Abstract
Abstract To enhance adsorption of harmful ions on type-A zeolites (LTA), hydroxyapatite (HAp) thin layers were synthesized on the LTA surface by an ion exchange reaction of Ca2+ for NH4+ under hydrothermal treatment. The temperatures and durations in the reactions were varied ranging from 25 to 200 °C and from 1 to 168 h. The samples synthesized were characterized by X-ray diffraction method (XRD), scanning electron microscopy (SEM), transmission electron microscopy (TEM) and Brunauer–Emmet–Teller method (BET). The structure of LTA was not destroyed by the hydrothermal treatments at 25 to 160 °C for 8 h and also at 120 °C for 1 to 72 h. The yield of HAp grown on the LTA surface, synthesized at 120 °C for 8 h, showed a maximum value of 0.82. The morphologies of HAp were dependent mainly on the temperatures. The specific surface area remained unchanged in the treatments at 25 to 40 °C for 8 h, as compared to the specific surface area of Ca-LTA, however up to 80 °C, the value decreased with an increase of exchange temperature.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Bone Tissue Engineering Materials · Chemical Synthesis and Characterization · Radioactive element chemistry and processing
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (17)
Show source-provided references
1. Breck · 1974 · 1
2. Atlas of zeolite structure types
3. Ion exchange behavior of natural zeolites in distilled water, hydrochloric acid, and ammonium chloride solution10.1081/SS-120019090 ↗
4. Ammonium ion exchange of synthetic zeolites: the effect of their open-window sizes, pore structures, and cation exchange capacities10.1081/SS-120039306 ↗
5. Effect of cage-size on ammonium adsorption by synthetic zeolites
6. Adsorption behavior of cesium and strontium on synthetic Zeolite-P10.1080/18811248.1993.9734500 ↗
7. Simultaneous removal of the radiotoxic nuclides Cs-137 and I-129 from aqueous solution10.1016/S1383-5866(97)00045-2 ↗
8. Fluoridated hydroxyapatite solubility and caries formation10.1038/247064a0 ↗
9. Morphology of apatite formed on surface of wollastonite coating soaked in simulate body fluid10.1016/S0167-577X(02)00848-0 ↗
10. Apatite formed on the surface of plasma-sprayed wollastonite coating immersed in simulated body fluid10.1016/S0142-9612(00)00386-0 ↗
11. Formation of hydroxyapatite on CaSiO3 powders in simulated body fluid10.1016/S0955-2219(01)00301-6 ↗
12. Preparation of hydroxyapatite in a reaction between alite and phosphoric acid
13. Hydrothermal preparation of type-A zeolite with hydroxyapatite surface layers10.1111/j.1151-2916.2004.tb07746.x ↗
14. Characterization of type-A zeolite with hydroxyapatite surface layer prepared by hydrothermal treatment
15. Crystalline zeolites I. The properties of a new synthetic zeolite, type A10.1021/ja01604a001 ↗
16. Formation process of mullite from NH4+-exchanged zeolite A10.2109/jcersj.103.93 ↗
17. Preparation of needle-like hydroxyapatite by homogeneous precipitation under hydrothermal conditions10.1002/jctb.280570409 ↗