Microstructure evolution and tribological properties of TiB2/Ni–Ta cermets
Source abstract
Abstract
Abstract Cermets containing TiB2 and single or mixed metals were produced by conventional hot-pressing technique at 2100 °C for 1 h. Nickel, tantalum and their mixtures were used as alloying substances to enhance the density of TiB2 composites. The influence of metal addition on the microstructure and tribological properties were investigated. The addition of Ta powder greatly refined the microstructure of sintered samples. Similarly, the mixture of Ni and Ta metals hindered the grain growth of TiB2 particles during the hot-pressing while the samples were sintered up to 98% of theoretical density. The wear behaviour of the composites was assessed by ball on disk tests. The wear rate against alumina counterbody varied in the range of (5.9–21.2) × 10−6 mm3/Nm. The friction coefficient was not affected significantly by the alloying substances and only slightly increased from 0.58 for pure TiB2 to 0.67 for samples with Ta addition.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced materials and composites · Aluminum Alloys Composites Properties · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (18)
Show source-provided references
1. Influence of hot pressing sintering temperature and time on microstructure and mechanical properties of TiB2 ceramics10.1016/S0955-2219(01)00424-1 ↗
2. Thermally sprayed Ni(Cr)–TiB2 coatings using powder produced by self-propagating high temperature synthesis: microstructure and abrasive wear behaviour10.1016/S0921-5093(01)01918-9 ↗
3. Continuous turning with TiB2 cermets: preliminary cutting tests10.1016/0263-4368(93)90020-G ↗
4. Effect of microstructure on the properties of TiB2 ceramics
5. Preparation of a TiB2 composite with a nickel matrix by pulse plasma sintering with combustion synthesis10.1016/j.jeurceramsoc.2005.05.001 ↗
6. Lide · 2000
7. Bansal · 2005
8. Studies of the Mechanical Properties of TiB2–6%TaB2–1%CoB–x%mZrO210.1016/S0955-2219(96)00189-6 ↗
9. Ni–Ta (nickel–tantalum)10.1361/105497100770339798 ↗
10. The Ta–Ti (tantalum–titanium) system10.1007/BF02873705 ↗
11. Interdiffusion in the body cubic centered β-phase of Ta–Ti alloys10.1016/S1359-6454(97)00272-3 ↗
12. Adhesion and abrasion of sputter-deposited ceramic thin films on glass
13. Sliding wear behaviour and tribofilm formation of ceramics at high temperatures10.1016/j.surfcoat.2003.10.157 ↗
14. Sliding wear of silicon carbide–titanium boride ceramic matrix composites10.1111/j.1151-2916.1993.tb03815.x ↗
15. Tribological performance of SiC and TiB2 against SiC and Al2O3 at low sliding speeds10.1016/S0043-1648(03)00444-7 ↗
16. Tribological investigation of tantalum boride coating under dry and simulated body fluid conditions10.1016/j.wear.2007.01.009 ↗
17. Unlubricated fretting wear of TiB2-containing composites against bearing steel10.1007/s11661-002-0257-4 ↗
18. A TiB2 metal matrix composite coating enriched with nitrogen: microstructure and wear properties10.1016/j.apsusc.2007.12.044 ↗