Modeling the effect of damage on electrical resistivity of melt-infiltrated SiC/SiC composites
Source abstract
Abstract
Electrical resistivity (ER) measurements are a possible health monitoring technique for CMC components in future aerospace applications. In order to use ER measurements to detect and identify damage, it is necessary to understand how each specific damage state will affect the ER response. In this paper, finite element models are developed and applied to quantify the effect of specific damage states on the electrical resistivity response in a melt-infiltrated silicon carbide (SiC) fiber-reinforced silicon carbide composite. The electrical resistivity of several damage states are calculated by simulating the electric current flow through the damaged micro-structure. This is achieved by performing the numerical solution of the steady-state conservation of charge density equation. Numerical results reveal that cracking of the inter-tow matrix has the most profound effect on the composite electrical resistivity. Also, fiber/matrix debonding at matrix cracks in the 0° tows (tows aligned with the loading direction) may cause a significant increase in the electrical resistivity, but only if the fiber coating resistivity is 1000 Ω-cm or less. Cracks in the 90° tows and the crack opening displacement have very little effect on the composite electrical resistivity.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Smart Materials for Construction · Advanced ceramic materials synthesis · Concrete Corrosion and Durability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (18)
Show source-provided references
1. Monitoring damage accumulation in ceramic matrix composites using electrical resistivity10.1016/j.scriptamat.2008.04.033 ↗
2. Electrical resistance as a nondestructive evaluation technique for SiC/SiC ceramic matrix composites under creep-rupture loading10.1111/j.1744-7402.2010.02587.x ↗
3. Acoustic emission and electrical resistance in SiC-based laminate ceramic composites tested under tensile loading10.1016/j.jeurceramsoc.2017.05.003 ↗
4. COMSOL, Inc · 2016
5. Smith · 2016
6. Microstructural optimization of high temperature SiC/SiC composites
7. Almansour · 2017
8. Accuratus · 2013
9. Ceratec Technical Ceramics BV · 2018
10. Precision Ceramics · 2018
11. Electrical properties of boron nitride thin films grown by neutralized nitrogen ion assisted vapor deposition10.1063/1.116488 ↗
12. Variations in crystalline structures and electrical properties of single crystalline boron nitride nanosheets10.1038/srep16703 ↗
13. Jones · 1975
14. Matrix cracking of cross-ply ceramic composites10.1016/0956-7151(94)90018-3 ↗
15. On the tensile strength of a fiber-reinforced ceramic composite containing a crack-like flaw10.1016/0022-5096(94)90048-5 ↗
16. The mechanics of matrix cracking in brittle-matrix fiber composites10.1016/0001-6160(85)90124-5 ↗
17. Single and multiple fracture. The properties of fiber composites
18. Effects of pull-out on the mechanical properties of ceramic matrix composites10.1016/0001-6160(88)90083-1 ↗