journal article·2012-02

Influence of brick pattern interface structure on mechanical properties of continuous carbon fiber reinforced lithium aluminosilicate glass–ceramics matrix composites

Long Xia, Xinyu Wang, Guangwu Wen, Xia Li, Chunlin Qin, Liang Song

Publisher page

Abstract

Abstract Continuous carbon fiber reinforced lithium aluminosilicate glass–ceramic matrix composites have been fabricated by sol–gel process and hot pressing technique. The results show that the Cf/β-eucryptite composites hot pressed at 1300 °C and Cf/β-spodumene composites hot pressed at 1400 °C form weak interface with brick pattern characteristics, leading to high mechanical performance. The maximum flexural strength and fracture toughness reach 571 ± 32 MPa and 9.8 ± 0.6 MPa m1/2 for Cf/β-eucryptite composites and 640 ± 72 MPa and 19.9 ± 1.8 MPa m1/2 for Cf/β-spodumene composites. On increasing the hot pressing temperature, the active chemical diffusion consumes brick pattern interface layer, which leads to the formation of strong bonding between carbon fiber and the matrix. As a result, the composites exhibit brittle fracture behavior and the mechanical properties decrease significantly.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Recycling and utilization of industrial and municipal waste in materials production · Concrete and Cement Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (51)

Show source-provided references
1. Anisotropic thermal expansion in silicates: a density functional study of β-eucryptite and related materials10.1103/PhysRevB.62.11487 ↗
2. Crystallization kinetics and mechanism of low-expansion lithium aluminosilicate glass–ceramics by dilatometry10.1111/j.1151-2916.2002.tb00498.x ↗
3. Crystallization behavior of β-spodumene in the calcinations of Li2O–Al2O3–SiO2–ZrO2 gels10.1007/BF00362157 ↗
4. Preparation and crystallization of precursor powders in Li2O–Al2O3–SiO2 system
5. Electrical resistance as a tool in determining the failure of fibres in a nicalon-reinforced LAS glass–ceramic with Ta2O5 additions10.1023/A:1018676524760 ↗
6. Assessment of the mechanical behaviour of SiC fibre reinforced magnesium lithium aluminosilicate glass–ceramic matrix composite tested under uniaxial tensile loading10.1016/S0955-2219(96)00074-X ↗
7. Thermal conductivity of vapor liquid solid and vapor solid silicon carbide whisker-reinforced lithiumaluminosilicate glass ceramic composites10.1111/j.1151-2916.1996.tb07937.x ↗
8. Hot sodium sulphate corrosion of a Nicalon silicon carbide fibre-reinforced lithium aluminosilicate glass–ceramic matrix composite10.1007/BF00369663 ↗
9. SiC fiber-reinforced lithium aluminosilicate matrix composites fabricated by the sol–gel process10.1007/BF01178438 ↗
10. Fiber reinforced glasses and glass–ceramics for high performance applications
11. The mechanical properties of carbon fiber reinforced Pyrex glass10.1007/BF00574937 ↗
12. Carbon fiber composites with ceramic and glass matrices10.1007/BF00549379 ↗
13. Interfacial bonding and the toughness of carbon fiber reinforced glass and glass–ceramics10.1007/BF00541756 ↗
14. Development of low-thermal-expansion silicon carbide/zirconium tungstate porous ceramics10.1111/j.1551-2916.2010.03952.x ↗
15. Low-temperature sintering of ZrW(2)O(8)–SiO(2) by spark plasma sintering10.1007/s10853-008-3128-6 ↗
16. Low-temperature sintering of high-strength beta-eucryptite ceramics with low thermal expansion using Li(2)O–GeO(2) as a sintering additive10.1111/j.1551-2916.2010.04279.x ↗
17. Solid state sintering of very low and negative thermal expansion ceramics by spark plasma sintering10.1016/j.ceramint.2010.11.035 ↗
18. Spark plasma sintering of fine alpha-silicon nitride ceramics with LAS for spatial applications10.1016/j.jeurceramsoc.2010.10.026 ↗
19. Enhancing performance of ceramic composites
20. Processing of metal and ceramic matrix composites
21. The effect of TiO2 addition on the crystallization and phase formation in lithium aluminum silicate (LAS) glasses nucleated by P2O510.1016/j.jpcs.2008.06.003 ↗
22. Raman spectroscopy quantifying the composition of stuffed β-quartz derivative phases in lithium aluminosilicate glass–ceramics10.1016/j.jnoncrysol.2008.07.016 ↗
23. Growth behavior, morphology and properties of lithium aluminosilicate glass ceramics with different amount of CaO, MgO and TiO2 additive10.1016/j.ceramint.2007.03.032 ↗
24. Nucleation of lithium aluminosilicate glass containing complex nucleation agent10.1016/j.ceramint.2006.04.019 ↗
25. Effect of Y2O3 addition on viscosity and crystallization of the lithium aluminosilicate glasses10.1016/j.tca.2007.01.022 ↗
26. Raman spectroscopy study of phase transformations in titania-containing lithium aluminosilicate glasses doped with CoO10.1016/j.jnoncrysol.2005.07.019 ↗
27. The crystallization behavior and thermal expansion properties of β-eucryptite prepared by sol–gel route10.1016/j.matchemphys.2009.10.003 ↗
28. Sol–gel synthesis and crystallization behaviour of beta-spodumene10.1007/s10971-009-2001-7 ↗
29. The interface, microstructure and mechanical properties of Cf/LAS glass–ceramic composites10.1007/BF00354403 ↗
30. Hardy · 1988
31. The effect of aluminum sources on synthesis of low expansion glass–ceramics in lithia–alumina–silica system by sol–gel route10.1016/j.jnoncrysol.2009.08.020 ↗
32. Effects of interface modification on mechanical behavior of Hi-Nicalon fiber-reinforced Celsian matrix composites10.1002/9780470294437.ch43 ↗
33. The applications of CMCs in high integrity gas turbine engine10.4028/www.scientific.net/KEM.127-131.165 ↗
34. Interfacial characterization of glass/Nicalon fiber composites: a thermodynamic approach10.1002/9780470310496.ch16 ↗
35. Interface characterization and fracture of calcium aluminosilicate glass–ceramic reinforced with Nicalon fibres10.1007/BF00540709 ↗
36. Reaction–layer interfaces in SiC-fiberreinforced glass–ceramics: a high resolution scanning transmission electron microscopy study10.1111/j.1151-2916.1990.tb06694.x ↗
37. Sintering Li2O–Al2O3–4SiO2 precursor powders with ultrafine TiO2 additives10.1016/S0254-0584(01)00519-3 ↗
38. SIMS, EDX, EELS, AES, XPS study of interphases in Nicalon fibre-LAS glass matrix composites, Part I. Composition of the interphases10.1007/BF00357346 ↗
39. SIMS, EDX, EELS, AES, XPS study of interphases in Nicalon fibre-LAS glass matrix composites, Part II. Chemistry of the interphases10.1007/BF00376276 ↗
40. Structure and chemistry of the fibrematrix interfaces in silicon carbide fibre-reinforced glass–ceramic composites: an electron microscopy study10.1007/BF01161176 ↗
41. TEM study of carbon fiber reinforced aluminium matrix composites: influence of brittle phases and interface on the mechanical properties10.1016/S0955-2219(00)00021-2 ↗
42. Skin/bulk nanostructure and corrosion of SiC-based fibres: a surface Rayleigh and Raman study10.1002/jrs.1053 ↗
43. Strong fibers
44. Very low thermal expansion coefficient materials10.1146/annurev.ms.19.080189.000423 ↗
45. Strand · 1986
46. Ceramic matrix composite toughening mechanisms: an update10.1002/9780470320280.ch11 ↗
47. The role of the fiber–matrix interface in ceramic composites
48. Effect of interface mechanical properties on pullout in a SiC-fiber-reinforced lithium aluminum silicate glass–ceramic10.1111/j.1151-2916.1989.tb06171.x ↗
49. Oxide ceramic matrix/oxide fibre woven fabric composites exhibiting dissipative fracture behaviour10.1016/0010-4361(95)91380-N ↗
50. Effect of hot pressing time and post-heat treatment on the microstructure and mechanical properties of SiC-fiber-reinforced glass–ceramics composites10.1007/BF00357328 ↗
51. Tensile and flexural strength of silicon carbide fiber-reinforced glass–cermics10.1007/BF02403007 ↗