Hot corrosion of V2O5-coated NdMgAl11O19 ceramic in air at 950°C
Source abstract
Abstract
Abstract NdMgAl11O19 ceramic was prepared by solid-state reaction at 1700 °C for 10 h in air, and exhibited a single phase of magnetoplumbite structure. Reaction between molten V2O5 and NdMgAl11O19 was investigated at 950 °C using an X-ray diffractometer, scanning electron microscopy and energy-dispersive X-ray spectroscopy. Molten V2O5 reacts with NdMgAl11O19 to form α-Al2O3, NdVO4 and MgAl2O4 at 950 °C in air. After hot corrosion at 950 °C for 50 h, α-Al2O3 is the main corrosion product. The thickness of the corrosion layer gradually increases with increasing corrosion time from 10 to 50 h.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Nuclear materials and radiation effects · Catalytic Processes in Materials Science
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. Thermal barrier coatings for gas-turbine engine applications10.1126/science.1068609 ↗
2. Recent developments in the field of thermal barrier coatings10.1007/s11666-009-9312-7 ↗
3. Yttria-stabilized zirconia thermal barrier coatings – a review10.1142/S0218625X06008670 ↗
4. Crystal structures of zirconia phases and their inter-relation10.4028/www.scientific.net/KEM.153-154.1 ↗
5. Ceramic materials for thermal barrier coatings10.1016/S0955-2219(03)00129-8 ↗
6. Phase equilibria in the refractory oxide systems of zirconia, hafnia and yttria with rare-earth oxides10.1016/j.jeurceramsoc.2008.01.009 ↗
7. Yb2O3 and Gd2O3 doped strontium zirconate for thermal barrier coatings10.1016/j.jeurceramsoc.2008.05.013 ↗
8. Hot corrosion behavior of V2O5-coated Gd2Zr2O7 ceramic in air at 700–850°C10.1016/j.jeurceramsoc.2009.01.001 ↗
9. Preparation and thermo-physical properties of La1−xNdxMgAl11O19 (x=0, 0.1, 0.2) ceramics10.1016/j.jallcom.2009.06.068 ↗
10. High-temperature hot corrosion behavior of gadolinium zirconate by vanadium pentoxide and sodium sulfate in air10.1016/j.jeurceramsoc.2010.05.002 ↗
11. Hot corrosion behaviour of Yb2Zr2O7 ceramic coated with V2O5 at temperatures of 600–800°C in air10.1016/j.corsci.2010.06.007 ↗
12. Thermal conductivity of the gadolinium calcium silicate apatites: effect of different point defect types10.1016/j.actamat.2011.03.008 ↗
13. Thermal aging behavior of plasma sprayed LaMgAl11O19 thermal barrier coating10.1016/j.jeurceramsoc.2011.05.036 ↗
14. Failure of the plasma-sprayed coating of lanthanum hexaluminate10.1016/j.jeurceramsoc.2008.01.023 ↗
15. Thermal properties of oxides with magnetoplumbite structure for advanced thermal barrier coatings10.1016/j.surfcoat.2007.09.048 ↗
16. Bose · 2007
17. Hot corrosion behavior of laser-glazed plasma-sprayed yttria-stabilized zirconia thermal barrier coatings in the presence of V2O510.1016/j.surfcoat.2006.07.018 ↗
18. Degradation of yttria-stabilized zirconia thermal barrier coatings by vanadium pentoxide, phosphorous pentoxide, and sodium sulfate10.1111/j.1551-2916.2007.01941.x ↗
19. Investigation of reactions between vanadium oxide and plasma-sprayed yttria-stabilized zirconia coatings10.1016/j.jeurceramsoc.2008.09.016 ↗
20. Degradation of plasma-sprayed yttria-stabilized zirconia coatings via ingress of vanadium oxide10.1016/j.jeurceramsoc.2008.10.003 ↗
21. Hot corrosion behaviour of plasma sprayed YSZ/LaMgAl11O19 composite coatings in molten sulfate–vanadate salt10.1016/j.corsci.2011.03.019 ↗