Corrosion of silicon nitride in aqueous acidic solutions: penetration monitoring
Source abstract
Abstract
The degradation behaviour of silicon nitride in aqueous acidic solutions under steady state conditions was studied at 90 C and different flow rates. Two different compositions were chosen: Si3N4+4 wt.% Al2O3+6% Y2O3 (SN0) and Si3N4+2.4 wt.% MgAl2O4+1.3 wt.% Y2O3 (SN1). Corrosion was monitored by mass change, eluate chemistry, microstructure of the penetrated zone and fracture strength. The main corrosion mechanism is the leaching of the grain boundary phases. The penetrated depths consists of at least two zones with an outer layer, which is characterised by a complete or at least extensive removal of the total grain boundary phase and an inner zone, where pure silica, from which Y and Al have been leached, persists. The rates of dissolution of Al, Y and Si ions decreased with corrosion time. The fracture strength decreased with increasing degree of dissolution of the grain boundary phase. Changes in the chemistry of the grain boundary phases result in strong changes of corrosion resistance. Successful corrosion penetration depth monitoring can be done by polarised reflected light optical microscopy (colour changes), Micro Raman Spectroscopy (luminescence changes) and SEM (porosity changes). The corrosion process and its kinetics are evidenced best by microanalysis of cross sections, Raman spectroscopy and the eluate chemistry changes in addition to mass changes. # 2003 Elsevier Science Ltd. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Semiconductor materials and devices · Magnesium Oxide Properties and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (16)
Show source-provided references
1. Fletcher, A., Silicon Nitride and the SIALONS, Vol. 1. Elsevier Science publishers, 1993.10.1016/0926-6410(93)90001-L ↗
2. Lewis · 1984
3. Strength degradation of Si3N4–SiC-based ceramics in salt enviroments10.1016/0272-8842(86)90045-3 ↗
4. High-temperature gaseous corrosion of Si3N4 in H2-H2O and Ar-O2-environments10.1111/j.1151-2916.1990.tb06708.x ↗
5. Berthold, C., Degradation von Si3N4 als Ventilwerkstoff durch Oxidation und Salzschmelzkorrosion bei Einsatztemperaturen. Dissertation, Shaker Verlag, 1997.
6. Sangster R.S., Si: Silicon Nitride: Chemical Reactions (continued). Springer-Verlag, 1995, Suppl. Vol. B 5d2.
7. Corrosion of silicon nitride ceramics in aqueous hydrogen chloride solutions10.1111/j.1151-2916.1988.tb05794.x ↗
8. Corrosion of silicon nitride ceramics in aqueous HF solutions10.1007/BF00540476 ↗
9. Corrosion of silicon nitride ceramics by nitric acid
10. Corrosion behavior of silicon nitride ceramics in aqueous solutions (Part 2)10.2109/jcersj.100.80 ↗
11. Deutsches Institut f. Normung e.V., Testing of advanced technical ceramics, four bending test at room temperature. DIN 51110, 1990.
12. Corrosion behavior of silicon nitride ceramics in aqueous solutions (Part 1)
13. Corrosion of silicon nitride ceramics in aqeous HCl and HF solutions at 27–80 °C10.1016/S0010-938X(98)00011-0 ↗
14. Raman and IR absorbtion spectroscopic studies on α,β, and amorphous Si3N410.1016/0022-3093(81)90169-1 ↗
15. Catholuminescence microcharacterization of the defect structure of quartz10.1103/PhysRevB.52.3122 ↗
16. Korrosionsverhalten keramischer Werkstoffe für Anwendungen in Wälzlagern und im Anlagenbau