Mechanical properties of PECVD thin ceramic films
Source abstract
Abstract
Abstract Silicon dioxide (thickness 350 nm and 969 nm) and silicon nitride (thickness 218 nm) films deposited on silicon substrate using plasma enhanced chemical vapor deposition process were investigated using a Berkovich nanoindenter. The load-depth measurements revealed that the oxide films have lower modulus and hardness compared to the silicon substrate, where as the nitride film has a higher hardness and slightly lower modulus than the substrate. To delineate the substrate effect, a phenomenological model, that captures most of the ‘continuous stiffness measurement’ data, was proposed and then extended on both sides to determine the film and substrate properties. The modulus and hardness of the oxide film were around 53 GPa and 4–8 GPa where as those of the nitride film were around 150 GPa and 19 GPa, respectively. These values compare well with the measurements reported elsewhere in the literature.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · Semiconductor materials and devices
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (40)
Show source-provided references
1. Determination of mechanical properties of PECVD silicon nitride thin films for tunable MEMS Fabry–Pérot optical filters10.1088/0960-1317/15/3/024 ↗
2. Tunable Fabry–Pérot cavities fabricated from PECVD silicon nitride employing zinc sulphide as the sacrificial layer10.1088/0960-1317/11/5/323 ↗
3. Bulge testing and fracture properties of plasma-enhanced chemical vapor deposited silicon nitride thin films10.1016/j.tsf.2008.10.042 ↗
4. Mechanical properties of sputtered silicon nitride thin films10.1063/1.1626799 ↗
5. Growth and characterization of red–green–blue cathodoluminescent ceramic films10.1063/1.2209728 ↗
6. Nanomechanical characterisation of solid surfaces and thin films10.1179/095066003225010227 ↗
7. Development of the CAE-assisted nano-indentation method for the evaluation of the anisotropic mechanical-properties of thin films10.1016/j.jmatprotec.2004.04.072 ↗
8. Freund · 2003
9. Effect of substrate hardness and film structure on indentation depth criteria for film hardness testing10.1088/0022-3727/41/7/074010 ↗
10. Tensile testing of free-standing Cu, Ag and Al thin films and Ag/Cu multilayers10.1016/S1359-6454(00)00128-2 ↗
11. Deformation behavior of thin copper films on deformable substrates10.1016/S1359-6454(01)00293-2 ↗
12. Mechanical deflection of cantilever microbeams—a new technique for testing the mechanical properties of thin-films10.1557/JMR.1988.0931 ↗
13. Nanoindentation of coatings10.1088/0022-3727/38/24/R01 ↗
14. Nanoindentation stress–strain curves as a method for thin-film complete mechanical characterization: application to nanometric CrN/Cr multilayer coatings10.1007/s00339-002-1669-0 ↗
15. Investigation of the mechanical properties of thin films by nanoindentation, considering the effects of thickness and different coating–substrate combinations10.1016/j.surfcoat.2004.03.037 ↗
16. Determination of the mechanical properties of metallic thin films and substrates from indentation tests10.1080/01418610208235713 ↗
17. Inference of mechanical properties from instrumented depth sensing indentation at tiny loads and indentation depths10.1002/1521-4079(200004)35:4<377::AID-CRAT377>3.0.CO;2-Q ↗
18. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
19. Measurement of hardness and elastic modulus by instrumented indentation: advances in understanding and refinements to methodology10.1557/jmr.2004.19.1.3 ↗
20. Critical issues in making small-depth mechanical property measurements by nanoindentation with continuous stiffness measurement10.1557/jmr.2009.0096 ↗
21. Analysis of elastic and plastic deformation associated with indentation testing of thin films on substrates10.1016/0020-7683(88)90091-1 ↗
22. Determination of elastic modulus of thin layers using nanoindentation10.1557/JMR.1997.0327 ↗
23. Multi-parameter models of the viscoelastic/plastic mechanical properties of coatings via combined nanoindentation and non-linear finite element modeling10.1016/S0300-9440(03)00145-0 ↗
24. Finite element analysis of substrate effects on indentation behaviour of thin films10.1016/S0040-6090(03)01071-X ↗
25. The effect of a substrate on the sintering of constrained films10.1016/j.actamat.2008.09.041 ↗
26. Size dependent nanoindentation of a soft film on a hard substrate10.1016/j.actamat.2003.10.039 ↗
27. Characterization of mechanical properties of thin films using nanoindentation test10.1016/j.mechmat.2006.02.011 ↗
28. Nanoindentation of plasma-deposited nitrogen-rich silicon nitride thin films10.1063/1.2217105 ↗
29. Elastic–plastic indentation damage in ceramics: the lateral crack system10.1111/j.1151-2916.1982.tb10782.x ↗
30. Elastic–plastic indentation damage in ceramics: the median/radial crack system10.1111/j.1151-2916.1980.tb10768.x ↗
31. An elastic–plastic-cracking model for finite element analysis of indentation cracking in brittle materials10.1016/S0020-7683(00)00406-6 ↗
32. Direct observation and analysis of indentation cracking in glasses and ceramics10.1111/j.1151-2916.1990.tb05119.x ↗
33. Toughness of hard nanostructured ceramic thin films10.1016/j.surfcoat.2006.07.020 ↗
34. A simple indentation stress–strain relation for contacts with spheres on bilayer structures10.1016/S0040-6090(97)00919-X ↗
35. Evaluation of elastic modulus and hardness of thin films by nanoindentation10.1557/JMR.2004.0380 ↗
36. Buckle · 1973 · 453
37. Substrate effects on nanoindentation mechanical property measurement of soft films on hard substrates10.1557/JMR.1999.0042 ↗
38. The mechanical properties and microstructure of plasma enhanced chemical vapor deposited silicon nitride thin films10.1116/1.577257 ↗
39. Dynamic micromechanics on silicon—techniques and devices10.1109/T-ED.1978.19259 ↗
40. Effect of deposition conditions on mechanical properties of low-temperature PECVD silicon nitride films10.1016/j.msea.2006.07.015 ↗