journal article·2013-09

Molten salt attack on t′ yttria-stabilised zirconia by dissolution and precipitation

Narender Reddy, Ashutosh S. Gandhi

Publisher page

Abstract

Abstract Degradation due to molten salt attack is one of the failure mechanisms of thermal barrier coatings. Thermochemical attack of the salt mixture Na 2 SO 4 –30 mol% NaVO 3 on ZrO 2 –8 mol% YO 1.5 (8YSZ) at 950 °C was studied by two types of experiments. Sintered compacts were exposed to 25 mg cm −2 salt dosage for up to 96 h. In the other set of experiments, 10–35 wt.% 8YSZ powder was mixed with the salts to study the dissolution of 8YSZ in the molten salt. The role of volatile losses was also examined. The results show that more than 25 wt.% 8YSZ dissolves in the sulphate-vanadate melt at 950 °C, followed by slow reactions to form YVO 4 and NaYV 2 O 7 at 950 °C. The unreacted Y 2 O 3 and monoclinic ZrO 2 precipitate out separately during rapid cooling (∼300 °C/min). Slow cooling at ∼3 °C/min leads to the formation of ZrOS apart from ZrO 2 and Y 2 O 3 .
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Nuclear Materials and Properties · Nuclear materials and radiation effects

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (22)

Show source-provided references
1. Materials design for the next generation thermal barrier coatings10.1146/annurev.matsci.33.011403.113718 ↗
2. Thermal barrier coatings for gas-turbine engine applications10.1126/science.1068609 ↗
3. The influence of oxides on the performance of advanced gas turbines10.1016/j.jeurceramsoc.2007.12.023 ↗
4. Impurity deposits in gas turbines from fuels containing sodium and vanadium10.1149/1.2123941 ↗
5. Destabilization of yttria-stabilized zirconia induced by molten sodium vanadate-sodium sulfate melts10.1149/1.2113609 ↗
6. Degradation of plasma-sprayed yttria-stabilized zirconia coatings via ingress of vanadium oxide10.1016/j.jeurceramsoc.2008.10.003 ↗
7. Investigation of reactions between vanadium oxide and plasma-sprayed yttria-stabilized zirconia coatings10.1016/j.jeurceramsoc.2008.09.016 ↗
8. Destabilization of zirconia thermal barriers in the presence of V2O510.1111/j.1151-2916.1988.tb07570.x ↗
9. Effect of Al2O3 overlay on hot-corrosion behavior of yttria-stabilized zirconia coating in molten sulfate-vanadate salt10.1016/S0040-6090(03)00670-9 ↗
10. Some aspects of the hot corrosion of thermal barrier coatings10.1007/BF02646315 ↗
11. Hot corrosion studies of zirconia ceramics10.1016/0257-8972(87)90119-8 ↗
12. Microscopic observation of degradation behavior in yttria and ceria stabilized zirconia thermal barrier coatings under hot corrosion10.1016/j.surfcoat.2004.04.065 ↗
13. Burner rig evaluation of ceramic coatings with vanadium-contaminated fuels10.1115/1.2906201 ↗
14. In situ Raman spectroscopic study of yttria-stabilized zirconia attack by molten sodium vanadate10.1111/j.1151-2916.1984.tb19683.x ↗
15. Rebollo NR. Phase stability of thermal barrier oxides based on t′-zirconia with trivalent oxide additions. Ph.D. Thesis. Santa Barbara: University of California; 2005.
16. Fracture toughness of t′ ZrO2 stabilised with MO1.5 (M=Y, Yb & Gd) for thermal barrier application10.1007/s12666-011-0014-8 ↗
17. Effect of phase transformations on the fracture toughness of t′ yttria stabilized zirconia10.1016/j.msea.2012.07.095 ↗
18. Phase stability of thermal barrier oxides: a comparative study of Y and Yb additions10.3139/146.101595 ↗
19. Narender RB. Studies on molten salt attack on zirconia based thermal barrier materials. M.S. Thesis. Chennai, India: Indian Institute of Technology Madras; 2012.
20. Belyaev · Russ J Inorg Chem (Engl Transl) · 1973 · 18 · 711
21. Phase relationships in the zirconia–yttria system10.1007/BF01031853 ↗
22. Effect of yttria content on the zirconia unit cell parameters10.1111/j.1551-2916.2011.04862.x ↗