Threshold stress intensity factor in soda-lime silicate glass by interrupted static fatigue test
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: Concrete and Cement Materials Research · Structural Analysis of Composite Materials · Building materials and conservation
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. Stress corrosion and static fatigue of glass10.1111/j.1151-2916.1970.tb15962.x ↗
2. A simple method for evaluating slow crack growth in brittle materials10.1007/BF00049195 ↗
3. Subcritical crack growth in ceramics
4. Slow crack growth in brittle materials under dynamic loading conditions10.1007/BF00113930 ↗
5. Effect of corrosion processes on subcritical crack growth in glass10.1111/j.1151-2916.1981.tb15870.x ↗
6. Crack velocity functions and threshold in brittle solids10.1016/0955-2219(90)90053-I ↗
7. Effect of corrosive media on crack growth of model glasses and commercial silicate glasses
8. Fatigue limit and crack arrest in alkali-containing silicate glasses10.1007/BF02403942 ↗
9. Dependence of ultimate strength of glass under constant load on temperature, ambient atmosphere, and time10.1111/j.1151-2916.1953.tb12831.x ↗
10. Experimental study of fracture of glass: I, The fracture process10.1111/j.1151-2916.1954.tb14005.x ↗
11. Strength and static fatigue of abraded glass under controlled ambient conditions: II, Effect of various abrasions and the universal fatigue curve10.1111/j.1151-2916.1959.tb13578.x ↗
12. Strength and static fatigue of abraded glass under controlled ambient conditions: III, Aging of fresh abrasions10.1111/j.1151-2916.1960.tb14332.x ↗
13. Fracture velocity and fracture energy of glass in the fatigue range10.1111/j.1151-2916.1961.tb15341.x ↗
14. Strength and static fatigue of abraded glass under controlled ambient conditions: IV, Effect of surrounding medium10.1111/j.1151-2916.1961.tb13710.x ↗
15. The effect of chemical composition on the strength and static fatigue of soda-lime glass
16. Strength of glass — the Griffith method revised10.1111/j.1151-2916.1965.tb11791.x ↗
17. Surfaces, stresses-dependent surface reactions, and strength
18. Static fatigue in glass — a reappraisal10.1016/0022-3093(76)90115-0 ↗
19. Strength and fatigue of some binary and ternary silicate glasses10.1016/0022-3093(86)90406-0 ↗
20. Correlation between multistage crack growth and time-dependent strength in commercial silicate glasses. Part 1. Influence of ambient media and types of initial cracks
21. Correlation between multistage crack growth and time-dependent strength in commercial silicate glasses. Part 2. Influence of surface treatment
22. A method for evaluating the time-dependent failure characteristics of brittle materials — and its application to polycrystalline alumina10.1007/BF00550196 ↗
23. The stress corrosion limit: its measurement and implications
24. The interrupted static fatigue test for evaluating threshold stress intensity factor in ceramic materials: a theoretical analysis10.1016/0955-2219(95)00048-Y ↗
25. Static fatigue limit with particular reference to glass
26. Determination of threshold stress intensity for crack growth at high temperature in silicon carbide ceramics10.1111/j.1151-2916.1983.tb10044.x ↗
27. Static fatigue limit for sintered silicon carbide at elevated temperatures10.1111/j.1151-2916.1983.tb10560.x ↗
28. Threshold stress intensity for crack growth at elevated temperatures in a silicon nitride ceramic
29. Threshold stress intensity for crack growth in silicon carbide ceramics10.1111/j.1151-2916.1993.tb05329.x ↗
30. A fracture statistics estimate of the fatigue limit of a borosilicate glass10.1016/0955-2219(93)90083-4 ↗
31. Threshold stress intensity for oxidative crack healing in sintered silicon nitride10.1007/BF00278010 ↗
32. Fracture surface energy of glass10.1111/j.1151-2916.1969.tb13350.x ↗
33. Hahn · 1967