Pest-resistance in SiC/BN/SiC composites
Source abstract
Abstract
Abstract State-of-the-art non-oxide ceramic-matrix composites (consisting of SiC fibers, cvi -BN interphase coating, and mi -SiC matrix) exhibit excellent mechanical properties at room temperature, as well as above ∼1000 °C (where oxidation easily seals flaws with silica); but they are prone to pest degradation at intermediate temperatures in an oxidizing environment, and especially so in the fast, moist flame of a jet engine. Two modes of pest may be distinguished in these composites. The more severe type of pest is promoted by extraneous factors, like a layer of elemental carbon underlying the BN interphase and undermining its intrinsic oxidation resistance. It is shown that, when care is taken to exclude such a carbon layer, SiC/BN/SiC composite can easily survive a 100-h exposure in a burner rig without noticeable loss of strength or strain to fracture.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · MXene and MAX Phase Materials · Boron and Carbon Nanomaterials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (16)
Show source-provided references
1. DiCarlo, J., Yun, H.M., Morscher, G.N., and Ogbuji, L.U.J.T., Progress in SiC/SiC composites for engine applications. Proceedings of Materials Week 2001, Munich, Germany.10.1002/3527605622.ch118 ↗
2. Oxidation of the carbon interface in Nicalon-fiber-reinforced SiC composite10.1111/j.1151-2916.1997.tb02868.x ↗
3. Oxidation embrittlement probe for ceramic-matrix composites10.1111/j.1151-2916.1995.tb08621.x ↗
4. Oxidation of BN-coated SiC fibers in ceramic-matrix composites10.1111/j.1151-2916.1996.tb08163.x ↗
5. A pervasive mode of oxidative degradation in a SiC-SiC composite10.1111/j.1151-2916.1998.tb02696.x ↗
6. Tensile stress-rupture of SiC/SiC minicomposite with carbon and boron nitride interphases at elevated temperatures in air10.1111/j.1151-2916.1997.tb03087.x ↗
7. High-temperature oxidation of boron nitride10.1111/j.1151-2916.1999.tb01944.x ↗
8. Environmental durability of BN-based interphases (for SiC/SiC composites) in H2O-containing atmospheres at intermediate temperatures10.1002/9780470294437.ch58 ↗
9. Models of high-temperature, environmentally assisted embrittlement in ceramic-matrix composites10.1111/j.1151-2916.1996.tb08982.x ↗
10. Oxidation embrittlement probe for ceramic-matrix composites10.1111/j.1151-2916.1995.tb08621.x ↗
11. Intermediate-temperature stress rupture of a woven Hi-Nicalon, BN-interphase, SiC-matrix composite in air10.1111/j.1151-2916.2000.tb01408.x ↗
12. Identification of carbon sublayer in a Hi-Nicalon/BN/SiC composite10.1023/A:1006695105463 ↗
13. Silicon-based ceramic matrix composites for advanced turbine engines: degradation issues
14. HSR/EPM combustor materials development program10.1016/S0921-5093(98)01079-X ↗
15. Rebillat, F., Gallet, S.L., Bourrat, X., and Naslain, R., Oxidation resistance of BN coatings with different textures (poster). Materials Week 2001, Munich.10.1002/3527605622.ch31 ↗
16. Yun, H., and DiCarlo, J., unpublished work.