The beneficial effect of water vapour on the oxidation at 600 and 700 °C of a MoSi2-based composite
Source abstract
Abstract
The oxidation characteristics of a MoSi2-based composite in O2 and O2+10% H2O at 600 and 700 °C were investigated. The effects of temperature and water vapour on oxidation were examined. The oxidation kinetics were studied using a thermobalance and furnace exposure, while the morphologies and compositions of the oxides were examined using XRD, ESEM/EDX, and SEM/EDX. We propose that oxidation proceeds by the initial formation of MoO3 crystals and amorphous SiO2 on the surface. The MoO3 is then evaporated; as volatile (MoO3)3 species in O2 and additional MoO2(OH)2 species in O2+10% H2O, which results in a porous, Mo-depleted oxide. However, the pores in the Mo-depleted SiO2 scale heal, and a protective crystalline scale is established eventually. The vapour pressures of the abovementioned volatile species increase with temperature and/or water vapour content in the atmosphere, which leads to accelerated Mo depletion from the oxide scale. A shorter time elapses before the oxide scale is transformed into the relatively Mo-free protective SiO2 scale, which results in less oxide being formed. Thus, the formed scale becomes thinner in O2+10% H2O than in O2. Thereby the Mo removal is beneficial when water vapour is added to the exposure atmosphere.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Intermetallics and Advanced Alloy Properties · Advanced ceramic materials synthesis · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (14)
Show source-provided references
1. Low-temperature oxidation of molybdenum disilicide10.1007/BF02804369 ↗
2. Molybdändisilizid als Komponente morderner Hochtemperatur-verbundwerkstoffe
3. Oxidation of MoSi2 and comparison with other silicide materials10.1016/0921-5093(92)90324-T ↗
4. Fitzer, V. E., Molybdändisilizid als Hochtemperaturwerkstoff. In Proceedings of the Second Plansee Seminar, ed. F. Benesovsky. Pregamon press, Berlin, 1955, pp. 56–79.
5. Pesting of the high-temperature intermetallic MoSi210.1007/BF03222509 ↗
6. High-temperature oxidation of molybdenum disilicide10.1111/j.1151-2916.1966.tb13227.x ↗
7. The influence of water vapour on the oxidation of MoSi2 at 450C10.4028/www.scientific.net/MSF.369-372.419 ↗
8. Hansson, K., Halvarsson, M., Tang, J.-E., Pompe, R., Sundberg, M. and Svensson, J. E., Oxidation behaviour of a MoSi2 based composite in different atmospheres in the low temperature range (400–550 °C). J. Eur. Ceram. Soc. 2004, 24, 3559–3573.10.1016/j.jeurceramsoc.2003.11.024 ↗
9. Kingery, W.D., Introduction to Ceramics. Wiley, London, 1960, pp. 217–243.
10. Volatility of the oxides of tungsten and molybdenum in the presence of water vapour10.1038/163601b0 ↗
11. Polymeric gaseous species in the sublimation of molybdenum trioxide10.1063/1.1743417 ↗
12. Glemser, V. O. and Haeseler, R. V., Uber gasförmige hydroxide des molybdäns und wolframs. Zeitschrift fur anorganische und allgemeine Chemie, 1962, Band 316.10.1002/zaac.19623160309 ↗
13. Barin, I., Thermochemical Data of Pure Substances. VCH Verlsgsgesellschaft mbh., 1995.10.1002/9783527619825 ↗
14. NIST-JANAF Thermochemical Tables (4th ed.) J. Phys. Chem. Ref. Data, Monograph 9, 1998.