Microstructural development of liquid-phase-sintered silicon carbide during annealing with uniaxial pressure
Source abstract
Abstract
Abstract β-SiC powders containing 1.1 wt.% α-SiC particles as seeds were hot-pressed at 1800 °C and then annealed at 2000 °C under 25 MPa uniaxial pressure to enhance grain growth. Microstructural development during annealing with pressure was investigated quantitatively and statistically using image analysis. The bimodal grain-thickness distribution in samples annealed with pressure was obtained due to abnormal grain growth of some grains. In situ-toughened microstructure has been developed after 3-h annealing. The grain-thickness and aspect ratio of large grains increase with annealing time, but grain growth comes mainly from increases in thickness after 3-h annealing, owing to the impingement of large gains. Typical flexural strength and fracture toughness of 4-h annealed sample were ∼500 MPa and ∼7.5 MPa m 1/2 , respectively.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. In situ-toughened silicon carbide10.1111/j.1151-2916.1994.tb07024.x ↗
2. Mechanical properties of β-SiC pressureless sintered with Al2O3 additions10.1016/0956-7151(94)90072-8 ↗
3. In situ toughened silicon carbide with Al-B-C additions10.1111/j.1151-2916.1996.tb08145.x ↗
4. High temperature mechanical behaviour of liquid phase sintered silicon carbide10.1016/S0955-2219(97)00163-5 ↗
5. Toughness properties of a silicon carbide with an in situ induced heterogeneous grain structure10.1111/j.1151-2916.1994.tb04637.x ↗
6. Grain growth and fracture toughness of fine-grained silicon carbide ceramics10.1111/j.1151-2916.1995.tb09100.x ↗
7. Microstructural development of silicon carbide containing large seed grains10.1111/j.1151-2916.1997.tb02796.x ↗
8. Microstructure and mechanical properties of self-reinforced alpha-silicon carbide10.1016/S0272-8842(97)00047-3 ↗
9. Microstructure and mechanical properties of α-silicon carbide sintered with yttrium-aluminum garnet and silica10.1111/j.1551-2916.1999.tb20082.x ↗
10. Effect of initial particle size on microstructure of liquid-phase sintered α-silicon carbide10.1016/S0955-2219(99)00239-3 ↗
11. Effect of annealing conditions on microstructural development and phase transformation in silicon carbide10.1111/j.1151-2916.2000.tb01395.x ↗
12. Relationship between microstructure and fracture toughness of toughened silicon carbide ceramics10.1111/j.1151-2916.2001.tb00840.x ↗
13. A critical evaluation of indentation techniques for measuring fracture toughness10.1111/j.1151-2916.1981.tb10320.x ↗
14. Effect of initial α-phase content on microstructure and mechanical properties of sintered silicon carbide10.1111/j.1151-2916.1998.tb02748.x ↗
15. Core/rim structure of liquid-phase-sintered silicon carbide10.1111/j.1151-2916.1993.tb03677.x ↗
16. Abnormal growth of faceted WC grains in a Co liquid matrix10.1007/BF02652373 ↗
17. Effect of heating rate on the exaggerated grain growth behavior of β-Si3N410.1016/S0167-577X(97)00018-9 ↗
18. Stress thickening creep in superplastic silicon nitride10.1111/j.1151-2916.1992.tb05540.x ↗
19. Diffusion models for hot pressing with surface energy and pressure effects as driving force10.1063/1.1658543 ↗
20. Coarsening in liquid-phase-sintered α-SiC10.1016/S1359-6454(98)00371-1 ↗
21. Crack-growth resistance-curve behavior in silicon carbide small versus long cracks10.1111/j.1151-2916.1997.tb03115.x ↗