Influence of residual and bridging stresses on the R-curve behavior of Mo- and FeAl-toughened alumina
Source abstract
Abstract
Abstract Alumina matrix was toughened using either metal molybdenum or intermetallic FeAl particles. Mo and FeAl dispersoids were chosen because they have different thermomechanical properties (i.e. Young's modulus, Poisson ratio, as well as thermal expansion coefficient), giving rise to different residual stresses in the matrix. The R-curve behavior of these composites was first studied by stable-crack propagation experiments as a function of the volume fraction of dispersoid. The optimum fraction for toughening was different in the two composites: 25 and 15 vol% addition led to maximum toughness in the Mo- and FeAl added composite, respectively. This difference was ascribed to residual stresses. Microscopic observation of the crack path revealed, in both composites, the systematic presence of dispersoids acting as bridging sites in the crack wake, but only a few of them were plastically stretched. Residual stresses in the Al 2 O 3 matrix, after sintering and microscopic bridging tractions during crack propagation, were quantitatively assessed using microprobe fluorescence spectroscopy. Bridging microstresses were assessed in situ by a linear map along the crack profile, at the critical condition for fracture propagation. Experimentally collected residual stresses and bridging stresses were discussed to explain the different fracture behavior of the composites.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Numerical methods in engineering
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (18)
Show source-provided references
1. Toughening of ceramics through crack bridging by ductile particles10.1111/j.1151-2916.1989.tb06112.x ↗
2. Evans, A. G., The new high toughness ceramics. In Materials Science Research, Vol. 6, ed. J. A. Pask and A. G. Evans. Plenum Press, New York, 1987, pp. 775–794.10.1007/978-1-4613-1933-7_78 ↗
3. The mechanics of toughness development in ductile phase reinforced brittle matrix composites10.1016/0956-7151(92)90078-S ↗
4. On the shielding effect of a multiligament zone of a crack in WC-Co10.1016/S1359-6454(97)00014-1 ↗
5. Effect of chromium on properties of Fe3Al10.1557/JMR.1989.1156 ↗
6. Measurement of microscopic bridging stresses in alumina/molybdenum composite by in situ fluorescence spectroscopy10.1111/j.1151-2916.1999.tb01904.x ↗
7. Stable crack extension of an alumina ceramic in three-point bending test10.2472/jsms.42.412 ↗
8. Measurement of rising R-curve behavior in toughened silicon nitride by stable crack propagation in bending10.1111/j.1151-2916.1995.tb09092.x ↗
9. Effect of notch-root radius on the fracture toughness of a fine-grained alumina10.1111/j.1151-2916.1994.tb07038.x ↗
10. Pressure measurement made by the utilization of ruby sharp line luminescence10.1126/science.176.4032.284 ↗
11. Determination of the piezospectroscopic coefficients for chromium-doped sapphire10.1111/j.1151-2916.1995.tb08493.x ↗
12. On the near-tip toughening by crack-face bridging in particulate and platelet-reinforced ceramics10.1016/1359-6454(95)00250-2 ↗
13. In situ measurements of frictional/bridging stresses in alumina using Raman spectroscopy10.1111/j.1151-2916.1998.tb02312.x ↗
14. Fracture behaviour of ZrO2-Zr composites10.1111/j.1151-2916.1977.tb14096.x ↗
15. Average stress in matrix and average energy of materials with misfitting inclusions10.1016/0001-6160(73)90064-3 ↗
16. Toughening of a particulate-reinforced ceramic-matrix composite by thermal residual stress10.1111/j.1151-2916.1990.tb05209.x ↗
17. Underwood, E. E., In Quantitative Stereology, Addison-Wesley Publ., Reading, Massachussets, 1970.
18. Irwin, G. R., Fracture. In Handbuch der Physik, Vol. 6, Springer-Verlag, Berlin, 1958, pp. 551–5940.10.1007/978-3-642-45887-3_5 ↗