Abstract SiC-30vol%VB 2 ceramic composite was pressureless densified at 2150 °C with excess B 4 C and C as sintering aids after in-situ formation of VB 2 in SiC matrix. The sintered bulk gained a considerably high fracture toughness of 7.0 ± 0.4 MPa m 1/2 , which was ∼2.4 times as high as that of the monolithic SiC ceramic, owing to the existences of weak heterophase boundaries, thermal residual stresses and microcracks. Meanwhile, since the VB 2 particle has a lower elastic modulus than SiC and significantly suppressed the grain growth of SiC, the composite exhibited a high flexural strength of 458 ± 36 MPa and a relatively low Young’s modulus of 356 ± 6 GPa, resulting in an increase of ∼59.3% in mechanical strain tolerance (1.29 × 10 −3 ) compared with that of single-phase SiC ceramic. Besides, the residual stresses and microcracks also induced a lower-than-expected Vickers hardness of 20.8 ± 0.5 GPa in the composite.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · MXene and MAX Phase Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (27)

Show source-provided references
1. High temperature strength of silicon carbide sintered with 1wt.% aluminum nitride and lutetium oxide10.1016/j.jeurceramsoc.2012.09.005 ↗
2. Effect of intergranular phase chemistry on the sliding-wear resistance of pressureless liquid-phase-sintered alpha-SiC10.1016/j.jeurceramsoc.2011.09.011 ↗
3. Effect of the sintering additive content on the protective passive oxidation behaviour of pressureless liquid-phase-sintered SiC10.1016/j.jeurceramsoc.2012.05.004 ↗
4. Tribological characterization of silicon carbide and carbon materials10.1016/j.jeurceramsoc.2014.10.038 ↗
5. Sintering of in-situ synthesized SiC-TiB2 composites with improved fracture toughness10.1111/j.1151-2916.1992.tb05600.x ↗
6. Microcracking and R-curve behavior in SiC-TiB2 composites10.1016/0956-7151(92)90475-T ↗
7. In-situ synthesized TiB2 toughened SiC10.1016/0955-2219(95)00116-6 ↗
8. Silicon carbide-titanium diboride ceramic composites10.1016/j.jeurceramsoc.2013.03.031 ↗
9. SiC-TiC and SiC-TiB2 composites densified by liquid-phase sintering10.1007/BF00354442 ↗
10. Improvements in mechanical properties in SiC by the addition of TiC particles10.1111/j.1151-2916.1984.tb19174.x ↗
11. Microstructure and mechanical properties of hot-pressed SiC-TiC composites10.1007/BF01184969 ↗
12. Elastic properties and microcracking behavior of particulate titanium diboride-silicon carbide composites10.1111/j.1151-2916.1997.tb02886.x ↗
13. Reaction mechanism and microstructure development of strain tolerant in situ SiC-BN composites10.1016/S1359-6454(00)00297-4 ↗
14. In situ reaction synthesis of silicon carbide-boron nitride composites10.1111/j.1151-2916.2001.tb00863.x ↗
15. Thermal expansion studies on the group IV-VII transition metal diborides10.1016/0022-5088(88)90219-6 ↗
16. Samsonov · 1964
17. Martienssen · 2005
18. Sintering of silicon carbide powder containing metal boride10.2109/jcersj.111.878 ↗
19. SiC matrix composites containing transition metal boride particulates internally synthesised by carbothermal reaction10.1007/BF00557141 ↗
20. Pure single-crystal rutile vanadium dioxide powders: synthesis, mechanism and phase-transformation property10.1021/jp8073688 ↗
21. A critical evaluation of indentation techniques for measuring fracture toughness: I direct crack measurements10.1111/j.1151-2916.1981.tb10320.x ↗
22. Deep level transient spectroscopic and Hall effect investigation of the position of the vanadium acceptor level in 4H and 6H SiC10.1063/1.115640 ↗
23. Doping peculiarities of SiC epitaxial layers grown by sublimation sandwich-method10.1007/978-3-642-84402-7_50 ↗
24. Kingery · 1976
25. Samsonov · 1980
26. Sintering of silicon carbide I. Effect of carbon10.1016/S0272-8842(02)00117-7 ↗
27. Thermal expansion and thermal expansion anisotropy of SiC polytypes10.1111/j.1151-2916.1987.tb05673.x ↗