Long term oxidation behaviour of liquid phase pressureless sintered SiC–AlN ceramics obtained without powder bed
Source abstract
Abstract
Abstract This paper describes the results of the investigation of the oxidation behaviour of 50 wt.% SiC–50 wt.%AlN composites obtained by means of pressureless sintering with Y 2 O 3 as sintering-aid and without using a powder bed to limit the weight loss. Sintered bodies show high density (>98%T.D.) and the microstructure reveals a matrix composed by SiC–AlN solid solution with Y 10 Al 2 Si 3 O 18 N 4 as grain boundary phase. This material exhibits a parabolic oxidation kinetic in the temperature range 1200–1500 °C. Long term oxidation (200 h) induces the formation of a protective oxide scale, composed by mullite, cristobalite and yttrium disilicide, up to 1400 °C. At higher temperature (1500 °C), SiC oxidation behaviour changes from “passive” to “active” and the oxide layer consequently shows porosity due to the formation of gaseous species like SiO and CO.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · MXene and MAX Phase Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. New materials in the Si–C–Al–O–N and related system10.1038/275434a0 ↗
2. Composition and properties of hot-pressed SiC–AlN solid solution10.1111/j.1151-2916.1982.tb10429.x ↗
3. Fabrication and characteristics of SiC–AlN alloys10.1007/BF00586311 ↗
4. High temperature creep of SiC densified using a transient liquid phase10.1557/JMR.1991.1945 ↗
5. Phase relationship in the silicon carbide-aluminum nitride system10.1111/j.1151-2916.1988.tb07541.x ↗
6. Gas pressure sintering of SiC–AlN composites in nitrogen atmosphere10.1016/S0272-8842(01)00070-0 ↗
7. Fabrication, microstructure and properties of SiC–AlN ceramic alloys10.1002/9780470313008.ch39 ↗
8. Phase separation and toughening of SiC–AlN solid-solution ceramics10.1007/BF00353191 ↗
9. Pressureless sintering and high-temperature strength of SiC–AlN ceramics10.2109/jcersj.102.727 ↗
10. Properties of liquid phase pressureless sintered SiC-based materials obtained without powder bed
11. Microstructure and mechanical properties of hot-pressed silicon carbide-aluminum nitride composition10.1111/j.1151-2916.1992.tb08182.x ↗
12. The SiC–AlN system: influence of elaboration routes on the solid solution formation and its mechanical properties10.1016/0272-8842(91)90038-2 ↗
13. Microstructure and high-temperature property of reaction HIP-sintered SiC–AlN ceramic alloys10.2320/matertrans1989.37.807 ↗
14. Effect of a-SiC on the microstructure and toughening of hot-pressed SiC–AlN solid solution10.1023/A:1004743230570 ↗
15. Features of corrosion resistance of AlN–SiC ceramics in air up to 1600°C10.1016/S0955-2219(98)00240-4 ↗
16. Oxidation behaviour of pressureless sintered AlN–SiC composite10.1023/B:JMSC.0000047539.40056.1a ↗
17. SiC–AlN particulate composite10.1016/S0955-2219(98)00280-5 ↗
18. Effect of weight loss on liquid-phase-sintered silicon carbide10.1111/j.1151-2916.1997.tb02945.x ↗
19. Liquid-phase sintered SiC ceramics with oxynitride addittives
20. Microstructural changes in liquid-phase-sintered silicon carbide during creep in an oxidizing environment10.1111/j.1151-2916.2003.tb03328.x ↗
21. Compositional identification of the intergranular phase in liquid phase sintered SiC10.1016/S0955-2219(02)00006-7 ↗
22. Formation of solid solutions between SiC and AlN during liquid-phase sintering10.1016/S0167-577X(96)00110-3 ↗
23. High-temperature corrosion of AlN-based composite ceramic in air and in combustion products of commercial fuel. I. Corrosion of ceramic composites in the AlN-SiC system in air and in combustion products of kerosene and diesel fuel10.1023/B:PMMC.0000035707.58363.f5 ↗
24. Oxidation behaviour of liquid-phase sintered silicon carbide with aluminium nitride and rare-earth oxides (Re2O3, where Re=Y, Er, Yb)10.1111/j.1151-2916.2002.tb00448.x ↗
25. Oxidation and microhardness of SiC–AlN composite at high temperature10.1016/S0025-5408(97)00200-6 ↗
26. Thermodynamics and kinetics of oxidation of hot-pressed silicon nitride10.1007/BF00540931 ↗
27. Some new perspective on oxidation of silicon carbide and silicon nitride10.1111/j.1151-2916.1991.tb04348.x ↗
28. Effect of rare-earth cation additions on the high temperature oxidation behaviour of LPS-SiC10.1016/j.msea.2003.11.037 ↗
29. Mullite based oxidation protection for SiC–C/C composites in air at temperatures up to 1900K10.1016/S0955-2219(98)00242-8 ↗
30. High-temperature effects in the fracture mechanical behaviour of silicon carbide liquid-phase sintered with AlN–Y2O3 addittives10.1016/S0955-2219(00)00317-4 ↗
31. Silica to silicon: key carbothermic reactions and kinetics10.1111/j.1151-2916.1990.tb09820.x ↗
32. The high-temperature oxidation, reduction, and volatilization reactions of silica and silicon carbide10.1007/BF00613092 ↗
33. Oxidation behaviour of silicon carbide10.1111/j.1151-2916.1958.tb12932.x ↗
34. Thermal oxidation of Al2O3–SiC whiskers composites: mechanism and kinetics
35. Oxidation behaviour of SiC-whisker-reinforced-alumina-airconia composites10.1111/j.1151-2916.1991.tb07790.x ↗
36. Formation of beta-SiAlON as an intermediate oxidation product of SiC–AlN ceramics10.1111/j.1151-2916.1995.tb08051.x ↗