Preparation of SiC layer with sub-micro grain structure in TRISO particles by spouted bed CVD
Source abstract
Abstract
Abstract The previous studies showed that the SiC layer with sub-micro grain structure can prevent fission products release more effectively. Usually, the silicon carbide (SiC) layer in TRISO (Tristructural isotropic) particles was deposited at 1500–1600 °C by spouted bed chemical vapor deposition (CVD) from methyltrichlorosilane in H2 environment. It has grain size in micro scale (1–10 μm). In this work, we proposed a novel method for preparation of sub-micro grained SiC layer by adjusting the deposition parameters. The as-prepared SiC layer had grain size about 200 nm and pure phase (β-SiC). The fined grain SiC layer also exhibited higher mechanical property than SiC layer with larger grain size.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Silicon Carbide Semiconductor Technologies · Advanced ceramic materials synthesis · Ion-surface interactions and analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. Comparison study of silicon carbide coatings produced at different deposition conditions with use of high temperature nanoindentation10.1007/s10853-016-0476-5 ↗
2. Radiation effects in SiC for nuclear structural applications10.1016/j.cossms.2012.03.005 ↗
3. Microstructure and ablative properties of Si-SiC coating prepared by spark plasma sintering10.1016/j.ceramint.2018.02.033 ↗
4. Current status and future development of coated fuel particles for high temperature gas-cooled reactors10.1016/j.pnucene.2010.10.003 ↗
5. Diffusion of fission products and radiation damage in SiC10.1088/0022-3727/46/47/473001 ↗
6. Key differences in the fabrication, irradiation and high temperature accident testing of US and German TRISO-coated particle fuel, and their implications on fuel performance10.1016/S0029-5493(03)00033-5 ↗
7. Effect of microstructure on the resilience of Silicon Carbide to palladium attack10.1111/j.1551-2916.2010.04005.x ↗
8. Microstructure of TRISO coated particles from the AGR-1 experiment: SiC grain size and grain boundary character10.1016/j.jnucmat.2012.08.052 ↗
9. Ag diffusion in SiC high-energy grain boundaries: kinetic Monte Carlo study with first-principle calculations10.1016/j.commatsci.2016.04.027 ↗
10. Fission products silver, palladium, and cadmium identification in neutron-irradiated SiC TRISO particles using a Cs-Corrected HRTEM10.1016/j.jnucmat.2016.04.010 ↗
11. Recent advances on understanding the origin of superhardness in nanocomposite coatings: a critical review10.1007/s10853-006-6577-9 ↗
12. TRISO coated fuel particles with enhanced SiC properties10.1016/j.jnucmat.2009.03.013 ↗
13. Preparation of fine grained SiC layer by fluidized bed chemical vapor deposition with pulsed propylene10.1111/jace.14281 ↗
14. Control of stoichiometry, microstructure, and mechanical properties in SiC coatings produced by fluidized bed chemical vapor deposition10.1557/JMR.2008.0220 ↗
15. CVD of SiC from methyltrichlorosilane part II: composition of the gas phase and the deposit
16. Microstructure of SiC deposited from methyltrichlorosilane10.1016/S0955-2219(02)00364-3 ↗
17. On the homogeneous chemistry of the thermal decomposition of methyltrichlorosilane
18. Growth characteristics of CVD beta-silicon carbide
19. The effect of input gas ratio on the growth behavior of chemical vapor deposited SiC films10.1023/A:1017508205412 ↗
20. CVD of SiC from methyltrichlorosilane part I deposition rates
21. Analytics of CVD processes in the deposition of SiC by methyltrichlorosilane10.1007/s006040070095 ↗
22. Sintering of silicon carbideI. Effect of carbon10.1016/S0272-8842(02)00117-7 ↗
23. Effects of thermal treatment on the mechanical integrity of silicon carbide in HTR fuel up to 2200°C10.1016/j.jnucmat.2014.03.039 ↗
24. Nanoscale engineering of radiation tolerant silicon carbide10.1039/c2cp42342a ↗
25. Application of Raman microscopy to the analysis of silicon carbide monofilaments10.1023/B:JMSC.0000045606.60263.27 ↗
26. Structural defects in (100) 3C-SiC heteroepitaxy: influence of the buffer layer morphology on generation and propagation of stacking faults and microtwins10.1016/j.diamond.2009.09.012 ↗
27. Growth mechanism and defects of <111>-Oriented β-SiC films deposited by laser chemical vapor deposition10.1111/jace.13248 ↗
28. Silicon carbide polytype characterisation in coated fuel particles by Raman spectroscopy and 29Si magic angle spinning NMR10.1016/j.jnucmat.2012.08.047 ↗
29. Raman scattering in polycrystalline 3C-SiC: influence of stacking faults10.1103/PhysRevB.58.9858 ↗