surface hardness and wear resistance of Ti3SiC2 by boronizing treatment10.1016/j.surfcoat.2006.11.008 ↗
7. Crystallographic relations between Ti3SiC2 and TiC10.1007/PL00010876 ↗
8. Chemical reaction and stability of Ti3SiC2 in Cu during high-temperature processing of Cu/Ti3SiC2 composites10.3139/146.017911 ↗
9. Microstructure and mechanical strength of diffusion bonded Ti3SiC2/Ni joints10.1557/jmr.2006.0290 ↗
10. The topotactic transformation of Ti3SiC2 into a partially ordered cubic Ti(C0.67Si0.06) phase by the diffusion of Si into molten cryolite10.1149/1.1392573 ↗
11. Reaction of Al with Ti3SiC2 in the 800–1000°C temperature range10.1016/S0921-5093(00)01281-8 ↗
12. Thickness dependence of the structural and electrical properties of copper films deposited by dc magnetron sputtering technique10.1016/j.mejo.2005.09.016 ↗
13. Young · 1993
14. Relationships between hardness. Young's modulus and elastic recovery in hard nanocomposite coatings10.1016/S0257-8972(01)01714-5 ↗
15. Grain growth, agglomeration and interfacial reaction of copper interconnects10.1016/S0040-6090(02)00810-6 ↗
16. Evaluation of the thermal stability of reactively sputtered (Ti, Zr)Nx nano-thin films as diffusion barriers between Cu and silicon10.1016/j.tsf.2005.02.025 ↗
17. Structure stability of Ti3AlC2 into Cu and microstructure evolution of Cu–Ti3AlC2 composites10.1016/j.actamat.2007.03.033 ↗
18. Pearson · 1958
19. Olesinski · 1990 · vol. 2
20. Properties of rapidly solidified binary copper alloys10.1016/S0167-577X(96)00253-4 ↗
21. Understanding the fretting wear of Ti3SiC210.1016/j.jeurceramsoc.2005.05.006 ↗