Influence of pyrolysis temperature on fracture response in SiOC based composites reinforced by basalt woven fabric
Source abstract
Abstract
Abstract The fracture resistance of ceramic based composites reinforced by various ceramic fibres can be dramatically enhanced when an efficient fracture mechanism takes place during the crack propagation. Presented work shows an effect of the pyrolysis temperature of the composite matrix on the fracture behaviour of the composite. The matrix is formed from the polysiloxane resin precursor and the reinforcement is a basalt woven fabric. The temperature range under investigation was from 600 °C, where the onset of fracture properties were observed up to 800 °C. Above this temperature basalt fibres suffer by rapid degradation of the microstructure. The optimum stage of the polysiloxane resin transformation maximizing the fracture resistance of the composite was identified. The fractographic analysis of the fracture surfaces revealed the differences in the acting fracture mechanism.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Innovative concrete reinforcement materials · Concrete and Cement Materials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (41)
Show source-provided references
1. A probabilistic-statistical approach to the ultimate failure of ceramic–matrix composites-part I: experimental investigation of 2d woven sic/sic composites10.1016/S0266-3538(01)00224-X ↗
2. Probabilistic-statistical approach to matrix damage and stress–strain behavior of 2-d woven sic/sic ceramic matrix composites10.1016/S0955-2219(98)00119-8 ↗
3. Fracture behaviour and toughness of a plane-woven sic fibre-reinforced sic matrix composite10.1016/0921-5093(96)10170-2 ↗
4. Oxide ceramic matrix/oxide fibre woven fabric composites exhibiting dissipative fracture behaviour10.1016/0010-4361(95)91380-N ↗
5. Polymer impregnation and pyrolysis (PIP) method for the preparation of laminated woven fabric/mullite matrix composites with pseudoductility10.1016/S0955-2219(03)00127-4 ↗
6. Processing and properties of c/si–b–c–n fiber-reinforced ceramic matrix composites prepared by precursor impregnation and pyrolysis10.1016/j.actamat.2007.12.001 ↗
7. Processing of damage-tolerant, oxidation-resistant ceramic matrix composites by a precursor infiltration and pyrolysis method10.1016/0921-5093(94)06513-6 ↗
8. Miracle · 2001
9. Performance of glass fiber reinforced polymer bars under elevated temperatures10.1016/j.compositesb.2012.01.034 ↗
10. Mechanical response of novel sioc glasses to high temperature exposition10.1016/j.jeurceramsoc.2012.07.023 ↗
11. Mechanical property and microstructure evolutions of cf/sioc composites with increasing annealing temperature in reduced pressure environment10.1016/j.ceramint.2011.07.049 ↗
12. Silicon oxycarbide glasses. 1. Preparation and chemistry10.1557/JMR.1991.2716 ↗
13. Silicon oxycarbide glasses. 2. Structure and properties10.1557/JMR.1991.2723 ↗
14. Properties of modified polysiloxane based ceramic matrix for long fibre reinforced composite materials10.1179/174328911X12948334590321 ↗
15. Effect of pyrolysis temperature on the pore structure evolution of polysiloxane-derived ceramics10.1016/j.ceramint.2011.11.033 ↗
16. Preparation and characterization of mesoporous silicon oxycarbide ceramics without free carbon from polysiloxane10.1016/j.jeurceramsoc.2012.10.014 ↗
17. Fiber coating concepts for brittle–matrix composites10.1111/j.1151-2916.1993.tb03749.x ↗
18. Oxidation of bn/nicalon fiber interfaces in ceramic-matrix composites and its effect on fiber strength10.1111/j.1151-2916.1999.tb02271.x ↗
19. Fabrication and characterisation of Ni-coated carbon fibre-reinforced alumina ceramic matrix composites using electrophoretic deposition10.1016/S1359-6454(01)00018-0 ↗
20. The effect of partially carbonized fibers on the mechanical properties of carbon/carbon composites10.1016/j.jmatprotec.2011.08.018 ↗
21. Role of pyrolysis conditions on fracture behaviour of fibre reinforced composites
22. Optimization of sol–gel/pyrolysis routes to silicon oxycarbide glasses10.1016/j.jnoncrysol.2012.06.027 ↗
23. Influence of the organic/inorganic pyrolysis conversion level on mechanical properties of composites with e-glass or basalt fibre reinforcement
24. Relation between mechanical properties and pyrolysis temperature of phenol formaldehyde resin for gas separation membranes
25. Formation of hybrid organic/inorganic composite membranes via partial pyrolysis of poly(dimethyl siloxane)10.1016/S0009-2509(98)00013-X ↗
26. Mechanisms of the pyrolysis of phenolic resin in a carbon/phenolic composite10.1016/0008-6223(95)00092-R ↗
27. Strength, elasticity and failure of composites with pyrolyzed matrices based on polymethylsiloxane resins with optimized ratio of d and t components10.1177/0021998312445591 ↗
28. Partially pyrolyzed composites with basalt fibres – mechanical properties at laboratory and elevated temperatures10.1016/j.compositesa.2009.08.002 ↗
29. Thermal-shock behavior of a Nicalon–fiber-reinforced hybrid glass–ceramic composite10.1016/S0266-3538(01)00096-3 ↗
30. Effect of static pre-loading on fracture toughness of Nicalon (r) fibre glass matrix composite10.1016/j.msea.2003.09.058 ↗
31. Crack resistance curve in glass matrix composite reinforced by long Nicalon (r) fibres10.1007/s10853-007-2317-z ↗
32. Comparison of mechanical properties and structural changes of continuous basalt and glass fibres at elevated temperatures
33. 2007
34. Resonant frequency study of tensile and shear elasticity moduli of carbon fibre reinforced composites (CFRC)10.1016/S0008-6223(00)00071-3 ↗
35. 2006
36. 2010
37. Slice synthesis of a three dimensional “work of fracture” specimen10.1016/0013-7944(75)90059-4 ↗
38. Reliability of the chevron-notch technique for fracture toughness determination in glass10.1016/S0921-5093(02)00612-3 ↗
39. Reliability of the chevron notch technique for fracture toughness determination in glass composites reinforced by continuous fibres10.1016/S1359-6462(00)00601-1 ↗
40. Fracture resistance of hybrid glass matrix composite and its degradation due to thermal ageing and thermal shock
41. Response of inherently brittle materials on higher loading rates10.1016/j.engfracmech.2009.04.014 ↗