Fatigue-less electrocaloric effect in relaxor Pb(Mg1/3Nb2/3)O3 multilayer elements
Source abstract
Abstract
Abstract A study was made of the electrocaloric (EC) effect’s stability in relaxor Pb(Mg1/3Nb2/3)O3 multilayer elements. The sample was subjected to 106 unipolar cycles at an electric field amplitude of 110 kV cm−1. The dielectric and ferroelectric properties of the material change only slightly, while the microstructure does not reveal any detrimental evidence of the cycling. The initially measured EC temperature change of 1.45 K decreases by only 0.01 K upon cycling, exhibiting a fatigue-less behavior. The results justify the choice of relaxor multilayers as the working bodies in EC cooling devices, where the material should withstand numerous electric field cycles with high amplitudes, sometimes exceeding 100 kV cm−1.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Ferroelectric and Piezoelectric Materials · Microwave Dielectric Ceramics Synthesis · Multiferroics and related materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. More than will soon abandon its pursuit
2. Electrocaloric materials10.1146/annurev-matsci-062910-100341 ↗
3. Electrocaloric materials for future solid-state refrigeration technologies10.1016/j.pmatsci.2012.02.001 ↗
4. Electrocaloric effect: an introduction
5. Giant electrocaloric effect in thin-film PbZr0.95Ti0.05O310.1126/science.1123811 ↗
6. Simulation of chip-size electrocaloric refrigerator with high cooling-power density10.1063/1.4796184 ↗
7. Bulk relaxor ferroelectric ceramics as a working body for an electrocaloric cooling device10.1063/1.4907258 ↗
8. Active electrocaloric demonstrator for direct comparison of PMN-PT bulk and multilayer samples10.1080/00150193.2016.1160466 ↗
9. Coupling of the electrocaloric and electromechanical effects for solid-state refrigeration10.1063/1.4964124 ↗
10. Giant electrocaloric response over a broad temperature range in modified BaTiO3 Ceramics10.1002/adfm.201302386 ↗
11. Large electrocaloric effect in grain-size-engineered 0.9Pb(Mg1/3Nb2/3)O3-0.1PbTiO310.1016/j.jeurceramsoc.2015.09.031 ↗
12. Next-generation electrocaloric and pyroelectric materials for solid-state electrothermal energy interconversion10.1557/mrs.2014.256 ↗
13. Fatigue of lead zirconate titanate ceramics.I: Unipolar and DC loading10.1111/j.1551-2916.2007.01520.x ↗
14. Bipolar fatigue caused by field screening in Pb(Zr,Ti)O3 ceramics10.1111/j.1551-2916.2007.02041.x ↗
15. Electric fatigue of lead-free piezoelectric materials10.1111/jace.12811 ↗
16. Fatigue in bulk lead zirconate titanate actuator materials10.1002/adem.200500117 ↗
17. Mechanisms of aging and fatigue in ferroelectrics10.1016/j.mseb.2014.10.003 ↗
18. Discrimination between bulk and interface scenarios for the suppression of the switchable polarization (fatigue) in Pb(Zr,Ti)O3 thin films capacitors with Pt electrodes10.1063/1.121386 ↗
19. Relaxorlike dielectric properties and history-dependent effects in the lead-free K0.5Na0.5NbO3-SrTiO3 ceramic system10.1063/1.1779947 ↗
20. Effect of ferroelectric long-range order on the unipolar and bipolar electric fatigue in Bi1/2Na1/2TiO3-based lead-free piezoceramics10.1111/j.1551-2916.2011.04605.x ↗
21. Effect of composition and temperature on electric fatigue of La-doped lead zirconate titanate ceramics10.1063/1.356637 ↗
22. Cycling stability of lead-free BNT-8BT and BNT-6BT-3KNN multilayer actuators and bulk ceramics10.1016/j.jeurceramsoc.2013.09.006 ↗
23. Both high reliability and giant electrocaloric strength in BaTiO3 ceramics10.1038/srep02895 ↗
24. Electrocaloric properties in relaxor ferroelectric (1-x)Pb(Mg1/3Nb2/3)O3–xPbTiO3 system10.1063/1.4829012 ↗
25. Influence of the critical point on the electrocaloric response of relaxor ferroelectrics
26. Electrocaloric cooling: the importance of electric-energy recovery and heat regeneration10.1209/0295-5075/111/57009 ↗
27. Progress on electrocaloric multilayer ceramic capacitor development
28. Multilayer 0.9Pb(Mg1/3Nb2/3)O3-0.1PbTiO3 elements for electrocaloric cooling10.1016/j.jeurceramsoc.2016.09.010 ↗
29. Comparison of direct electrocaloric characterization methods exemplified by 0.92 Pb(Mg1/3Nb2/3)O3-0.08 PbTiO3 multilayer ceramics10.1111/jace.14805 ↗
30. Feret‘s statistical diameter as a measure of particle size10.1038/162329b0 ↗
31. Wilcox · 2002
32. JCPDS-International Center for Diffraction Data, P.D.F. 01-081-0861, NewtonSquare (2002).
33. Indirect and Direct Measurements of the Electrocaloric Effect
34. Mechanochemically synthesized lead magnesium niobate10.1111/j.1151-2916.1999.tb01925.x ↗
35. Synthesis of Pb(Mg1/3Nb2/3)O3 by self-assembled colloidal aggregates10.1111/j.1551-2916.2011.04443.x ↗
36. Aging of the linear and nonlinear dielectric susceptibility in a PLZT relaxor system10.1080/00150190008227980 ↗
37. Energy-storage properties and high-temperature dielectric relaxation behaviors of relaxor ferroelectric Pb(Mg1/3Nb2/3)O3–PbTiO3 ceramics10.1088/0022-3727/49/9/095302 ↗
38. High-resolution calorimetric study of Pb(Mg1/3Nb2/3)O3 single crystal10.1103/PhysRevLett.109.037601 ↗