Toughening of NiAl–alumina composites by self-constructed compressive surface layers under oxidation

Osami Abe, Satoshi Takata, Yoshitaka Ohwa

Publisher page

Abstract

Abstract Self-constructing protective layers have been fabricated on the surface of NiAl–alumina composites by the oxidation of NiAl to NiAl 2 O 4 . Dense NiAl–alumina materials for these tri-layer composites can be fabricated by a pressure-less sintering of the fine spherical powders derived from the chemically precipitated precursors. The sintered NiAl–alumina materials indicate high fracture toughness (5–6 MPa · m 1/2 ) suitable as the inner layer material sustained in the tensile stress against the compressive surface stress. The volume expansion under the oxidation of NiAl forming NiAl 2 O 4 provides the compressive surface stress exhibiting the resistance to crack propagation. The determined compressive surface stress attaining to 128 MPa agrees with the estimation from the crack propagation, 170 MPa. The fracture toughness of the tri-layer materials containing fine-grained NiAl exceeds 8 MPa·m 1/2 . However, the excess oxidation for the 10 vol.%NiAl composition causes the formation of voids around the layer boundary to degrade the toughness with the relaxed residual stress.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Intermetallics and Advanced Alloy Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (11)

Show source-provided references
1. A simple way to make tough ceramics10.1038/347455a0 ↗
2. Enhanced fracture toughness in layered microcomposites of Ce–ZrO210.1111/j.1151-2916.1991.tb04290.x ↗
3. Preparation of multi-layer composites by combination of centrifugal filter pressing and rate-controlled sintering10.2109/jcersj.102.627 ↗
4. A strong and damage-tolerant oxide laminate10.1111/j.1151-2916.1997.tb03137.x ↗
5. Measurement of residual stress in oxide-ZrO2 three layer composites
6. Damage-resistant SiC–AlN layered composites with surface compressive stresses10.1111/j.1151-2916.1992.tb05550.x ↗
7. Toughening by metallic lamina in nickel/alumina composites10.1111/j.1151-2916.1993.tb03750.x ↗
8. Al2O3–Ni compacts with high strength and fracture toughness10.1111/j.1151-2916.2000.tb01368.x ↗
9. Preparation of NiAl/Al2O3 composites
10. Abe, O. Intelligent alumina–NiAl material having sensitivity to oxidation damages. In Proc. 6th Japan International SAMPE Symposium, ed. Tanimoto, T., Morii, T. Japan Chapter of SAMPE, Tokyo, pp. 237–240, 1999.
11. Thermophys. Properties of Mater., The TPRC Data Series, Vol.13, Thermal Expansion of Nonmetallic Solids. p.176, 1977.