Build-up formation and corrosion of monolithic refractories in cement kiln preheaters
Source abstract
Abstract
Abstract Nowadays, the cost of energy and the environmental standards have encouraged cement manufacturers to replace conventional fuels by alternative fuels (industrial wastes and agricultural and forest residues). Therefore, the increasing uses of these alternative fuels in cement plants have severely increased build-up formation and attack of the monolithic refractories used. All this strongly affects the durability of the refractory castables. In order to investigate this issue a number of samples, taken from five cement kiln preheaters, were studied. The results obtained confirm that the build-up constitution varies broadly and they consist of alternate layers of slightly different compositions as a consequence of changes in operating conditions of the furnaces. Their growth and compactness are due to a vitreous phase formation. On the other hand, the main compounds causing the attack of the monolithic refractories are: K2O, SO3, CaO and Cl−. These give place, in the matrix of the refractory material, to a liquid phase together with minor amounts of different crystalline phases. The depth of the attack depends on the SiC content in the refractory castable, as the proportion of SiC in the matrix increases the depth of attack decreases. The liquid phase brings about the adherence of the ring to the refractory castables. Therefore, when build-up is removed, part of the refractory material adhered to them is also removed. The thickness of the peeled off material depends on the depth of the attack.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Recycling and utilization of industrial and municipal waste in materials production · Concrete and Cement Materials Research · Pigment Synthesis and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. 2004
2. Monolithic refractories for the cement industry
3. Improvement of resistance to alkali attack of refractory materials of the SiO2–Al2O3 system for temperatures up to 1300°C in rotary cement kilns
4. Monolithic refractories containing SiC
5. Alternative fuels for the cement industry10.1016/S0306-2619(02)00135-6 ↗
6. Solid wastes as a fuel in the cement industry in the UK
7. Use of wastes as fuels in the cement industry: Pros & Cons
8. The European Cement Association (CEMBUREAU). Alternative fuels in cement manufacture. Technical and environmental review. Copyright: CEMBUREAU. N° Editeur: D/1997/5457/April. Rue d’Arlon 55, B-1040 Brussels.
9. Boberg LM. Alternative fuels in cement production. PhD Project 2007, Book Partner, Nørhaven Digital Copenhagen, Denmark. ISBN:978-87-91435-49-8.
10. Mineral composition of build-up in cement kiln preheater10.1023/A:1010118824904 ↗
11. Ring formation process in rotary cement kilns
12. Alternative fuels and their impact on refractory linings
13. The use of alternative fuels in the cement industry
14. A contribution to the crystal chemistry of ellestadite and the silicate sulphate apatites
15. Identification of the incrustation in heat-recovery cyclones of the Dopol Kiln
16. Chlorellestadite in the preheater system of cement kilns as an indicator of HCl formation10.1016/j.cemconres.2004.05.028 ↗
17. Nonstoichiometry in chlorellestadite10.1016/j.solidstatesciences.2004.10.014 ↗
18. Thermal analysis of spurrite from a rotary cement kiln10.1007/BF01913030 ↗
19. Thermal decomposition of syngenite, K2Ca(SO4)2·H2O10.1016/j.tca.2003.12.001 ↗
20. Ternesite, Ca5(SiO4)2SO4, a new mineral from the Ettringer Bellerberg/Eifel, Germany10.1007/BF01163138 ↗
21. Rowe JJ, Morey GW, Zen CZ. System (NaCl)2–(KCl)2–CaSO4. Geol. Surv., Prof. Pap. (US), 1972, No. 741, 37 pp. Fig. 6070 in Phase Diagram for Ceramists. Vol. V, Edited by The Am. Ceram. Soc. Inc, 1983.