journal article·2002-08

Joining alumina using an alumina/metal composite

J.Q Li, P Xiao

Publisher page

Abstract

Abstract Alumina/alumina (Al 2 O 3 /Al 2 O 3 ) joints and alumina/aluminium metal–matrix composite (Al 2 O 3 /Al–MMC) joints were fabricated using an Al 2 O 3 –Al composite as an interlayer. The Al 2 O 3 /Al 2 O 3 joining procedures involved the sintering of silica or silicate glass on the surface of the Al 2 O 3 , followed by the reactive penetration of liquid aluminium into the sintered glass to form an Al 2 O 3 –Al composite interlayer between the two Al 2 O 3 pieces. To join Al 2 O 3 to Al–MMC, after the fabrication of the Al 2 O 3 –Al composite layer on the surface of Al 2 O 3 using the combination of sintering and reactive penetration, Al 2 O 3 /composite/MMC joints were fabricated by using diffusion bonding between the Al 2 O 3 –Al composite layer and the MMC. The microstructures, phase composition and mechanical properties of the joints were examined using scanning electron microscopy (SEM), XRD analysis and shear testing, respectively. Experimental results showed that the high porosity in the sintered glass layer led to the formation of a porous Al 2 O 3 –Al composite layer between two Al 2 O 3 pieces. The addition of cordierite (2MgO·2Al 2 O 3 ·5SiO 2 ) to the pure silica lowered the melting point of the glass and led to the formation of a dense glass layer at the surface of the Al 2 O 3 . Consequently, a dense composite layer was produced. Stronger joints were fabricated with shear strengths of the Al 2 O 3 /Al 2 O 3 and Al-MMC/Al 2 O 3 joints of 105.2 and 47.6 MPa respectively.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (29)

Show source-provided references
1. Influence of welding conditions and residual-stresses on strength of Al2O3/Ti diffusion welds10.1179/026708390790191576 ↗
2. Properties of alumina/Al/alumina joints produced in air atmosphere10.1179/mst.1993.9.2.155 ↗
3. Influence of pressure on bonding of alumina with molten aluminium as insert10.1179/mst.1995.11.12.1287 ↗
4. Diffusion bonding of alumina to steel using soft copper interlayer10.1007/BF02403866 ↗
5. Transient liquid-phase bonding of alumina and metal matrix composite base materials10.1023/A:1018529228375 ↗
6. Effect of alloying elements in the brazing sheet on the bonding strength between Al2O3 and aluminum
7. The influence of brazing condition on joint strength in Al2O3/Al2O3 bonding10.1007/BF01151094 ↗
8. Solid state bonding of Al2O3 with Cu, Ni and Fe10.1023/A:1004397019927 ↗
9. Transient liquid-phase insert metal bonding of Al2O3 and AISI 304 stainless steel10.1023/A:1018581312445 ↗
10. Microstructure and bond strength of Ni–Cr steel/Al2O3 joints brazed with Ag–Cu–Zr alloys containing Sn or Al10.1179/026708399101505293 ↗
11. Some observation on the wetting and bonding of nitride ceramics10.1007/BF00584866 ↗
12. 1993
13. 1995
14. Residual strains in an Al2O3–Ni joint bonded with a composite interlayer10.1111/j.1151-2916.1998.tb02514.x ↗
15. Fabrication of ceramic/metal composites by reduction of glass SiO2 preforms in molten metals and alloys10.1007/BF00241164 ↗
16. Kinetics of metal-ceramic composite formation by reactive penetration of silicates with molten aluminum10.1111/j.1151-2916.1998.tb02634.x ↗
17. Variations in processing, microstructure and properties of Al/Al2O3 composites fabricated by displacement reaction10.1504/IJMPT.2001.005392 ↗
18. Fabrication and mechanical properties of Al/Al2O3 composite bodies by reactive infiltration of molten Al into SiO2 preform10.1557/JMR.2000.0333 ↗
19. MMCs with controlled non-uniform distribution of submicrometre Al2O3 particles in 6061 aluminium alloy matrix10.1179/026708300101508676 ↗
20. Hlavac · 1983
21. Synthesis of Al2O3–Al composites by reactive metal penetration10.1111/j.1151-2916.1996.tb07876.x ↗
22. Microstructure and composition of Al–Al2O3 composites made by reactive metal penetration10.1007/BF00352664 ↗
23. Smithells · 1976
24. Kingery · 1976
25. Joining of zirconia to metal with Cu–Ga–Ti and Cu–Sn–Pb–Ti fillers10.1016/S0921-5093(00)00916-3 ↗
26. Bond strength of ceramic-metal joints
27. Ceramic-metal composite formation by reactive metal penetration
28. Microstructure and properties of Al2O3–Al(Si) and Al2O3–Al(Si)–Si composites formed by in situ reaction of Al with aluminosilicate ceramics10.1007/BF02651867 ↗
29. Counteracting particulate segregation during transient liquid-phase bonding of MMC–MMC and Al2O3–MMC joints10.1023/A:1018624507922 ↗