Influence of WC particles on the microstructural and mechanical properties of 3mol% Y2O3 stabilized ZrO2 matrix composites produced by hot pressing

N. Ünal, F. Kern, M.L. Öveçoğlu, R. Gadow

Publisher page

Abstract

Abstract Yttria stabilized polycrystalline tetragonal zirconia (Y-TZP)–tungsten carbide (WC) composites were fabricated by hot pressing. Yttria (Y2O3) stabilizer content was kept at 3 mol% to ensure the phase structure of the Y-TZP composites to be tetragonal. To increase the moderate hardness of the 3 mol% Y2O3 added TZP structure, hard WC particles were added with various proportions up to 40 vol%. The TZP/WC composites were sintered at different sintering temperatures between 1450 and 1550 °C. The mechanical and microstructural properties of the resulting composites as well as the phase compositions were investigated. Reciprocating pin-on-disk tests were carried out to determine the wear behavior of the Y-TZP/WC composites. Using bi-modal WC reinforcement, the performance of the composite against wear was improved. Using dry wear sliding conditions under 55 N normal load and 45 km sliding distance, the worn volume of the 75 vol% nanosized – WC distributed 3Y-TZP/40WC composite was about 0.003 mm3.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced materials and composites · Advanced ceramic materials synthesis · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
1. High toughness ceramics and ceramic composites10.1016/0079-6425(89)90005-4 ↗
2. Perspective on the development of high-toughness ceramics10.1111/j.1151-2916.1990.tb06493.x ↗
3. Transformation-toughened ZrO2: correlations between grain size control and composition in the system ZrO2–Y2O310.1111/j.1151-2916.1986.tb07416.x ↗
4. Influence of fracture toughness on the wear resistance of yttria-doped zirconium oxide10.1111/j.1151-2916.1989.tb06110.x ↗
5. ZrO2–WC nanocomposites with superior properties10.1016/j.jeurceramsoc.2006.05.028 ↗
6. Computational investigation of microstructural effects on abrasive wear of composite materials10.1016/j.wear.2005.02.017 ↗
7. National Materials Advisory Board · 1988
8. Correlation of abrasive wear with microstructure and mechanical properties of pressure die-case aluminum hard-particle composite10.1007/s11661-001-0080-3 ↗
9. Effect of size and volume fraction of particulates on the sliding wear resistance of CuSn composites10.1016/S0043-1648(01)00823-7 ↗
10. How microstructure affects abrasive wear resistance
11. Microstructure and wear characteristics of rapidly solidified Al–Pb–Cu alloys10.1016/S0921-5093(00)00813-3 ↗
12. DIN EN ISO 6872 · 1998
13. A fracture mechanics analysis of indentation-induced Palmqvist crack in ceramics10.1007/BF00725625 ↗
14. Properties of zirconia–tungsten carbide composites produced by hot pressing
15. Calister · 1994
16. Dowling · 1993
17. Reed-Hill · 1994
18. Grain size dependence of toughness and transformability of 2mol-% Y-TZP ceramics10.1007/BF01742233 ↗
19. Effect of heat treatment on grain size, phase assemblage, and mechanical properties of 3mol% Y-TZP10.1111/j.1151-2916.1996.tb08980.x ↗
20. Sintering, microstructure and mechanical properties of commercial Y-TZPs10.1007/BF01152158 ↗
21. Powder Diffraction Files. Card No. 81-1544. Database edition. International Centre for Diffaction Data (ICDD). Newton Square, PA 19073-3273, USA; 2006.
22. Powder Diffraction Files. Card No. 51-0939. Database edition. International Centre for Diffaction Data (ICDD). Newton Square, PA 19073-3273, USA; 2006.
23. Powder Diffraction Files. Card No. 71-6322. Database edition. International Centre for Diffaction Data (ICDD). Newton Square, PA 19073-3273, USA; 2006.
24. Haberko · 1998
25. Weimer · 1997
26. Pedzich · 1996 · 379
27. Toughening mechanisms in the TZP–WC particulate composites10.4028/www.scientific.net/KEM.132-136.2076 ↗
28. Zhan · J Mater Sci · 1996 · 31 · 290310.1007/BF00356000 ↗
29. Transformation toughening10.1007/BF00809059 ↗
30. The wear of metals under unlubricated conditions10.1098/rspa.1956.0144 ↗
31. Bhushan B. Modern tribology handbook. vol. 1. CRC Press, Boca Raton, Florida; 2000.10.1201/9780849377877 ↗
32. Sliding wear of electrically conductive ZrO2–WC composites against WC–Co cemented carbide10.1007/s11249-008-9326-1 ↗
33. The TZP matrix—WC particulate composites