The manufacture of partially-stabilised and fully-stabilised zirconia fibres blow spun from an alkoxide derived aqueous sol–gel precursor
Source abstract
Abstract
Aligned fibres of partially stabilised zirconia (PSZ, 4 mol% Y2O3) and fully stabilised zirconia (FSZ, 8 mol% Y2O3), 3–5 μm in diameter, were blow spun from a sol–gel precursor, and then fired to give the ceramic fibre. Various potential sol precursors were investigated and characterised, the optimum being an aqueous sol made from hydrolysed and peptised zirconium iso-propoxide. The resulting zirconia fibres were characterised and their evolution studied by XRD, DTA/TGA and SEM, and their mechanical properties assessed. It was found that both PSZ and FSZ fibres formed poorly crystalline cubic zirconia at only 200°C, which became fully crystalline after firing to 400°C. The cubic form was the only phase seen in the FSZ fibre, whereas the PSZ fibre formed the tetragonal phase after firing between 1000 and 1200°C/3 h, and all fibres were nanocrystalline (grain diameter<0.1 μm). Unusually the monoclinic form of zirconia was never observed in the PSZ fibres. After firing above 1200°C the fibres had a strain to break of 0.59%, and appeared to be well sintered from shrinkage data. They had superior creep resistance to Saffil zirconia fibres, creeping at temperatures 50°C higher.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Microwave Dielectric Ceramics Synthesis · Recycling and utilization of industrial and municipal waste in materials production
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (22)
Show source-provided references
1. Naumann, A. W. and Gortsena, F. P. (Union Carbide Corp.), Ger. Offen. 2007209, September 1970.
2. Stabilization of the tetragonal structure in zirconia microcrystals10.1021/j100491a016 ↗
3. Garvie · Nature · 1975 · 258 · 70310.1038/258703a0 ↗
4. Tetragonal-to-monoclinic phase-transformation during thermal cycling and isothermal aging in yttria partially-stabilized zirconia10.1007/BF02403953 ↗
5. High-strength zirconia fibres10.1111/j.1151-2916.1987.tb05721.x ↗
6. Synthesis of polycrystalline zirconia with organozirconium precursor10.1007/BF00638033 ↗
7. Preparation of continuous zirconia fibres from polyzirconoxane synthesized by the facile one-pot reaction10.1023/A:1004357405815 ↗
8. The manufacture of yttrium aluminium garnet (YAG) fibres by blow spinning from a sol–gel precursor10.1016/S0955-2219(98)00088-0 ↗
9. Blow spun strontium zirconate fibres produced from a sol–gel precursor10.1023/A:1013225224143 ↗
10. Inorganic sol gel synthesis of zirconium titanate fibres10.1007/BF01160801 ↗
11. A novel aqueous route for the synthesis of mullite fibres10.1007/BF00636186 ↗
12. Novel aqueous sol–gel preparation and characterization of barium M ferrite, BaFe12O19 fibres10.1023/A:1018593014378 ↗
13. Aligned hexagonal ferrite fibres of Co2W, BaCo2Fe16O27 produced from an aqueous sol–gel process10.1023/A:1018541314320 ↗
14. The manufacture, characterisation and microwave properties of aligned M ferrite fibres10.1016/S0304-8853(98)00107-3 ↗
15. The synthesis and characterisation of aligned fibres of the ferroxplana ferrites Co2Z, 0.67% CaO-doped Co2Z, Co2Y and Co2W10.1016/S0304-8853(98)00098-5 ↗
16. The manufacture and characterisation of single phase magnetite and haematite aligned fibres from an aqueous sol–gel process10.1023/A:1004488005428 ↗
17. The sintering behaviour, mechanical properties and creep resistance of aligned polycrystalline yttrium aluminium garnet (YAG) fibres, produced from an aqueous sol–gel precursor10.1016/S0955-2219(98)00283-0 ↗
18. Morton, M. J., Birchall, J. D. and Cassidy, J. E., UK Pat. 1360197, July 1974
19. A simple test for thermomechanical evaluation of ceramic fibers10.1111/j.1151-2916.1992.tb05455.x ↗
20. Duwez, P. S., Brown, F. H. and Odell, F., Phase Diagrams for Ceramists. American Ceramic Society, Columbus, OH 1964, Diag. 355, p. 140 (from Journal of the Electrochemical Society 98, 1951, 360).10.1149/1.2778219 ↗
21. The comparison of alumina and zirconia fibres using simple thermal and mechanical techniques10.1023/A:1004533612141 ↗
22. Fulrath, R. M. and Pask, J. A. (eds.), Ceramic Microstructures. John Wiley and Sons Inc., New York, 1968.