journal article·2003-12

Influence of long term oxidation on the microstructure, mechanical and electrical properties of pressureless sintered AlN–SiC–MoSi2 ceramic composites

Kristoffer Krnel, Diletta Sciti, Alida Bellosi

Publisher page

Abstract

The effects of long term oxidation on the microstructural modification and on the electrical resistivity and mechanical strength of a AlN-SiC-MoSi2 electroconductive ceramic composite are presented. The microstructure of the pressureless sintered composite is described and the oxidation behaviour is discussed. The formation of protective mullite layer at temperatures above 1000°C provides good oxidation resistance for use at higher temperatures. At temperatures below 1000°C, the AlN/SiC matrix disables the “pesting” phenomena and strength degradation, despite the fact that at these temperatures MoSi2 oxidizes rapidly. The surface modification induced by oxidation on AlN-SiC-MoSi2 composites do not affect mechanical strength, while the electrical conductivity strongly decreases.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · MXene and MAX Phase Materials · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (22)

Show source-provided references
1. The physical properties of composite materials10.1007/BF02403361 ↗
2. Electrically conductive ceramic composites10.1016/S0167-2738(97)00315-9 ↗
3. High temperature oxidation and pesting of Mo(Si,Al)210.1016/S0921-5093(97)00673-4 ↗
4. Formation and reaction kinetics of Mo and Mo silicides in the preparation of MoSi2/SiC Composites10.1016/S0955-2219(97)00156-8 ↗
5. Fabrication and characterisation of SiC/MoSi2 composites10.1016/S0921-5093(97)00553-4 ↗
6. Processing and properties of MoSi2–SiC and MoSi2–Al2O310.1016/S0921-5093(98)01073-9 ↗
7. Strong monolithic and composite MoSi2 materials by nanostructure design10.1016/S0921-5093(98)01044-2 ↗
8. The AlN–SiC system10.1016/0272-8842(91)90038-2 ↗
9. Investigation of SiC–AlN system: part I. Microstructure and solid solution10.1557/JMR.1995.0651 ↗
10. Low temperature oxidation of fully dense and porous MoSi210.1016/S0921-5093(98)01078-8 ↗
11. Oxidation behaviour of aluminum nitride10.1557/JMR.1993.0565 ↗
12. Low temperature oxidation behavour of a MoSi2-based material10.1016/S0921-5093(98)01071-5 ↗
13. Thermal oxidation kinetics of MoSi2-based powders10.1111/j.1151-2916.1999.tb02156.x ↗
14. Kinetics and products of molybdemun disilicide powder oxidation10.1111/j.1151-2916.2002.tb00124.x ↗
15. Oxidation behaviour of molybdenum silicides and their composites10.1016/S0966-9795(00)00060-1 ↗
16. Effect of third elements on the pesting suppresion of Mo–Si–X intermetallics (X=Al, Ta, Ti, Zr and Y)10.1016/0966-9795(96)00019-2 ↗
17. Oxidation kinetics and composite scale formation in the system Mo(Al,Si)210.1111/j.1151-2916.2002.tb00109.x ↗
18. Features of corrosion resistance of AlN–SiC ceramics in air up to 1600 °C10.1016/S0955-2219(98)00240-4 ↗
19. Pressureless sintering and high-temperature strength of SiC–AlN ceramics10.2109/jcersj.102.727 ↗
20. The intermediate and high-temperature oxidation behaviour of Mo(Si1−xAlx)2 intermetallic alloys10.1016/S0966-9795(96)00068-4 ↗
21. Crack healing behaviour and high-temperature strength of mullite/SiC composite ceramics10.1016/S0955-2219(01)00431-9 ↗
22. Electrical resistivity of transition metal ion doped mullite10.1016/S0955-2219(99)00058-8 ↗