journal article·2017-11

Degradation evaluation of Si 3 N 4 ceramic surface layer in contact with molten Al using microcantilever beam specimens

Saho Fujita, Junichi Tatami, Tsukaho Yahagi, Takuma Takahashi, Motoyuki Iijima

Publisher page

Abstract

Abstract Although Si3N4 ceramics are often utilized as structural components in the Al casting industry due to their excellent properties, they occasionally suffer breakage after long-term use. In this study, the bending strength, fracture toughness, and Young’s modulus in the vicinity of the Si3N4 ceramic surfaces after contact with molten Al were evaluated using microcantilever beam specimens, which were fabricated using a focused ion beam technique. Fracture testing of the specimens was carried out by nanoindentation. The bending strength of the ceramic surface before and after contact with molten Al was 5.89 ± 1.33 and 3.03 ± 0.28 GPa, respectively. The fracture toughness of the corroded layer in Si3N4 ceramics also decreased compared to that of the polished surface. Using fractography by observation with scanning electron microscopy, it was shown that changes in the grain boundary glassy phase resulted in the degradation of strength and fracture toughness.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced Surface Polishing Techniques · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (29)

Show source-provided references
1. Dense silicon nitride10.1179/pom.1961.4.8.011 ↗
2. Aluminum nitride and silicon nitride for high temperature gas turbine engines10.4271/740237 ↗
3. Pressure sintering of Si3N410.1007/BF02396645 ↗
4. Pressureless sintering of Si3N410.1007/BF00541399 ↗
5. High-strength silicon nitride ceramics obtained by grain-boundary crystallization10.1007/BF02403951 ↗
6. A tough SiAlON ceramic based on alpha Si3N4 with a whisker-like microstructure10.1038/39542 ↗
7. Strength retention in hot-pressed Si3N4 ceramics with Lu2O3 additives after oxidation exposure in air at 1500°C10.1111/j.1151-2916.2002.tb00319.x ↗
8. Fracture resistance and contact damage of TiN particle reinforced Si3N4 ceramics10.2109/jcersj.114.1049 ↗
9. Fabrication and wear properties of TiN nanoparticle-dispersed Si3N4 ceramics10.2109/jcersj2.116.749 ↗
10. Rapid fabrication of Si3N4 ceramics by reaction-bonding and pressureless sintering10.1016/j.jeurceramsoc.2016.06.007 ↗
11. Wear damage of Si3N4-graphene nanocomposites at room and elevated temperatures10.1016/j.jeurceramsoc.2014.02.025 ↗
12. Effect of crystallizing the grain-boundary glass phase on the high temperature strength of hot-pressed Si3N410.1111/j.1151-2916.1975.tb11488.x ↗
13. Development of nitrogen ceramics
14. Analysis of sintering behavior of silicon nitride based on master sintering curve theory of liquid phase sintering10.2109/jcersj2.15291 ↗
15. Fabrication of c-axis oriented Si3N4 ceramics using multilayered-graphene-coated β-Si3N4 seeds and their orientation in an innovative low magnetic field10.1016/j.apt.2016.07.006 ↗
16. Application of silicon nitride to molten aluminum
17. Measurement of hardness and elastic modulus by instrumented indentation: advances in understanding and refinements to methodrogy10.1557/jmr.2004.19.1.3 ↗
18. Nanoindentation induced deformation anisotropy in β-Si3N4 ceramic crystals10.1016/j.jeurceramsoc.2015.11.028 ↗
19. Deformation characteristics of WC micropillars10.1016/j.jeurceramsoc.2014.05.045 ↗
20. Local fracture toughness of Si3N4 ceramics measured using single-edge notched microcantilever beam specimens10.1111/jace.13391 ↗
21. Large increase in fracture resistance of stishovite with crack extension less than one micrometer10.1038/srep10993 ↗
22. Microcantilever investigation of fracture toughness and subcritical growth on the scale of the microstructure in Al2O310.1016/j.jeurceramsoc.2015.08.023 ↗
23. Analysis of stresses and strains near the end of a crack traversing a plate10.1115/1.4011547 ↗
24. Reaction between SiO2 and molten aluminum
25. Processing, microstructure, and properties of Co-continuous alumina-aluminum composites10.1016/0921-5093(94)06510-1 ↗
26. Thin-film studies of the reduction of SiO2 by Al10.1111/j.1151-2916.1973.tb12449.x ↗
27. Microstructure of Al/Al2O3 composite bodies obtained by reaction between SiO2 and molten Al at temperatures ranging from 1073 to 1473K10.2320/matertrans1989.41.399 ↗
28. The effect of microcracks on the elastic moduli of brittle materials10.1007/BF00721363 ↗
29. Preparation and mechanical properties of Y-Si-Al-O-N glass