Foaming inhibition of SiC-containing porcelain ceramics by using Si powders during sintering
Source abstract
Abstract
Abstract Porcelain green bodies were prepared using porcelain stoneware tile powder as the major raw material, with silicon carbide (SiC) and Si powders as additives. These were fired at 1000–1200 °C. The effects of Si powder addition on the microstructure, crystalline phases, and relative density of SiC-containing porcelain bodies were systematically investigated, and the related mechanism was also discussed in detail. The results show that even with the addition of a small amount of Si powder, the foaming degree of the porcelain bodies containing SiC with particle size and content in a wide range can be effectively inhibited. In particular, this effect becomes more pronounced as the Si powder particle size is reduced. It is believed that this work will have important scientific value for the oxidation protection of SiC and the foaming inhibition during the direct recycling of large amounts of polishing porcelain tile residues in the world.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Recycling and utilization of industrial and municipal waste in materials production · Advanced ceramic materials synthesis · Nuclear materials and radiation effects
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (27)
Show source-provided references
1. Pyroplastic deformation of porcelain stoneware tiles: wet vs. dry processing10.1016/j.jeurceramsoc.2016.08.015 ↗
2. Reusing sanitaryware waste products in glazed porcelain tile production10.1016/j.ceramint.2016.11.123 ↗
3. Porcelain tile: almost 30 years of steady scientific-technological evolution10.1016/j.ceramint.2009.11.016 ↗
4. Effect of microstructure on mechanical properties of porcelain stoneware10.1016/j.jeurceramsoc.2010.07.015 ↗
5. Porcelain tile microstructure: implications for polished tile properties10.1016/j.jeurceramsoc.2005.06.002 ↗
6. Dependence of surface porosity on the polishing depth of porcelain stoneware tiles10.1016/j.jeurceramsoc.2010.11.028 ↗
7. Analysis and laboratory simulation of an industrial polishing process for porcelain ceramic tiles10.1016/j.jeurceramsoc.2004.07.005 ↗
8. Effect of silicon carbide particle size and CaO content on foaming properties during firing and microstructure of porcelain ceramics10.1016/j.ceramint.2014.04.153 ↗
9. The reliability of polished porcelain stoneware tiles10.1016/j.jeurceramsoc.2004.05.030 ↗
10. Effects of magnesium oxychloride and silicon carbide additives on the foaming property during firing for porcelain ceramics and their microstructure10.1016/j.jeurceramsoc.2012.04.001 ↗
11. Characterization of cellular ceramics made by porcelain tile residues10.1016/j.msea.2006.07.130 ↗
12. Synthesis, characterization and modeling of new building insulation material using ceramic polishing waste residue10.1016/j.conbuildmat.2015.03.089 ↗
13. Recycling of polished tile waste as a main raw material in porcelain tiles10.1016/j.jclepro.2015.12.064 ↗
14. Oxidation treatments for SiC particles and its compatibility with glass10.1016/j.jeurceramsoc.2006.04.041 ↗
15. Oxidation protection of C/SiC coated carbon/carbon composites with Si-Mo coating at high temperature10.1016/j.corsci.2011.02.024 ↗
16. Evaluation of ceramic coatings on silicon carbide10.1016/0257-8972(89)90042-X ↗
17. Oxidation resistance of SiC-AlN ceramics coated by oxidation-assisted-pack cementation process10.1016/j.jeurceramsoc.2010.10.015 ↗
18. Microstructure and anti-erosion property of SiC coated 2D C/C composites by chemical vapor reaction10.1016/j.ceramint.2016.08.083 ↗
19. Yttrium silicate coatings on chemical vapor deposition-SiC- precoated C/C-SiC: thermodynamic assessment and high-temperature investigation10.1111/j.1551-2916.2005.00077.x ↗
20. A novel laser technique for oxidation-resistant coating of carbon?carbon composite10.1016/S0008-6223(00)00200-1 ↗
21. Deposition of SiC/La2Zr2O7 multi-component coating on C/SiC substrate by combining sol-gel process and slurry10.1016/j.surfcoat.2016.05.079 ↗
22. Mullite-gadolinium silicate environmental barrier coatings for melt infiltrated SiC/SiC composites10.1016/j.surfcoat.2010.12.031 ↗
23. Effect of the green porous texture on porcelain tile properties10.1016/j.jeurceramsoc.2006.07.005 ↗
24. Hot corrosion of sintered alpha-SiC at 1000°C10.1111/j.1151-2916.1985.tb10170.x ↗
25. Kinetics and mechanism of corrosion of SiC by molten salts10.1111/j.1151-2916.1986.tb04698.x ↗
26. Effect of silicon carbide additive on microstructure and properties of porcelain ceramics10.1016/j.ceramint.2011.01.026 ↗
27. Development of lightweight porcelain stoneware tiles using foaming agents10.1016/j.jeurceramsoc.2011.10.028 ↗