journal article·2003-08

Design, fabrication and properties of layered SiC/TiC ceramic with graded thermal residual stress

Shuyi Qin, Dongliang Jiang, Jingxian Zhang, Jining Qin

Publisher page

Abstract

Abstract The finite element method (FEM) was used to design a symmetrical layered SiC/TiC ceramic with gradual thermal residual stress distribution. In the final model ceramic, the sequence of layers, from surface to inside, was SiC, SiC+2 wt.% TiC (S2T), SiC+4 wt.% TiC (S4T), SiC+6 wt.% TiC (S6T), SiC+8 wt.% TiC (S8T), and SiC+10 wt.% TiC (S10T); the thickness ratio of SiC:S2T:S4T:S6T:S8T:S10T was 1:1:1:1:1:10. After the model ceramic had been cooled from assumed sintering temperature 1850–20 °C in FEM calculation, gradual thermal residual stress, varying from surface compressive stress to inner tensile stress, was introduced. The designed ceramic then was fabricated by aqueous tape casting, stacking and hot-press sintering at 1850 °C, under 35 MPa pressure, for 30 min. The surface stress conditions of the sintered ceramic were tested by X-ray stress analysis, and those results were very close to the results from the FEM calculations. Compared with pure SiC and S10T ceramics fabricated by the same process, the designed ceramic showed excellent mechanical properties. The tested strength was close to the theoretical value. The strengthening and toughening mechanisms of the ceramic were ascribed to surface compressive residual stress.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · MXene and MAX Phase Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (22)

Show source-provided references
1. ZrO2/ZrO2 layered composites for crack bifurcation10.1111/j.1151-2916.1999.tb01949.x ↗
2. The Si3N4 and Si3N4/TiC layered composites by slip casting10.1016/S0272-8842(96)00044-2 ↗
3. Al2O3/TiC/(MoSi2+Mo2B5) multilayer composites prepared by tape casting10.1016/S0955-2219(99)00031-X ↗
4. Laminar ceramics that exhibit a threshold strength10.1126/science.286.5437.102 ↗
5. Damage-resistant SiC-AlN layered composites with surface compressive stresses10.1111/j.1151-2916.1992.tb05550.x ↗
6. Surface properties of ceramic laminates fabricated by die pressing10.1111/j.1151-2916.1996.tb08167.x ↗
7. Enhanced fracture toughness in layered microcomposites of Ce-ZrO2 and Al2O310.1111/j.1151-2916.1991.tb04290.x ↗
8. A simple way to make tough ceramics10.1038/347455a0 ↗
9. The fabrication and failure of laminar ceramic composites10.1016/0956-7151(92)90471-P ↗
10. Crack deflection and propagation in layered silicon nitride/boron nitride ceramics10.1111/j.1151-2916.1998.tb02438.x ↗
11. Laminar ceramic composites10.1016/0955-2219(95)93055-8 ↗
12. Timoshenko, S., Strength of Materials Part I: Elementary, 3rd edn. Van Nostrand Reinhold Company, 1955.
13. The effect of particle shape on ductility of SiCp reinforced 6061 Al matrix composites10.1016/S0921-5093(99)00503-1 ↗
14. Finite element analysis of stresses associated with transformations in magnesia partially stabilized zirconia10.1016/S0921-5093(99)00507-9 ↗
15. Kingery, W.D., Introduction to Ceramics. John Wiley & Sons, 1960.
16. Studies on the strengthening of silicon carbide-based multiphase ceramics I10.1016/0921-5093(89)90621-7 ↗
17. Toughening of layered ceramic composites with residual surface compression10.1111/j.1151-2916.1996.tb07883.x ↗
18. Noyan · 1987
19. Predecki · Adv. X-ray Anal. · 1988 · 31 · 23110.1007/978-1-4613-1035-8_25 ↗
20. Fullrath · J. Am. Ceram. Soc. · 1959 · 42 · 42310.1111/j.1151-2916.1959.tb12967.x ↗
21. Abuhasan · J. Am. Ceram. Soc. · 1990 · 73 · 247410.1111/j.1151-2916.1990.tb07615.x ↗
22. Grossman · J. Am. Ceram. Soc. · 1961 · 44 · 56710.1111/j.1151-2916.1961.tb11659.x ↗