journal article·2013-09

CO2 laser peeling of Al2O3 ceramic and an application for the polishing of laser cut surfaces

Yinzhou Yan, Lin Li, Tian Long See, Lingfei Ji, Yijian Jiang

Publisher page

Abstract

A laser controlled fracture peeling technique is demonstrated to smooth the Al2O3 ceramic surface without thermal damages. It was found that a chip can be separated and curled from the ceramic surface during a focused CO2 continuous wave (CW) laser dual-scanning. The thickness of the curled chip is similar to 50 mu m and the formed subsurface roughness (R-a approximate to 2 mu m) is close to the surface machined by mechanical breaking (R-a = 1.84 mu m). The chip formation is attributed to the controlled fracture by the residual tensile stress in the recast layer, whereas the chip curling only occurs when the melting depth is shallower than the position of lateral cracks. The peeling technique can be applied to polish the cut surface of laser fusion cutting in ceramics. The polished cut surface (R-a = 2.18 mu m) is free from recast, crack and heat effects. The microstructure is similar to the base material. The material removal rate during polishing is up to 0.125 mm(3)/s. (C) 2013 Elsevier Ltd. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Laser Material Processing Techniques · Advanced Surface Polishing Techniques · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (22)

Show source-provided references
1. Ceramics grinding under the condition of constant pressure10.1016/S0924-0136(02)00636-2 ↗
2. Laser machining of structural ceramics – a review10.1016/j.jeurceramsoc.2008.11.010 ↗
3. Three-dimensional laser machining of structural ceramics10.1016/j.jmapro.2010.01.001 ↗
4. Study of laser carving three-dimensional structures on ceramics: quality controlling and mechanisms10.1016/j.optlastec.2006.10.010 ↗
5. Optimized nanosecond pulsed laser micromachining of Y-TZP ceramics10.1111/j.1551-2916.2007.02163.x ↗
6. Pulsed laser micromachining of yttria-stabilized zirconia dental ceramic for manufacturing10.1111/j.1744-7402.2008.02203.x ↗
7. Nanosecond-laser postprocessing of millisecond-laser-machined zirconia (Y-TZP) surface10.1111/j.1744-7402.2008.02222.x ↗
8. Laser micromachining of zirconia (Y-TZP) ceramics in the picosecond regime and the impact on material strength10.1111/j.1744-7402.2009.02420.x ↗
9. Femtosecond laser micro-structuring of alumina ceramic10.1016/j.apsusc.2005.03.005 ↗
10. Pulsed laser processing of ceramics in water10.1063/1.99591 ↗
11. CO2 laser micromachined crackless through holes of Pyrex 7740 glass10.1016/j.ijmachtools.2010.08.002 ↗
12. Crackless linear through-wafer etching of Pyrex glass using liquid-assisted CO2 laser processing10.1007/s00339-008-4863-x ↗
13. Investigation of underwater laser drilling for brittle substrates10.1016/j.jmatprotec.2008.06.057 ↗
14. CO2 laser underwater machining of deep cavities in alumina10.1016/j.jeurceramsoc.2011.06.015 ↗
15. Controlled separation of brittle materials using a laser
16. The laser shaping of ceramic by a fracture machining technique10.1007/s00170-003-1679-x ↗
17. Laser milling of cavity in ceramic substrate by fracture-machining element technique10.1016/S0924-0136(03)00133-X ↗
18. Machining a smooth surface of ceramic material by laser fracture machining technique10.1016/j.jmatprotec.2004.04.363 ↗
19. Experimental measurement on the absorption coefficients of Al2O3 ceramics to CO2 laser radiation
20. Crack-free cutting of thick and dense ceramics with CO2 laser by single-pass process10.1016/j.optlaseng.2008.04.020 ↗
21. Experimental and theoretical investigation of fibre laser crack-free cutting of thick-section alumina10.1016/j.ijmachtools.2011.08.004 ↗
22. Yan Y, Ji L, Bao Y, Jiang Y. Optimisation of laser close-piercing lapping technique for faster and crack-free cutting of thick-section alumina ceramic. Int J Adv Manuf Tech 2012; available online.