Effect of matrix modification on tensile mechanical behavior of Tyranno® Si-Ti-C-O fiber-reinforced SiC matrix minicomposite at room and elevated temperatures
Source abstract
Abstract
Abstract The effect of the addition of borosilicate glass powder in the matrix on tensile mechanical behavior in an unidirectional Si-Ti-C-O fiber-reinforced SiC matrix minicomposite fabricated by the polymer infiltration pyrolysis (PIP) process has been studied. Tensile test of the minicomposite is carried out in an argon atmosphere at 298, 1273 and 1573 K. The Si-Ti-C-O/SiC shows a nearly linear tensile load–displacement curve which is similar to a dry fiber bundle independent of test temperature; conversely, the glass-powder-containing Si-Ti-C-O/SiC(g) exhibits a pronounced tensile load–displacement curve with a large nonlinear domain of deformation; however, this nonlinear domain became smaller at 1573 K. The matrix cracking load of Si-Ti-C-O/SiC(g) remained nearly constant at and below 1273 K, and it decreased at 1573 K. The tensile fracture load of the minicomposite is increased remarkably by the addition of a borosilicate glass powder in the matrix, but the increase was larger at and below 1273 K than at 1573 K. This increase of the tensile fracture load was attributed to more effective load transfer at the fiber/matrix interface for the Si-Ti-C-O/SiC(g) than for the Si-Ti-C-O/SiC. Degradation of the increase at 1573 K is due to the interface degradation decreasing interfacial load transfer capacity.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Innovative concrete reinforcement materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (25)
Show source-provided references
1. Mechanical behavior and high-temperature performance of a woven Nicalon/Si-N-C ceramic–matrix composite10.1111/j.1151-2916.1998.tb02550.x ↗
2. Tensile and shear properties of continuous fiber-reinforced SiC™/Al2O3 composites processed by melt oxidation10.1111/j.1151-2916.1995.tb08056.x ↗
3. High-temperature tensile behavior of a boron nitride-coated silicon carbide-fiber glass–ceramic composite10.1111/j.1151-2916.1996.tb08760.x ↗
4. Mechanical properties of coating-free Si-Ti-C-O fiber-reinforced SiC matrix composites10.4028/www.scientific.net/KEM.164-165.133 ↗
5. Thermal stability and chemical corrosion resistance of newly developed continuous Si-Zr-C-O tyranno fiber10.1002/9780470294437.ch12 ↗
6. Improvemennt of Si-Ti(Zr)-C-O fiber and a precursor polymer for high temperature CMC10.1002/9780470314876.ch19 ↗
7. Mechanical behavior of Si-Ti-C-O fiber-bonded ceramic material10.4028/www.scientific.net/KEM.164-165.245 ↗
8. Tensile creep properties of Si-M-C-O(M=Ti or Zr) fibers in air derived from polymer precursors10.4028/www.scientific.net/KEM.164-165.303 ↗
9. Tensile fracture behavior and strength of surface-modified Si-Ti-C-O fiber SiC matrix minicomposites fabricated by PIP process10.1111/j.1151-2916.2000.tb01213.x ↗
10. Strength of a Hi-Nicalon™/silicon-carbide-matrix composite fabricated by the multiple polymer infiltration-pyrolysis process10.1111/j.1151-2916.1999.tb01960.x ↗
11. Temperature dependence of in situ constituent properties of polymer-infiltration-pyrolysis-processed Nicalon™ SiC fiber-reinforced SiC matrix composite10.1557/JMR.2000.0136 ↗
12. Low temperature processing of ceramic woven fabric/ceramic matrix composites10.1111/j.1151-2916.1994.tb06962.x ↗
13. Notch sensitivity of two-dimensional woven fabric SiC–SiC composite fabricated by polymer conversion process10.1023/A:1018551129863 ↗
14. Effect of PIP cycles on fracture behavior in unidirectional SiC fiber-reinforced SiC matrix composite10.1177/096369359900800305 ↗
15. Alumina as a devitrification inhibitor during sintering of borosilicate glass powders10.1111/j.1151-2916.1993.tb08325.x ↗
16. Microstructure and compressive strength of SiC-platelet-reinforced borosilicate composites10.1111/j.1151-2916.1995.tb08048.x ↗
17. Modeling brittle and tough stress–strain behavior in unidirectional ceramic matrix composites10.1016/S1359-6454(98)00041-X ↗
18. On the strength of classical fibers and fiber bundles10.1016/0022-5096(58)90039-5 ↗
19. The concept of filament strength and the Weibull modulus10.1520/JTE11131J ↗
20. Tensile and in situ fiber properties of 3D SiC/SiC-based composite tested at elevated temperature in vacuum and air with and without an oxidation protection system
21. Theory of mechanical properties of ceramic–matrix composites10.1111/j.1151-2916.1991.tb06852.x ↗
22. Effect of pullout on the mechanical properties of ceramic matrix composites10.1016/0001-6160(88)90083-1 ↗
23. Damage and failure in unidirectional ceramic–matrix composites10.1111/j.1151-2916.1992.tb05495.x ↗
24. Temperature dependence of tensile strength for a woven boron-nitride-coated Hi-Nicalon™ SiC fiber-reinforced silicon–carbide–matrix composite10.1111/j.1151-2916.2001.tb00961.x ↗
25. Mechanical behavior at 20° and 1200 °C of Nicalon-silicon-carbide-fiber-reinforced alumina–matrix composites10.1111/j.1151-2916.1997.tb03159.x ↗