journal article·2012-01

Electrical resistivity of silicon nitride–silicon carbide based ternary composites

Eveline Zschippang, Hagen Klemm, Mathias Herrmann, Kerstin Sempf, Ulrich Guth, Alexander Michaelis

Publisher page

Abstract

Abstract New electrically conductive ternary composites were developed by adding 8 vol.% of ZrN or ZrB 2 to a Si 3 N 4 –SiC matrix. During hot pressing, ZrB 2 reacted with Si 3 N 4 to form ZrSi 2 , ZrN, Si and BN whereas added ZrN did not undergo any reactions in the Si 3 N 4 –SiC–ZrN composite. The composites modified by ZrN or ZrB 2 addition showed a lower resistivity (7 × 10 3 Ω cm and 3 × 10 −1 Ω cm) compared to the matrix (3 × 10 4 Ω cm). Further studies on the grain size distribution and the volume ratio of conducting and non-conducting phases excluded a percolation network of ZrN and ZrSi 2 grains. In fact, doping of SiC grains and modified grain boundaries as a consequence of the formation of liquid phases during sintering are suggested to be the reason for the significantly lower resistivity of materials containing ZrSi 2 . A decrease in the composite resistivity due to a subsequent heat treatment was obtained for all hot-pressed composites.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · MXene and MAX Phase Materials · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (50)

Show source-provided references
1. Silicon nitride for high-temperature applications10.1111/j.1551-2916.2010.03839.x ↗
2. Corrosion of silicon-based ceramics in combustion environments10.1111/j.1151-2916.1993.tb03684.x ↗
3. Long-term stability of nonoxide ceramics in an oxidative environment at 1500 degrees C10.1016/S0955-2219(02)00267-4 ↗
4. Electrical-resistivity of composites10.1111/j.1151-2916.1990.tb07576.x ↗
5. Analytical functions for the dc and ac conductivity of conductor–insulator composites10.1023/A:1009954017351 ↗
6. Influence of particle-size ratio on continuity of aggregates10.1063/1.323560 ↗
7. Influence of particle size on electrical resistivity of compacted mixtures of polymeric and metallic powders10.1063/1.1660071 ↗
8. Percolation study on electrical resistivity of SiC/Si3N4 composites with segregated distribution10.1063/1.367020 ↗
9. An experimental-model for studying the effect of anisotropy on percolative conduction10.1051/jphyslet:019800041022053100 ↗
10. Piezoresistivity of heterogeneous solids10.1063/1.337932 ↗
11. Electrically conductive CNT-dispersed silicon nitride ceramics10.1111/j.1551-2916.2005.00539.x ↗
12. High temperature mechanical properties of Si3N4–MoSi2 and Si3N4–SiC composites with network structures of second phases10.1016/S0921-5093(98)01075-2 ↗
13. Mechanical and electrical-properties of silicon-nitride silicon-carbide nanocomposite material10.1111/j.1151-2916.1991.tb04357.x ↗
14. The effect of different sintering additives on the electrical and oxidation properties of Si3N4–MoSi2 composites10.1016/j.jeurceramsoc.2006.07.009 ↗
15. Properties of silicon-nitride molybdenum dislicide particulate ceramic composites10.1111/j.1151-2916.1993.tb04030.x ↗
16. MoSi2–Si3N4 composites: Influence of starting materials and fabrication route on electrical and mechanical properties10.1016/j.jeurceramsoc.2008.12.015 ↗
17. Microstructure and properties of Si3N4–MoSi2 composites
18. Preparation and properties of TiN–Si3N4 composites10.1016/S0955-2219(03)00218-8 ↗
19. Microstructural characterization of electroconductive Si3N4–TiN composites10.1016/S0167-577X(00)00214-7 ↗
20. Micro-electrode discharge machining of TiN/Si3N4 composites10.1179/096797800680866 ↗
21. Microstructural characterization and computer simulation of conductivity in Si3N4–TiN composites10.1016/j.jallcom.2003.10.036 ↗
22. Mechanical properties and tribology of Si3N4–TiB2 ceramic composites produced by hot pressing and hot isostatic pressing10.1016/S0955-2219(00)00294-6 ↗
23. Tribological characteristics of Si3N4-based composites in unlubricated sliding against steel ball10.1016/S0921-5093(04)00853-6 ↗
24. Riedel · 2000
25. Development and characterization of SiC(f)/MoSi2–Si3N4(p) hybrid composites10.1016/S0921-5093(98)01046-6 ↗
26. Ionenätzen - Stand und Perspektiven für die Gefügekontrastierung keramischer und metallischer Werkstoffe - I
27. Ionenätzen - Stand und Perspektiven für die Gefügekontrastierung keramischer und metallischer Werkstoffe - II
28. Ionenätzen - Stand und Perspektiven für die Gefügekontrastierung keramischer und metallischer Werkstoffe - III
29. Using the ion beam slope cutting technique for the examination of the microstructure of composite ceramics with extremely different components (BN/TiB2) in the scanning electron microscope
30. Phasencharakterisierung von Pulverpresslingen für Metallschäume mit dem Ionenstrahlpräparationsverfahren
31. Petzow · 2002
32. High-temperature chemistry and oxidation of ZrB2 ceramics containing SiC, Si3N4, Ta5Si3, and TaSi210.1111/j.1551-2916.2008.02420.x ↗
33. Densification and mechanical properties of titanium diboride with silicon nitride as a sintering aid10.1111/j.1151-2916.1999.tb02199.x ↗
34. Densification of ZrB2-based composites and their mechanical and physical properties: a review10.1016/j.jeurceramsoc.2008.11.008 ↗
35. Effect of the addition of silicon nitride on sintering behaviour and microstructure of zirconium diboride10.1016/S1359-6462(01)01229-5 ↗
36. Advances in microstructure and mechanical properties of zirconium diboride based ceramics10.1016/S0921-5093(02)00520-8 ↗
37. The effect of Si3N4 on microstructure, mechanical properties and oxidation resistance of HfB2-based composite10.1177/0021998308098236 ↗
38. The AC conductivity of liquid-phase-sintered silicon carbide10.1111/j.1551-2916.2007.01792.x ↗
39. Interface characteristics affecting electrical properties of Y-doped SiC10.1557/JMR.2003.0365 ↗
40. Doping in cubic silicon-carbide10.1063/1.124285 ↗
41. Thermoelectric properties of P-type silicon carbide. Xvii International Conference on Thermoelectrics
42. Doping of SiC by implantation of boron and aluminum10.1002/1521-396X(199707)162:1<277::AID-PSSA277>3.0.CO;2-C ↗
43. Preparation of p- and n-type SiC-based thermoelectric materials by spark plasma sintering
44. Modification of band gap of beta-SiC by N-doping
45. Reduced electrical resistivity of reaction-sintered SiC by nitrogen doping10.1557/jmr.2008.0144 ↗
46. Characterization of N-Type beta-SiC as a piezoresistor10.1109/16.214734 ↗
47. Phase-relations in the Mo–Si–C system relevant to the processing of MoSi2–SiC composites10.1007/BF02646670 ↗
48. Kim · 2006
49. Resistivities of conductive composites10.1063/1.352350 ↗
50. Zschippang E. unpublished work, 2011.