journal article·2011-05

Effect of MoSi2 content on the lubricated sliding-wear resistance of ZrC–MoSi2 composites

Beatriz Núñez-González, Angel L. Ortiz, Fernando Guiberteau, Nitin P. Padture

Publisher page

Abstract

Abstract The effect of MoSi 2 content (5, 10, and 20 vol.%) on the lubricated, sliding-wear behaviour of ZrC–MoSi 2 composites at room temperature is investigated and modeled. It was found that the resistance to sliding wear decreases markedly with increasing MoSi 2 content, with a greater rate of mild wear, an earlier transition from mild to severe wear, but essentially the same rate of severe wear. The analysis of the wear results using a mechanistic model indicated that the worsened sliding-wear resistance with the increase in MoSi 2 content derives from the decreased hardness and increased internal effective tensile stresses of the ZrC–MoSi 2 composite, which speed up the accumulation of damage induced by plastic deformation within the grains and shorten the onset of the grain-boundary fracture condition and subsequent grain pullout. Reduction of the MoSi 2 content thus emerges as an effective approach for making the ZrC–MoSi 2 composites more sliding-wear resistant under lubrication at room-temperature. These results may have important implications because ZrC holds promise for use in tribological applications requiring both wear resistance and electrical contact, and MoSi 2 is its commonest sintering additive.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced materials and composites · Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (23)

Show source-provided references
1. UHTCs: ultra-high temperature ceramic materials for extreme environment applications10.1149/2.F04074IF ↗
2. Engineering properties of carbides
3. Evolution of structure during the oxidation of zirconium diboride–silicon carbide in air up to 1500̊C10.1016/j.jeurceramsoc.2006.10.012 ↗
4. Lawn · 1993
5. A critical evaluation of indentation techniques for measuring fracture toughness: I. Direct crack measurements10.1111/j.1151-2916.1981.tb10320.x ↗
6. Microstructure and mechanical characterization of ZrC–Mo cermets produced by hot isostatic pressing10.1016/j.msea.2008.07.017 ↗
7. Elastic constants of MoSi2 and WSi2 single crystals10.1007/BF00587691 ↗
8. Indentation response of molybdenum disilicide10.1557/JMR.1998.0371 ↗
9. The deformation and ageing of mild steel. 3. Discussion of results10.1088/0370-1301/64/9/303 ↗
10. The cleavage strength of polycrystals
11. Model for toughness curves in two-phase ceramics: I. Basic fracture mechanics10.1111/j.1151-2916.1993.tb07759.x ↗
12. Model for toughness curves in two-phase ceramics: II. Microstructural variables10.1111/j.1151-2916.1993.tb07760.x ↗
13. Wear mechanisms
14. Grain-size and R curve effects in the abrasive wear of alumina10.1111/j.1151-2916.1989.tb09718.x ↗
15. The transition from mild to severe wear in alumina during sliding10.1016/0956-7151(92)90212-W ↗
16. Wear and wear transition mechanism in silicon carbide ceramics during sliding10.1111/j.1151-2916.1995.tb08440.x ↗
17. Wear and wear transition mechanisms of ceramics10.1016/0043-1648(95)06800-7 ↗
18. Wear and wear transition in silicon carbide ceramics during sliding10.1111/j.1151-2916.1996.tb08579.x ↗
19. Stepwise-graded Si3N4–SiC ceramics with Improved wear properties10.1111/j.1151-2916.2002.tb00404.x ↗
20. Wear-resistant ultra-fine-grained ceramics10.1016/j.actamat.2004.09.020 ↗
21. Effect of microstructure on sliding-wear properties of liquid-phase-sintered α-SiC10.1111/j.1551-2916.2005.00394.x ↗
22. Microstructural design of sliding-wear-resistant liquid-phase-sintered sic: an overview10.1016/j.jeurceramsoc.2007.02.190 ↗
23. Wear mechanism in ceramics