journal article·2013-01

Fabrication and characterization of porous ZrO2 with a high volume fraction of fine closed pores

Shinobu Hashimoto, Tomoya Umeda, Kiyoshi Hirao, Naoki Kondo, You Zhou, Hideki Hyuga, Sawao Honda, Yuji Iwamoto

Publisher page

Abstract

Abstract A novel technique for the fabrication of porous ZrO2 with a high volume fraction of fine closed pores was investigated. A partially stabilized ZrO2 (3 mol% Y2O3; Y-PSZ) body, with a 97–99% relative density and containing a small amount of impurities, exhibited a large volume expansion related to the formation of closed pores after heating at 1700 °C for 10 min in N2. These closed pores seemed to mainly form due to the vaporization of hydroxyl apatite: Ca10(OH)2(PO4)6 as an impurity and superplasticity of the ZrO2 during heating. Porous ZrO2 with approximately 24.6% closed pores (total porosity: 26.7%) was successfully fabricated by the addition of 1 mass% SiO2, 1 mass% TiO2, and 1 mass% hydroxyl apatite. The closed pore size and morphology of the resultant porous ZrO2 bodies were investigated, and the formation mechanism of the closed pores was examined on the basis of chemical thermodynamics.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Catalytic Processes in Materials Science · Advancements in Solid Oxide Fuel Cells

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (9)

Show source-provided references
1. Rahaman · 2003
2. Self-setting particle-stabilized foams with hierarchical pore structure10.1016/j.matlet.2010.03.062 ↗
3. Effect of additives on the pore evolution of zirconia based ceramic foams after sintering10.1016/j.jeurceramsoc.2006.08.008 ↗
4. Superplasticity of yttria-stabilized tetragonal ZrO2 polycrystals10.1111/j.1551-2916.1986.tb00026.x ↗
5. Levin · 1964
6. Brain · 1993
7. JANAF thermochemical tables, 3rd ed.
8. Superplasticity in SiO2-containing tetragonal zirconia polycrystal10.1016/0956-716X(93)90196-Y ↗
9. Doping dependence of high temperature plastic flow behavior in TiO2 and GeO2-doped tetragonal ZrO2 polycrystals10.2109/jcersj.114.155 ↗