Hydroxyapatite formation on bioactive-glazed alumina
Source abstract
Abstract
Alumina was coated with bioactive glass which is known to show a bonding behavior to living tissue. Another glass also coated between alumina and bioactive glass to compensate their differences in thermal expansion. After coating the alumina with bioactive glass, it reacted in simulated body fluids to investigate the formation of hydroxyapatite. The bioactive-glazed layer crystallized into α-wollastonite and β-wollastonite crystalline phases when the glaze was fired at 1200 °C and 1100 °C, respectively. When the samples reacted in SBF, α-wollastonite easily leached out of the surface and hydroxyapatite formed on the leached site. The leaching rate of α-wollastonite was faster than that of β-wollastonite, and the hydroxyapatite-forming rate was also faster in the sample containing α-wollastonite than in the other sample. No silica-rich layer was found underneath the newly developed hydroxyapatite.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Bone Tissue Engineering Materials · Facial Trauma and Fracture Management · Dental Implant Techniques and Outcomes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. Bonding mechanisms at the interface of ceramic prosthetic materials10.1002/jbm.820050611 ↗
2. Ceramic implants for humans10.1111/j.1551-2916.1986.tb00033.x ↗
3. Introduction of bioactive glass-ceramic by chemical treatment10.1016/S0142-9612(97)00084-7 ↗
4. Machinability and brittleness of glass-caramic10.1016/S0924-0136(96)02275-3 ↗
5. Apatite formation on the surface of Ceravital-type glass-ceramic in the body10.1002/jbm.820251105 ↗
6. Bioceramics:from concept to clinic10.1111/j.1151-2916.1991.tb07132.x ↗
7. Hench · 1993
8. In vitro stability of plasma-sprayed hydroxyapatite coatings on Ti-6Al-4V implant under cyclic loading10.1002/(SICI)1097-4636(200005)50:2<267::AID-JBM22>3.0.CO;2-7 ↗
9. The study of surface tranformation of pulsed laser deposited hydroxyapatite coating10.1002/(SICI)1097-4636(200005)50:2<239::AID-JBM19>3.0.CO;2-V ↗
10. Advances in bioceramics10.1111/j.1551-2916.1987.tb00047.x ↗
11. The ultrastructure of the plasma-sprayed hydroxyapatite-bone interface predisposing to bone bonding10.1016/S0142-9612(01)00177-6 ↗
12. Chemical and morphological changes of vacuum-plasma-sprayed hydroxyapatite coatings during immersion in simulated physiological solutions10.1111/j.1151-2916.1998.tb02298.x ↗
13. Thermal analysis of amorphous phases in hydroxyapatite coatings10.1111/j.1151-2916.1998.tb02301.x ↗
14. Hench, L. L., Bioglass Coated Al2O3 Ceramics. US Patent 4103002, 1978.
15. Bonding behavior of bioglass coated alumina
16. Sol-gel modification of silicon to induce apatite-forming ability10.1016/S0142-9612(98)00146-X ↗
17. Parsons T. R., Maita Y., C. Lalli M., A Manual of Chemical and Biological Methods for Seawater Analysis. Pergamon Press, 1984, pp. 22–28.10.1016/B978-0-08-030287-4.50015-3 ↗
18. Jee S. S., Behavior of Hydroxyapatite Formation in Bioactive Glass Coated on Alumina. MS Thesis, Inha University, 2002.
19. Hydroxyapatite formation on bioactive glass-ceramics of CaO–SiO2–P2O5 system10.1186/s40824-017-0102-x ↗
20. Induction of bioactivity of a non-bioactive glass ceramic by a chemical treatment10.1016/S0142-9612(97)00084-7 ↗
21. Compositional dependence of calcium phosphate layer formation in fluoride bioglass10.1002/jbm.820260905 ↗
22. Lee E. S., Hydroxyapatite Formation of Crystallized Bioactive Glaze on Alumina. MS Thesis, Inha University, 1995.
23. Effect of crystallization on apatite-layer formation of bioactive glass 45S510.1002/(SICI)1097-4636(199604)30:4<509::AID-JBM9>3.0.CO;2-T ↗
24. Hydroxyapatite formation on fluoride bioactive glasses coated on alumina
25. Early stages of calcium-phosphate layer formation in bioglasses10.1016/0022-3093(89)90011-2 ↗
26. Surface chemistry of bioactive glass-ceramics10.1016/0022-3093(90)90199-V ↗