Shrinkage behavior of LTCC hetero-laminates
Source abstract
Abstract
Abstract Shrinkage behavior of various stacking configurations consisting of three dissimilar dielectric tapes with different dielectric constants of k ∼ 8.2, 14.8 and 48.2 were investigated. The shrinkage behavior has been critical as a sensitive parameter in the design of embedded microcircuit passive components. Unexpectedly low x–y shrinkages of 2.5–7% observed for the hetero-configurations are believed to be associated with the physical constraining effect that results from the dissimilar sintering route and crystallization behavior of each tape. The constraining effect found depends on the sintering temperature and the total number of each tape layer in a given hetero-structure. The tendency of slope variation in the Arrhenius plots of thermo–mechanical curves suggests that increasing the number of embedded tapes can produce a potential lower activation energy with a higher x–y shrinkage.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Microwave Dielectric Ceramics Synthesis · Electrical and Thermal Properties of Materials · Ferroelectric and Piezoelectric Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (24)
Show source-provided references
1. Cho · 2001
2. New Pb free tape system for automotive and telecommunication applications
3. High k LTCC system for high frequency applications
4. Tunable active filters having multilayer stucture using LTCC10.1109/22.971630 ↗
5. A new planar-type dielectric resonatro using LTCC technology for mm-wave band applications10.1002/mop.20688 ↗
6. Acompact LTCC bluetooth system module with an integrated antenna10.1002/mmce.20147 ↗
7. Low temperature co-fired tape dielectric material systems for multilayer interconnections
8. Multilayer ceramic circuit board with copper conductors.
9. Low firing temperature multilayer glass–ceramic substrate10.1109/TCHMT.1983.1136194 ↗
10. LTCC interconnects in microsystems10.1088/0960-1317/16/6/S03 ↗
11. High K low loss dielectrics co-fireable with LTCC10.1080/08827510212346 ↗
12. Constrained densification kinetics of alumina/borosilicate glass+alumina/alumina sandwich structure10.1111/j.1151-2916.2002.tb00057.x ↗
13. Effect of crystallization on the stress required for constrained sintering of CaO–B2O3–SiO2 glass–ceramics10.1111/j.1551-2916.2005.00173.x ↗
14. Constrained sintering of low-temperature co-fired ceramics10.1111/j.1551-2916.2006.01079.x ↗
15. Densification and sintering viscosity of low-temperature co-fired ceramics10.1111/j.1551-2916.2005.00497.x ↗
16. Co-firing and shrinkage matching in low- and middle-permittivity dielectric compositions for a low-temperature co-fired ceramics system10.1111/j.1551-2916.2005.00748.x ↗
17. Use of titanates to achieve a temperature-stable low-temperature cofired ceramic dielectric for wireless applications10.1111/j.1151-2916.2002.tb00179.x ↗
18. Effect of alumina particle size on prevention of crystal growth in low-k silica dielectric composite10.1016/0254-0584(94)01454-O ↗
19. Wetting, densification and phase transformation of La2O3/A2O3/B2O3-based glass–ceramics10.1016/j.jeurceramsoc.2004.10.001 ↗
20. Phase evolution and microwave dielectric properties of lanthanum borate-based low-temperature co-fired ceramics materials10.1111/j.1551-2916.2006.01035.x ↗
21. Sintering kinetics and microstructure development of nanoscale Y-TZP ceramics10.1016/0955-2219(93)90031-L ↗
22. Initial sintering with constant rates of heating10.1111/j.1151-2916.1970.tb12036.x ↗
23. Kinetics of the initial stage of sintering from shrinkage date: simultaneous determination of activation energy and kinetic model from a single nonisothermal experiment10.1111/j.1151-2916.2002.tb00169.x ↗
24. German · 1996