The water vapor hot gas corrosion of MGC materials with Al2O3 as a phase constituent in a combustion atmosphere
Source abstract
Abstract
Abstract The hot gas corrosion behavior of two melt grown composite materials (Al 2 O 3 /YAG and Al 2 O 3 /GAP) in comparison with alumina and sapphire was investigated. The tests were performed in a high temperature burner rig at 1450 °C, a total pressure of 1 atm with a water vapor partial pressure of 0.28 atm, a gas flow velocity of 100 m/s and exposure times for up to 450 h. In comparison to sapphire, alumina showed comparable corrosion rates and similar corrosion traces on the corroded surface. The Al 2 O 3 /YAG and Al 2 O 3 /GAP melt grown composite materials were subject to degradation due to the corrosion attack of the alumina phase. This was the consequence of the formation and evaporation of volatile hydroxides (e.g., Al(OH) 3 ). In comparison to polycrystalline alumina the YAG or GAP showed a higher corrosion stability, which causes the formation of a porous YAG or GAP surface layer with increasing corrosion time. For short corrosion times, the porous YAG or GAP surface layer led to a small corrosion protection of the material. After longer corrosion times a switch to linear corrosion kinetics was observed due to spalling of the porous corrosion layer. The corrosion rates for long exposure times were comparable to bulk alumina or sapphire. In principle the regarded polycrystalline and single crystalline materials showed the same corrosion behavior.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Magnesium Oxide Properties and Applications · Glass properties and applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (17)
Show source-provided references
1. Ultra-high temperature compressive creep behavior of in situ single-crystal oxide Al2O3/YAG eutectic composite10.1016/S0955-2219(03)00640-X ↗
2. High temperature strength and thermal stability for melt growth composite10.1016/j.jeurceramsoc.2005.01.030 ↗
3. Fabrication and characterization of MGC components for ultra high efficiency gas turbine
4. Oxidation and volatilization of silica formers in water vapor10.1111/j.1151-2916.2003.tb03459.x ↗
5. Yuri, L., Hisamatsu, T., Etori, Y., and Yamamoto, T., Degradation of silicon carbide in combustion gas flow at high temperature and speed. In Proceedings of ASME Turbo Expo, 2000, ASME Paper 2000-GT-664.10.1115/2000-GT-0664 ↗
6. Corrosion of silicon nitride materials in gas turbine environment10.1016/S0955-2219(02)00143-7 ↗
7. Schenk, B., Strangman, T., Opila, E., Robinson, C., Fox, D., and Klemm, H., et al., Oxidation behavior of prospective silicon nitride materials for advanced microturbine applications. In Proceedings of ASME Turbo Expo, 2001, ASME Paper 2001-GT-0459.10.1115/2001-GT-0459 ↗
8. Corrosion of selected ceramic materials in hot gas environment10.1016/j.jeurceramsoc.2006.01.015 ↗
9. Yuri, I., and Hisamatsu, T., Recession rate prediction for ceramic materials in combustion gas flow. In Proceedings of ASME Turbo Expo, 2003, ASME Paper GT2003-38886.10.1115/GT2003-38886 ↗
10. Alumina volatility in water vapor at elevated temperatures10.1111/j.1551-2916.2004.01701.x ↗
11. SiC recession caused by SiO2 scale volatility under combustion conditions. I. Experimental results and empirical model10.1111/j.1151-2916.1999.tb02004.x ↗
12. Corrosion of a unidirectionally solidified Al2O3/YAG eutectic composite in a combustion environment10.1016/j.jeurceramsoc.2005.01.008 ↗
13. Effect of water vapour in degradation of in-situ single-crystal oxide eutectic composites
14. Nakagawa, N., Ohtsubo, H., Shibata, K., Mitani, A., Shimizu, K., and Waku, Y., High temperature stability of MGC's gas turbine components in combustion gas flow environments. In Proceedings of the ASME Turbo Expo, 2005, ASME Paper GT2005-68658.10.1115/GT2005-68658 ↗
15. High-temperature creep of some single crystal oxides10.1002/9780470313848.ch10 ↗
16. Corrosion behaviour of Al2O3 in static state water vapour environment at high temperature10.1023/B:JMSC.0000044908.23241.e5 ↗
17. The water-vapour hot gas corrosion behavior of Al2O3–Y2O3 Materials, Y2SiO5 and Y3Al5O12-coated alumina in a combustion environment