Mechanical properties of WC–WB–W2B composites prepared by reaction sintering of B4C–W–WC powders
Source abstract
Abstract
Abstract Composites of WC–WB–W 2 B with no metallic binder were prepared by the reaction sintering of a B 4 C–W–WC (mole ratio 1:5:80) powder mixture at sintering temperatures between 1500 and 1900 °C using resistance-heated hot pressing. WB, W 2 B and a part of WC in the composites were formed by the solid-state reaction between B 4 C and W. Dense sintered bodies were obtained at and above 1650 °C, in which small aggregates composed of WB and W 2 B were scattered in WC matrices. The rapid grain growth of WC occurred over a temperature range between 1650 and 1700 °C, and correspondingly resulted in decreases of both the hardness and fracture toughness. The sintering temperature 1650 °C was the most suitable for preparing dense sintered bodies with combined high values of Young's modulus, hardness and fracture toughness.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced materials and composites · Advanced ceramic materials synthesis · Powder Metallurgy Techniques and Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (24)
Show source-provided references
1. Toth · 1971
2. Effect of hot isostatic pressing on binderless cemented carbide
3. Properties of ultra-fine grain binderless cemented carbide ‘RCCFN’10.1016/0263-4368(95)92676-B ↗
4. Resistance of a binderless cemented carbide to abrasion and particle erosion10.1016/S0043-1648(99)00140-4 ↗
5. Microstructure and abrasive wear of binderless carbides10.1111/j.1151-2916.2000.tb01580.x ↗
6. Transient plastic phase processing of titanium–boron–carbon composites10.1111/j.1151-2916.1993.tb03924.x ↗
7. Microstructural evolution during transient plastic phase processing of titanium carbide–titanium boride composites10.1111/j.1151-2916.1996.tb08017.x ↗
8. Synthesis of a TiB2–TiC composite by reactive spark plasma sintering of B4C and Ti10.2497/jjspm.45.1065 ↗
9. Ambient- and high-temperature properties of titanium carbide–titanium boride composites fabricated by transient plastic phase processing10.1111/j.1151-2916.1999.tb01815.x ↗
10. Synthesis of composites of compounds in the Ti–B–C system by reactive spark plasma sintering of B4C and Ti10.2109/jcersj.108.1260_747 ↗
11. Reactive formation of coatings at boron carbide interface with Ti and Cr Powders10.1016/0955-2219(95)00014-L ↗
12. Synthesis of TiB2–TiN composites by reactive spark plasma sintering of BN and Ti10.2497/jjspm.46.383 ↗
13. Synthesis of TiB2–Ti(CN) composites by reactive spark plasma sintering10.2497/jjspm.47.308 ↗
14. Preparation of WC–WB–W2B composites from B4C–W–WC powders and their mechanical properties10.2320/matertrans.43.1197 ↗
15. Vickers indentation fracture toughness test part 110.1179/mst.1989.5.9.865 ↗
16. E. Rudy, Compendium of Phase Diagram Data, Technical Report AFML-TR-65-2, Part V, 1969, p. 192.
17. Kubaschewski · 1993
18. Elastic properties of polycrystalline monoclinic Sm2O310.1111/j.1151-2916.1974.tb10885.x ↗
19. The cleavage strength of polycrystals
20. Reexamination of experimental strength-vs-grain-size data for ceramics10.1111/j.1151-2916.1972.tb11272.x ↗
21. Relation of strength, composition, and grain size of sintered WC–Co alloys
22. Vickers indentation fracture toughness test part 210.1179/mst.1989.5.10.961 ↗
23. Effects of addition carbides on the grain size of WC–Co alloy10.2497/jjspm.19.67 ↗
24. Micro-grained cemented carbide with high strength10.1016/0263-4368(91)90024-I ↗