Corrosion of ceramics for vinasse gasification in supercritical water
Source abstract
Abstract
Abstract Supercritical water gasification (SCWG) is a very efficient process to convert wet biomass into energetic gases. Unfortunately, SCWG reactor may strongly corrode due to the addition of temperature, pressure and the presence of corrosive species. In the present paper, the corrosion of various ceramic materials in subcritical and supercritical water (SCW) gasification process was studied in a batch reactor. We compare the corrosion in distillated water and the corrosion in sugar beet slurry that will be gasified under supercritical conditions. The experimental temperatures were 350 °C and 550 °C and the pressure was 25 MPa. Technical ceramics (SiC, alumina, Y stabilized zirconia, Si3N4, BN, aluminosilicate, cordierite-mullite) show poor capability to sustain corrosion whereas graphite and glassy carbon are the highest performance materials in our working conditions.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Subcritical and Supercritical Water Processes · Environmental remediation with nanomaterials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (50)
Show source-provided references
1. Current and foreseeable applications of supercritical water for energy and the environment10.1002/cssc.200700167 ↗
2. Supercritical water for environmental technologies10.1002/jctb.2323 ↗
3. Review of supercritical fluids in inorganic materials science10.1016/j.supflu.2006.03.019 ↗
4. Hydrogen production by biomass gasification in supercritical water: a systematic experimental and analytical study10.1016/j.cattod.2007.05.027 ↗
5. Supercritical water gasification10.1002/bbb.93 ↗
6. Conversion of fern (Pteris vittata L.) biomass from a phytoremediation trial in sub- and supercritical water conditions10.1016/j.biombioe.2010.11.007 ↗
7. Ionic reactions and pyrolysis of glycerol as competing reaction pathways in near- and supercritical water10.1016/S0896-8446(01)00105-X ↗
8. Decomposition of formic acid in supercritical water10.1021/ef9005093 ↗
9. Corrosion in high-temperature and supercritical water and aqueous solutions: a review10.1016/S0896-8446(03)00031-7 ↗
10. Hydrothermal biomass gasification10.1016/j.supflu.2008.10.009 ↗
11. Corrosion control methods in supercritical water oxidation and gasification processes10.1016/j.supflu.2009.08.001 ↗
12. The corrosion of alloy 625 (NiCr22Mo9Nb; 2.4856) in high-temperature, high pressure aqueous solutions of phosphoric acid and oxygen. Corrosion at sub- and supercritical temperatures10.1002/(SICI)1521-4176(199811)49:11<831::AID-MACO831>3.0.CO;2-V ↗
13. The corrosion of nickel-base alloy 625 in sub- and supercritical aqueous solutions of oxygen: a long time study10.1023/A:1006607608189 ↗
14. Factors controlling corrosion in high-temperature aqueous solutions: a contribution to the dissociation and solubility data influencing corrosion processes10.1016/S0896-8446(99)00009-1 ↗
15. The corrosion of nickel-based alloys 625 in sub- and supercritical aqueous solutions of HNO3 in the presence of oxygen10.1023/A:1006628831166 ↗
16. Corrosion behaviour of nickel-based alloys in supercritical water oxidation systems10.1021/ie000124k ↗
17. SCC and corrosion evaluations of the F/M steels for a supercritical water reactor10.1016/j.jnucmat.2007.03.168 ↗
18. Influence of process variables on gasification of corn silage in supercritical water10.1021/ie050367i ↗
19. Evaluation of biomass gasification in supercritical water process for hydrogen production10.1016/j.enconman.2004.04.003 ↗
20. Supercritical water oxidation: state of the art10.1002/(SICI)1521-4125(199911)22:11<903::AID-CEAT903>3.0.CO;2-E ↗
21. Corrosion screening test of high performance ceramics in supercritical water containing oxygen and hydrochloric acid10.1016/S0955-2219(96)00072-6 ↗
22. Corrosion of CVD silicon carbide in 500°C supercritical water10.1111/j.1551-2916.2006.01401.x ↗
23. Effect of microstructure on the corrosion of CVD-SiC exposed to supercritical water10.1016/j.jnucmat.2009.08.008 ↗
24. Corrosion of alumina ceramics in acidic aqueous solutions at high temperatures and pressures10.1023/A:1026714218522 ↗
25. Corrosion of zirconia ceramics in acidic solutions at high pressures and temperatures10.1016/S0955-2219(98)00244-1 ↗
26. An anti-corrosive reactor for the decomposition of halogenated hydrocarbons with supercritical water oxidation10.1016/j.supflu.2005.04.001 ↗
27. Low-temperature oxidation of silicon nitride by water in supercritical condition10.1016/0955-2219(96)82256-4 ↗
28. Gasification study of winery waste using a hydrothermal diamond anvil cell10.1016/j.supflu.2010.02.015 ↗
29. Oxidation of ferritic–martensitic alloys T91, HCM12A and HT-9 in supercritical water10.1016/j.jnucmat.2007.05.023 ↗
30. Etude de la formation d’un complexe de surface graphite-eau. Relation avec la réaction d’oxydation10.1016/0008-6223(73)90307-2 ↗
31. Hydrothermal corrosion of nitride and carbide of silicon10.1016/S0254-0584(00)00434-X ↗
32. Corrosion of silicon nitride ceramics under hydrothermal conditions10.1007/BF00543597 ↗
33. Pitting corrosion in CVD SiC at 300°C in deoxygenated high-purity water10.1016/j.jnucmat.2008.03.025 ↗
34. The solubility of quartz in supercritical water10.2475/ajs.263.6.494 ↗
35. The solubility of amorphous silica in water at high temperatures and high pressures
36. Development of a solution model to correlate solubilities of inorganic compounds in water vapour under high temperatures and pressures10.1016/S0896-8446(01)00089-4 ↗
37. Oxidation and corrosion of ceramics and ceramic matrix composites10.1016/S1359-0286(01)00009-2 ↗
38. The solubility equilibrium and the rate of solution of quartz in water at high temperatures and high pressures
39. Quartz solubility in hydrothermal seawater: an experimental study and equation describing quartz solubility for up to 0.5M NaCl solutions10.2475/ajs.291.10.977 ↗
40. Influence of chemical composition on corrosion of alumina in acids and caustic solutions10.1016/0955-2219(92)90102-J ↗
41. Degradation during aging of transformation-toughened ZrO2–Y2O3 materials at 250°C10.1111/j.1151-2916.1986.tb07415.x ↗
42. Aqueous degradation and chemical passivation of yttria-tetragonally-stabilized zirconia at 25°C10.1111/j.1151-2916.2002.tb00288.x ↗
43. Role of H2O on the degradation process of Y-TZP10.1007/BF01756800 ↗
44. Generation-IV nuclear power: a review of the state of the science10.1016/j.enpol.2008.09.059 ↗
45. Effect of temperature on graphite oxidation behavior10.1016/j.nucengdes.2003.11.004 ↗
46. Biomass gasification in near- and super-critical water: status and prospects10.1016/j.biombioe.2005.04.006 ↗
47. A high throughput screening technique for conversion in hot compressed water10.1021/ie030732a ↗
48. SUPCRT92: a software package for calculating the standard molal thermodynamic properties of minerals, gases, aqueous species and reactions from 1 to 5000 bars and 0 to 1000°C10.1016/0098-3004(92)90029-Q ↗
49. Gasification of aqueous biomass in supercritical water: a thermodynamic equilibrium analysis10.1016/j.supflu.2009.10.014 ↗
50. Energetic analysis of gasification of aqueous biomass in supercritical water10.1016/j.biombioe.2010.08.030 ↗