journal article·2018-01Open access

Contact damage resistant SiC/graphene nanofiller composites

Manuel Belmonte, Pilar Miranzo, M. Isabel Osendi

Abstract

The short-crack domain and contact damage resistances of silicon carbide (SiC) ceramics containing graphene fillers (graphene nanoplatelets -GNPs- or reduced graphene oxide sheets -rGOs) are investigated by performing Hertzian contact tests. A progressive deviation from the linear Hertzian elastic response with increasing graphene content takes place, the composite containing 20 vol.% GNPs being the most deformable material. When adding increasing amounts of GNPs, the damage beneath the contact zone turns from well-defined cone cracks of monolithic SiC to a widespread subsurface damage where microcracks are generated due to the matrix/graphene interface debonding by a shear faulting process. This mechanism enhances the contact damage resistance of the composites, redistributing the stresses at the contact and limiting the long-crack formation. The composite containing 5 vol.% rGOs fully precludes the cone cracks development and enlarges the quasi-plastic damage zone, extraordinarily enhancing the contact damage resistance that approaches to that of a ductile material.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Graphene research and applications · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (20)

Show source-provided references
1. Schwetz · 2008
2. Indentation fatigue10.1080/01418619308219382 ↗
3. Indentation of ceramics with spheres: a century after Hertz10.1111/j.1151-2916.1998.tb02580.x ↗
4. Making ceramics ductile10.1126/science.263.5150.1114 ↗
5. Contact fatigue of a silicon carbide with a heterogeneous grain structure10.1111/j.1151-2916.1995.tb08834.x ↗
6. Enhanced machinability of silicon carbide via microstructural design10.1111/j.1151-2916.1995.tb08386.x ↗
7. Contact damage of silicon carbide/boron nitride nanocomposites10.1111/j.1551-2916.2007.01894.x ↗
8. Fabrication of machinable silicon carbide-boron nitride ceramic nanocomposites10.1111/j.1551-2916.2004.00565.x ↗
9. Contact-damage-resistant ceramic/single-wall carbon nanotubes and ceramic/graphite composites10.1038/nmat1161 ↗
10. Enhanced tribological performance of silicon nitride-based materials by adding carbon nanotubes10.1111/j.1551-2916.2011.04391.x ↗
11. From bulk to cellular structures: a review on ceramic/graphene filler composites10.1016/j.jeurceramsoc.2017.03.016 ↗
12. Contact-mechanical properties at pre-creep temperatures of fine-grained graphene/SiC composites prepared in situ by spark-plasma sintering10.1016/j.jeurceramsoc.2013.11.003 ↗
13. Effect of lateral size of graphene nano-sheets on the mechanical properties and machinability of alumina nano-composites10.1016/j.ceramint.2016.01.160 ↗
14. Toughened and strengthened silicon carbide ceramics by adding graphene-based fillers10.1016/j.scriptamat.2015.10.023 ↗
15. Enhanced electrical conductivity of silicon carbide ceramics by addition of graphene nanoplatelets10.1016/j.jeurceramsoc.2015.03.044 ↗
16. Multifunctional silicon nitride/graphene based nanostructures composites
17. Tribological performance under dry sliding conditions of graphene/silicon carbide composites10.1016/j.jeurceramsoc.2015.09.040 ↗
18. In situ processing of electrically conducting graphene/SiC nanocomposites10.1016/j.jeurceramsoc.2013.01.021 ↗
19. Stress analysis of contact deformation in quasi-plastic ceramics10.1111/j.1151-2916.1996.tb09023.x ↗
20. Tools (geometry and material) and tool wear