The effect of sintering temperature variations on the development of electrically active interfaces in zinc oxide based varistors
Source abstract
Abstract
Abstract A series of zinc oxide based varistors containing 0.5 wt.% Bi 2 O 3 and 0.5 wt.% Mn 2 O 3 were prepared by a conventional mixed oxide route and sintered at temperatures between 950 and 1300°C. All samples showed the varistor effect, although as the sintering temperature was increased above 1000°C, the non-linear coefficient decreased from 22 to 3 at 1300°C. Local grain boundary property measurements were carried out using remote electron beam induced current (REBIC) configuration conductive mode scanning electron microscopy. The proportions of electrically active interfaces and those showing strong resistive contrast were found to increase with sintering temperature.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: ZnO doping and properties · Transition Metal Oxide Nanomaterials · Thin-Film Transistor Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (25)
Show source-provided references
1. Non-ohmic properties of zinc oxide ceramics10.1143/JJAP.10.736 ↗
2. The physics of metal oxide varistors10.1063/1.321701 ↗
3. Conduction mechanism of non-ohmic zinc oxide ceramics10.1063/1.325139 ↗
4. Metal oxide varistor action — a homojunction breakdown mechanism10.1016/0378-5963(78)90035-1 ↗
5. Theory of conduction in ZnO varistors10.1063/1.326191 ↗
6. Characterisation of individual interfacial barriers in a ZnO varistor material10.1063/1.344453 ↗
7. Dependence of ZnO varistor grain-boundary resistance on sintering temperature10.1007/BF00701426 ↗
8. Different single grain junctions within a ZnO varistor10.1063/1.338091 ↗
9. Inhomogeneous conductivity in varistor ceramics: methods of investigation10.1111/j.1151-2916.1991.tb08260.x ↗
10. Observation of charge separating defects in HgCdTe using remote contact electron beam induced current10.1063/1.99173 ↗
11. Problems associated with imaging resistive barriers in PTC thermistor ceramics using the SEM conductive mode10.1016/0955-2219(95)00023-N ↗
12. Space-charge domains at dislocation sites10.1063/1.1657423 ↗
13. Panin, G. N. and Yakimov, E. B., Temperature dependent EBIC contrast investigations of grain boundaries and precipitates in CdTe. Institute of Physics Conference, Series No. 117, Bristol, 1991, pp. 763–766
14. Local grain boundary property measurements10.4028/www.scientific.net/SSP.37-38.171 ↗
15. SEM EBIC investigations of ZnO varistor ceramics
16. Direct determination of barrier voltage in ZnO varistors10.1063/1.326015 ↗
17. Processing induced resistive barriers in ZnO varistor material10.1007/BF00349637 ↗
18. Direct observation of grain boundary Schottky barrier behaviour in zinc oxide varistor material10.1007/BF00586176 ↗
19. Grain size measurement
20. Admittance spectroscopy of polycrystalline ZnO–Bi2O3 and ZnO–BaO systems10.1111/j.1151-2916.1988.tb05026.x ↗
21. Effect of heat-treatments on the wetting behaviour of bismuth- rich intergranular phases in ZnO-Bi-Co varistors10.1111/j.1151-2916.1989.tb06188.x ↗
22. Bi segregation at ZnO grain boundaries in equilibrium with Bi2O3-ZnO liquid10.1016/0167-2738(95)92537-H ↗
23. Grain boundary SEM conductive mode contrast effects in additive free ZnO ceramics10.1016/1359-6454(95)00348-7 ↗
24. The relationship between crystal misorientation and conductive mode contrast of grain boundaries in additive free zinc oxide10.1023/A:1018629503011 ↗
25. Leach, C., Interface Science, 2000, in press.