journal article·2006-01

Characteristic reaction processes in the system brushite–NaOH solution

Kei Furutaka, Hideki Monma, Toshinori Okura, Satoshi Takahashi

Publisher page

Abstract

Abstract The reaction of brushite (CaHPO 4 ·2H 2 O, DCPD) with NaOH solutions ranging in concentration from 0 to 40 mass% were investigated at 25 °C. At low NaOH concentrations below 20 mass%, hydroxyapatite (HAp) formed directly through the reaction (1) DCPD → HAp. At middle concentrations of 20–27 mass%, DCPD changed once into Ca(OH) 2 and then into HAp, i.e., through the consecutive reaction (2) DCPD → Ca(OH) 2 → HAp. At high concentrations above 27 mass%, the consecutive reaction (3) DCPD → HAp → Ca(OH) 2 was concluded. The boundary concentrations, i.e., singular points, between the first/second and the second/third reactions were estimated to be ca. 20 and 27 mass%, respectively. HAp particles obtained were platelet aggregates of very fine HAp microcrystals. The platelet form was compatible to the original platelet DCPD form. HAp samples prepared in this reaction system were structurally low crystalline and compositionally stoichiometric, and had a feature of large heating weight losses below 400 °C.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Calcium Carbonate Crystallization and Inhibition · Crystallization and Solubility Studies · Thermal and Kinetic Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (10)

Show source-provided references
1. Preparation and Solubility of hydroxyapatite10.6028/jres.072A.052 ↗
2. Hydroxyapatite: preparation and properties10.1007/BF02137328 ↗
3. The large scale preparation of chromatographic grade hydroxyapatite and its application in protein separation procedures10.1002/jctb.5020230708 ↗
4. Hydroxyapatite formed from coral skeletal carbonate by hydrothermal exchange10.1038/247220a0 ↗
5. Solubility of Ca5(PO4)3OH in the system Ca(OH)2–H3PO4–H2O at 5, 15, 25, and 37°C10.6028/jres.081A.017 ↗
6. Solution Ca/P ratio affects calcium phosphate crystal phases10.1007/BF02405100 ↗
7. Variability of hydroxyapatite preparation
8. Changes in composition and structure of tricalcium phosphate under different pH conditions
9. Consecutive formation of portlandite and hydroxyapatite from tricalcium phosphate in NaOH concentrated solutions near the solubility singular point
10. Reaction of tricalcium phosphate with NaOH solutions ranging from 0.8 to 50mass%10.3363/prb1992.17.0_165 ↗