journal article·2004-01

Creep behavior of a carbon-derived Si3N4/SiC nanocomposite

J. Dusza, J. Kovalčı́k, P. Hvizdoš, P. Šajgalı́k, M. Hnatko, M. Reece

Publisher page

Abstract

Abstract The creep behavior of a silicon nitride–silicon carbide nanocomposite prepared by in situ utilizing C+SiO 2 carbothermal reduction is investigated at the temperature from 1200 to 1450 °C in bending under stresses ranking from 50 to 150 MPa in air. The stress exponents are in the interval from 0.8 to 1.28 and the apparent activation energy is 480 kJ/mol. No cavitation was found and grain-boundary sliding accommodated by diffusion through the intergranular glassy phase is considered to be the main creep mechanisms. The higher creep resistance of the nanocomposite compared with the creep resistance of a monolithic silicon nitride with the same amount of sintering additive can be explained by the presence of the intergranularly located SiC nano particles which limit grain boundary sliding and improve viscosity of the intergranular phase due to its changed chemical composition.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Boron and Carbon Nanomaterials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. Grain boundary films in rare-earth- glass-based silicon nitride10.1111/j.1151-2916.1996.tb07946.x ↗
2. Strength and creep behavior of rare-earth-disilcate-silicon nitride ceramics10.1111/j.1151-2916.1992.tb04464.x ↗
3. Controlled crystallization of the amorphous phase in silicon nitride ceramics10.1111/j.1151-2916.1987.tb05676.x ↗
4. Grain- boundary -phase crystallization and strenght of silicon nitride sintered with YSiAlON glass10.1111/j.1151-2916.1990.tb09803.x ↗
5. High temperature properties of Yb-containing Si3N4
6. Effect of microsrtucture on strenght of Si3N4–SiC composite system10.1111/j.1151-2916.1973.tb12520.x ↗
7. New design concept of structural ceramics–ceramic nanocomposites10.2109/jcersj.99.974 ↗
8. Improved creep resistance of Si3N4/SiC nanocomposites fabricated from amorphous Si–C–A precursor powder10.1007/BF00275414 ↗
9. Effect of a silicon carbide nano-dispersion on the mechanical properties of silicon nitride10.1111/j.1151-2916.1994.tb04545.x ↗
10. Si3N4/SiC nanocomposite materials: II, hot strength, creep, and oxidation resistance10.1111/j.1151-2916.1998.tb02457.x ↗
11. High -temperature properties of Si3N4/SiC nanocomposites10.1002/9780470294628.ch85 ↗
12. Mechanical properties of gas pressure sintered Si3N4/SiC nanocomposites10.1016/S0955-2219(01)00526-X ↗
13. Si3N4/SiCN Nanocomposites10.1016/S0955-2219(98)00128-9 ↗
14. Review
15. R-curve behavior and stable crack growth at elevated temperature (1500°–1650 °C) in a Si3N4/SiC nanocomposite10.1111/j.1151-2916.1994.tb04576.x ↗
16. Reactions between SiC and sintering aids in Si3N4/SiC nanocomposites and their concequences10.1016/S0272-8842(01)00003-7 ↗
17. Low-cycle fatigue strength under step loading of a Si3N4+SiC nanocomposite at 1350 °C10.1023/A:1017982719694 ↗
18. Si3N4/SiC nanocomposites materials: I fabrication and mechanical properties at room temperature10.1111/j.1151-2916.1998.tb02456.x ↗
19. Microstructure and high-temperature strength of Si3N4–SiC nanocomposite10.1016/S0955-2219(97)00180-5 ↗
20. High resolution electron microscopy studies on silicon nitride ceramics
21. Silicon nitride based nanocomposite10.1111/j.1151-2916.1996.tb07914.x ↗
22. Younǵs modulus and fracture of silicon nitride ceramics at elevated temperature10.4028/www.scientific.net/MSF.383.3 ↗
23. Effect of heat treatments on microstructure and creep behaviour of silicon nitride based ceramics10.1016/S0955-2219(02)00112-7 ↗
24. Hnatko, M. PhD Thesis, IIC SAS, Bratislava, 2002.
25. Impulse excitation apparatus to measure resonant frequencies, elastic moduli and internal friction at room and high temperatures10.1063/1.1148422 ↗
26. Calculation of stresses and strains in four-point bending creep tests10.1111/j.1151-2916.1971.tb12263.x ↗
27. The microstructure and creep deformation of hot-pressed Si3N4 with different amounts of sintering additives10.1557/JMR.1996.0015 ↗
28. SiC/Si3N4 Nano/micro-composite- processing, RT and HT mechanical properties10.1016/S0955-2219(99)00176-4 ↗
29. Creep damage in an advanced self-reinforced silicon nitride10.1111/j.1151-2916.1999.tb01867.x ↗
30. Creep and stress rupture behaviour of an advanced silicon nitride10.1111/j.1151-2916.1994.tb05396.x ↗
31. Transient creep behaviour of hot isostatically pressed silicon nitride10.1007/BF00357822 ↗
32. The high-temperature Creep deformation of Si3N4–6Y2O3–2Al2O310.1007/BF00544528 ↗