Abstract

The crack initiation load and fracture toughness were characterized as a function of diamond particle content, up to 25 vol%, in silicon oxycarbide glass matrix by means of Vickers indentation and single edge notch beam (SENB) technique, respectively. The larger fracture toughness value of 3.21 ± 0.3 MPa m1/2 was reached for 20 vol% diamond content composites and the value was 4 times higher than that of the unreinforced glass. The addition of diamond particles greatly influenced the crack initiation load, which increased from 2.9 to 49.0 N. The enhancement in the fracture toughness and crack initiation load can be explained by both the intrinsic mechanical properties of diamond (especially the elastic properties; E ∼ 1100 GPa) and the diamond/SiOC glass interfacial bonding. A clear correlation was found between the fracture energy, the reinforced interparticle spacing and the residual stress arising upon cooling due to thermal expansion mismatch between the matrix and the diamond particles.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Diamond and Carbon-based Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. Fracture energy and strength behavior of a sodium borosilicate glass–Al2O3 composite system
2. Proposed fracture theory of a dispersion-strengthened glass matrix10.1111/j.1151-2916.1966.tb13210.x ↗
3. Effect of crystallites on surface damage and fracture behavior of a glass–ceramic10.1111/j.1151-2916.1983.tb10528.x ↗
4. The interaction of a crack front with a second-phase dispersion10.1080/14786437008221068 ↗
5. SiC particle reinforced oxynitride glass: processing and mechanical properties10.1016/S0955-2219(96)00165-3 ↗
6. Critical load for median crack initiation in Vickers indentation of glasses10.1111/j.1151-2916.1982.tb10496.x ↗
7. Surface damage resistance of gel-derived oxycarbide glasses: hardness, toughness, and scratchability10.1111/j.1151-2916.2001.tb00991.x ↗
8. Elastic properties and surface damage resistance of nitrogen-rich (Ca Sr)–Si–O–N glasses10.1016/j.jnoncrysol.2010.07.043 ↗
9. SiOC glass–diamond composites10.1111/j.1551-2916.2011.04921.x ↗
10. Mechanical characterization of a polysiloxane-derived SiOC glass10.1016/j.jeurceramsoc.2006.01.016 ↗
11. Silicon oxycarbide glasses. Part II. Structure and properties10.1557/JMR.1991.2723 ↗
12. Fracture and stiffness characteristics of particulate composites of diamond in zinc sulfide10.1111/j.1151-2916.1990.tb06719.x ↗
13. Theoretical strength and cleavage of diamond10.1103/PhysRevLett.84.5160 ↗
14. Strength, fracture and friction properties of diamond10.1016/0925-9635(95)00362-2 ↗
15. Understanding the mechanical reinforcement of uniformly dispersed multiwalled carbon nanotubes in alumino-borosilicate glass ceramic10.1016/j.actamat.2010.01.001 ↗
16. Mechanical characterization of ZrB2–SiC composites with varying SiC particle sizes10.1111/j.1551-2916.2011.04885.x ↗
17. The role of inclusions in the fracture of ceramic materials10.1007/BF00552831 ↗
18. High temperature behavior of a gel-derived SiOC glass: elasticity and viscosity10.1023/A:1008779915809 ↗
19. Evaluation of KIc of brittle solids by the indentation method with low crack-to-indent ratios10.1007/BF00724706 ↗
20. Calculation of stress intensity factors for SENB specimens by boundary collocation procedure10.2109/jcersj1950.93.1080_479 ↗
21. Srawley · 1976 · vol. 601
22. Indentation deformation/fracture of normal and anomalous glasses10.1016/0022-3093(79)90154-6 ↗
23. Micromechanics of crack nucleation during indentations10.1007/BF00611482 ↗
24. Direct observation and analysis of indentation cracking in glasses and ceramics10.1111/j.1151-2916.1990.tb05119.x ↗
25. Fracture of a brittle particulate composite10.1007/BF00549316 ↗
26. On the Vickers indentation fracture toughness test10.1111/j.1551-2916.2006.01482.x ↗
27. Thermal stability and mechanical properties of SiC particulate-reinforced Si–C–N composites after heating at 2000°C10.1016/j.jeurceramsoc.2009.07.001 ↗
28. Effects of adding SiC powder on the properties of carbon fiber reinforced Si–O–C composites fabricated via precursor pyrolysis10.4028/www.scientific.net/KEM.434-435.54 ↗
29. Fracture behavior of SiC-whisker-reinforced barium aluminosilicate glass–ceramic matrix composites10.1111/j.1151-2916.2001.tb00759.x ↗
30. Determination of subcritical crack growth parameters in polymer-derived SiOC ceramics by biaxial bending tests in water environment10.1111/j.1551-2916.2009.03566.x ↗
31. Hardness, toughness, and brittleness: an indentation analysis10.1111/j.1151-2916.1979.tb19075.x ↗
32. Study of the mechanical properties, toughening and strengthening mechanisms of Si3N4/Si3N4w/TiN nanocomposite ceramic tool materials10.1016/j.actamat.2007.03.016 ↗
33. Determination of fracture toughness and bridging tractions from crack-opening displacement measurements in particulate composites of diamond in zinc sulfide10.1016/0956-7151(94)90049-3 ↗
34. Fracture characteristics of SiC particle reinforced oxynitride glass using chevron-notch three-point bend specimens10.1023/A:1007474415485 ↗
35. Measurement of particle size in opaque bodies
36. R-curve behaviour of Al2O3 ceramics10.1016/0956-7151(90)90188-M ↗
37. Internal stresses in ceramics10.1111/j.1151-2916.1961.tb15475.x ↗
38. Chawla · 1998