journal article·2000-07

Influence of annealing on the mechanical properties of SiC–Si composites with sub-micron SiC microstructures

Matthias Wilhelm, Werner Wruss

Publisher page

Abstract

Abstract The influence of annealing temperature (1000, 1100 and 1200°C) on the mechanical properties of SiC–Si composites has been evaluated. Three SiC powders with particle sizes in the range of 0.24 to 0.7 μm were used to produce the composites. Before application the SiC powders were treated with hydrofluoric acid to remove the extent of SiO2. With this treatment a successful infiltration of green-bodies especially produced of SiC powder with a mean particle size of 0.24 μm was possible. The bending strength decreased with decreasing SiC starting particle size as well as with increasing annealing temperature. However, the fracture toughness was independent on SiC starting particle size and annealing temperature. XRD diffraction analysis showed that internal stress, expressed by broadening of XRD peaks, is low and had no effects on the mechanical properties of the composites.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (18)

Show source-provided references
1. Popper, P., The preparation of dense self-bonded silicon carbide. In Special Ceramics. Heywood, 1969, pp. 209–219.
2. Microstructure characterisation of REFEL (reaction-bonded) silicon carbides10.1007/BF00570528 ↗
3. Design techniques for ceramics in fusion reactors10.1016/0029-5493(79)90074-8 ↗
4. Development and processing of injection-moldable reaction-sintered SiC compositions
5. John, B. and Wachtman, J., Structural Ceramics. Vol. 29, Academic Press, 1989, pp. 91–163.
6. Transport of fine-grained β-SiC/liquid Si system10.1111/j.1551-2916.1988.tb00221.x ↗
7. Krauth, A. et al., Ingenieurkeramische Bauteile für Anwendungen in der Energietechnik, Verfahrenstechnik, Metallurgie und Motorenbrau, Keramische Komponenten für Fahrzeug-Gasturbinen III. Springer Verlag, 1984, pp. 647.10.1007/978-3-642-82299-5_30 ↗
8. Microstructural evolution in reaction bonded silicon carbide10.1007/BF00553278 ↗
9. Influence of grain size, free silicon content and temperature on the strength and toughness of reaction-bonded silicon carbide10.1016/0272-8842(94)90042-6 ↗
10. Development of SiC — Si composites with fine-grained SiC microstructures10.1016/S0955-2219(99)00029-1 ↗
11. Forrest, C.W., Kennedy, P. and Shennan, J.V., The fabrication and properties of self-bonded silicon carbide bodies. TRG Report 2053 (S), 1970.
12. Forrest, C., Kennedy, P. and Shennan, J., The fabrication and properties of self-bonded silicon carbide. In Special Ceramics, Vol. 5. Heywood, 1972, pp. 99–123.
13. The use of X-ray diffraction peak-broadening analysis to characterize ground Al2O3 powders10.1007/BF01026322 ↗
14. Conputerprograms for standardless quantitative analysis of minerals using the full power diffraction profile10.1017/S0885715600016778 ↗
15. (reaction bonded) silicon carbides: authors' reply10.1007/BF00550606 ↗
16. Discussion of microstructural characterization of REFEL (reaction bonded) silicon carbides10.1007/BF00688437 ↗
17. Jepps · Progress in Crystal Growth & Characterization · 1983 · 7 · 25910.1016/0146-3535(83)90034-5 ↗
18. Microstructural evolution in reaction bonded silicon carbide10.1007/BF00553278 ↗