journal article·2013-10

High temperature corrosion of oxide bonded silicon carbide refractory lining in WtE facilities

Jean-Michel Brossard, Pascal Prigent, Jacques Poirier

Publisher page

Abstract

Abstract This study investigated oxide bonded SiC refractories lining failure in Waste-to-Energy boilers taking into account SiC material description and operating conditions. SiC tiles located at different elevations are instrumented with thermocouples. Hot side temperatures range from 900 °C to 700 °C depending on flue gas temperature at corresponding elevations. On-site tile observation showed: (i) wear by slag phases, (ii) swelling and cracks of tiles and (iii) fractures. Post-mortem analysis after several thousand hours of operation revealed three main corrosion mechanisms: molten salt/slag attack (Na, K, Ca sulphate phases), salt condensation inducing new phase formation (SiO2–CaSO4–K2SO4) and SiC oxidation. The relative contributions of chemical degradation mechanisms are discussed and tile deformation is related to thermo-chemo-mechanical coupled effect.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Metallurgical Processes and Thermodynamics · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (27)

Show source-provided references
1. Alkali/chloride release during refuse incineration on a grate: full-scale experimental findings10.1016/j.fuproc.2007.10.003 ↗
2. Krause HH, Wright IG. Boiler tube failures in municipal waste-to-energy plants: case histories, paper No 561, Corrosion/95, NACE, Houston, Texas, 1995.10.5006/C1995-95561 ↗
3. Refractory attack by acid and alkali in municipal and industrial waste incinerators
4. Melt corrosion of oxide and oxide–carbon refractories10.1179/095066099101528234 ↗
5. Corrosion mechanism of boiler tubes lined with refractories
6. Kinetics and mechanism of corrosion of SiC by molten salts10.1111/j.1151-2916.1986.tb04698.x ↗
7. Alkali induced corrosion of silicon carbide heating elements in a high temperature furnace
8. Stability of protective oxide films in waste incineration environment – solubility measurements of oxides in molten chlorides10.1016/S0010-938X(01)00059-2 ↗
9. A thermodynamic approach on vapor-condensation of corrosive salts from flue gas on boiler tubes in waste incinerators10.1016/j.corsci.2008.02.004 ↗
10. Kinetics of HCl emission from inorganic chlorides in simulated municipal wastes incineration conditions10.1016/j.ces.2004.07.131 ↗
11. Study of the corrosion mechanisms of SiC refractory lining in municipal solid waste-to-energy facilities
12. Analysis and interpretation of refractories microstructures in studies of corrosion mechanisms by liquid oxides10.1016/j.jeurceramsoc.2007.10.012 ↗
13. Effect of slag impregnation on thermal degradations in refractories10.1111/j.1551-2916.2006.01348.x ↗
14. Refractory corrosion in industrial waste incineration processes
15. Modeling of high temperature asymmetric creep behavior of ceramics10.1016/j.jeurceramsoc.2004.06.004 ↗
16. Corrosion of oxide bonded silicon carbide refractories by molten salts in solid waste-to-energy facilities10.1016/j.ceramint.2012.04.007 ↗
17. Investigations of SiC aggregates oxidation: influence on SiC castables refractories life time at high temperature10.1016/j.jeurceramsoc.2011.10.044 ↗
18. Observations of accelerated silicon carbide recession by oxidation at high water-vapor pressures10.1111/j.1151-2916.2000.tb01172.x ↗
19. Corrosion of silicon carbide in gases and alkaline melts10.1111/j.1151-2916.1976.tb09514.x ↗
20. High temperature oxidation of ceramic matrix composites10.1351/pac199870020493 ↗
21. Thermodynamic evaluation optimization of the (NaCl+Na2SO4+Na2CO3+KCl+K2SO4+K2CO3) system10.1016/j.jct.2006.12.018 ↗
22. Towards a comprehensive thermodynamic database for ash-forming elements in biomass and waste combustion – current situation and future developments10.1016/j.fuproc.2011.08.008 ↗
23. High temperature alkali corrosion of SiC and Si3N410.1016/0378-3820(94)00113-8 ↗
24. Effect of cations on crystallization of amorphous silica II
25. Kinetics and mechanism of oxidation of silicon nitride bonded silicon carbide ceramic10.1007/BF02546752 ↗
26. The acidic and basic properties of oxides10.3891/acta.chem.scand.01-0592 ↗
27. Modeling of the thermo-chemo-mechanical behavior of SiC-based refractory used in waste-to-energy plants