journal article·2010-05

Mechanisms and orientation dependence of the corrosion of single crystal Cordierite by model diesel particulate ashes

Nicolas Maier, Klaus G. Nickel, Christine Engel, Andreas Mattern

Publisher page

Abstract

Abstract Cordierite Mg 2 Al 4 Si 5 O 18 is a material for diesel particulate filters (DPF) with high potential. Its resistance to two simplified model ashes has been tested on single crystals at temperatures up to 1050 °C, which are realistic for use under ‘worst case’ conditions. Single crystals were examined in order to investigate the orientation dependence of attack due to the strongly anisotropic nature of the Cordierite crystal lattice. A mixture of sodium carbonate and silica was used to study the attack of an alkali-rich ash composition and a mixture of the Ca, Mg and Zn orthophosphates to study an ash composed of typical main constituents of ashes found in DPF used in traffic. The sodium-rich ash formed a melt and attacked the Cordierite by dissolving it. No anisotropy in the corrosion was observed, because the attack is controlled by outward diffusion of Mg. A kinetic break occurs in the system, caused by the formation of a Nepheline product layer, slowing down corrosion. A much stronger corrosion of Cordierite occurs by the phosphate mixture at 1050 °C. Excessive melt formation from the ash causes fast dissolution of the substrate with melt saturation within minutes. Anisotropy of the dissolution process could not be detected. The initial kinetics is dominated by saturation effects, which slow down corrosion. The saturated melt attacks Cordierite by reaction processes leading to the formation of new crystalline phases. This process is much slower than the initial dissolution process but may significantly contribute to the destruction of Cordierite substrates if large contact areas between ash melt and Cordierite exist. Additionally, the formation and local growth of crystalline phases causes the extension of faults, which may eventually become critical.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metallurgical Processes and Thermodynamics · High-Temperature Coating Behaviors · Catalytic Processes in Materials Science

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. Considering some thermal applications for cordierite and cordierite–mullite materials
2. Thermal expansion of extruded cordierite ceramics
3. Merkel · 2001
4. Comparison of corrosion resistance of cordierite and silicon carbide diesel particulate filters to combustion products of diesel fuel containing Fe and Ce additives
5. Degradation resistance of silicon carbide diesel particulate filters to diesel fuel ash deposits10.1557/JMR.2004.0373 ↗
6. Agostini L, Borello C, Demaestri PP, Giachello A, De Portu G, Giucciardi S. Effects of sodium and iron on the thermomechanical properties of porous cordierite traps for diesel engines. Presentation at European Ceramic Society 2nd conference; 1991.
7. Frank RW, Hardenberg HO. Reduction of particulate emission from the break-in facilities of a heavy-duty engine plant by means of ceramic monolith traps. SAE-Paper 850268; 1985. p. 1–10.10.4271/850268 ↗
8. Influence of calcium oxide and sodium oxide on the microstructure of cordierite catalyst supports
9. Barris MA, Reinhart SB, Wahlquist FH. The influence of lubricating oil and diesel fuel ash accumulation in an exhaust particulate trap. SAE-Paper 910131; 1991. p. 19–28.10.4271/910131 ↗
10. Experimental analysis for accumulated ash in DPF—effect of high quality low ash oil
11. Givens WA, Buck WH, Jackson A, Kaldor A, Hertzberg A, Moehrmann W, et al. Lube formulation effects on transfer of elements to exhaust after-treatment system components. SAE-Paper 2003-01-3109; 2003. p. 1–15.10.4271/2003-01-3109 ↗
12. Influence of some pollutants on the durability of cordierite filters for diesel cars10.1016/0272-8842(94)90035-3 ↗
13. Rose D, Boger T. Diesel particulate filter durability for Euro 5 and future Euro 6 applications. Presentation at 4th international CTI forum “diesel particulate filter”, Frankfurt; 2007.
14. Reduction of particulate emissions from diesel passenger cars and heavy duty vehicles
15. von Watzdorf HV. Korrosionsbeständigkeit offenporöser Cordierit-Wabenkörper in natriumadditivierten dieselmotorischen Abgasen. PhD/Doctoral thesis. RWTH, Aachen; 1996.
16. Thermal stability of cordierite catalyst supports contaminated by Fe2O3, ZnO and V2O510.1016/0955-2219(94)90036-1 ↗
17. Montanaro L, Negro A. On the effects induced by the accumulation of sodium, iron and cerium, on diesel soot filters. SAE Technical Paper 980540; 1998. p. 139–147.10.4271/980540 ↗
18. Durability of ceramic filters in the presence of some diesel soot oxidation additives10.1016/S0272-8842(98)00051-0 ↗
19. Interaction between some oxides and cordierite10.1016/0955-2219(93)90084-5 ↗
20. Deterioration of cordierite honeycomb structure for diesel emissions control10.1016/0955-2219(94)90110-4 ↗
21. Cutler WA, Merkel GA. A new high temperature ceramic material for diesel particulate filter applications. SAE-Paper 2000-01-2844; 2000. p. 79–87.10.4271/2000-01-2844 ↗
22. Hot-corrosion resistance of Fe–Cr–Al substrate to alkali metals for NOx adsorption
23. Choi B, Kang H, Son G, Hwang C. Thermal aging behavior of SiC substrate in the presence of ash materials and alkali metals. SAE-Paper 2007-01-1939; 2007. p. 1031–1037.10.4271/2007-01-1939 ↗
24. Krutzsch B, Wenninger G, Lindner E, Pabel M. Diesel fuel containing an additive which improves the combustion of soot. United States Patent 5522905; 4 June 1996.
25. Fischer J. Biodiesel und Abgasnachbehandlung. Presentation at 3 FAD-Konferenz “Herausforderung Abgasnachbehandlung für Dieselmotoren”, Dresden; 2005.
26. Polymorphie von Cordierit in natürlichen Mineralien und in Cordieritwerkstoffen
27. Reaction sequence and structural changes in cordierite refractories10.1111/j.1151-2916.1960.tb13667.x ↗
28. New hypotheses on the mechanism of the deterioration of cordierite diesel filters in the presence of metal oxides
29. Molten-salt corrosion of silicon nitride. I. Sodium carbonate10.1111/j.1151-2916.1988.tb05828.x ↗
30. Kinetics and mechanism of corrosion of SiC by molten salts10.1111/j.1151-2916.1986.tb04698.x ↗
31. Levin · 1956
32. Kimura K, Lynskey M, Corrigan ER, Hickman DL, Wang J, Fang HL, et al. Real world study of diesel particulate filter ash accumulation in heavy-duty diesel trucks. SAE-Paper 2006-01-3257; 2006. p. 1–31.10.4271/2006-01-3257 ↗
33. Reactivation of severely aged commercial three-way catalysts by washing with weak EDTA and oxalic acid solutions10.1016/j.apcatb.2006.09.008 ↗
34. Levin · 1969
35. FactSage thermochemical software and databases10.1016/S0364-5916(02)00035-4 ↗
36. Barin · 1993
37. O'Sullivan D, Hampshire S, Pomeroy MJ, Fordham RJ, Murtagh J. Resistance of cordierite diesel particulate filters to corrosion by combustion products of diesel fuel containing ferrocene. Presentation at ISATA, Dublin; 2000.