Mechanical characterisation of the protective Al2O3 scale in Cr2AlC MAX phases
Source abstract
Abstract
MAX phases have great potential under demands of both high-temperature and high-stress performance, with their mixed atomic bonding producing the temperature and oxidation resistance of ceramics with the mechanical resilience of metals. Here, we measure the mechanical properties up to 980C by nanoindentation on highly dense and pure Cr$_2$AlC, as well as after oxidation with a burner rig at 1200C for more than 29 hours. Only modest reductions in both hardness and modulus up to 980C were observed, implying no change in deformation mechanism. Furthermore, micro-cantilever fracture tests were carried out at the Cr$_2$AlC/Cr$_7$C$_3$ and Cr$_7$C$_3$/Al$_2$O$_3$ interfaces after the oxidation of the Cr$_2$AlC substrates with said burner rig. The values are typical of ceramic-ceramic interfaces, below 4 MPa/m, leading to the hypothesis that the excellent macroscopic behaviour is due to a combination of low internal strain due to the match in thermal expansion coefficient as well as the convoluted interface.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: MXene and MAX Phase Materials · Aluminum Alloys Composites Properties · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (53)
Show source-provided references
1. Room-temperature ductile carbides10.1007/s11661-999-0325-0 ↗
2. The M(n+1)AX(n) phases: materials science and thin-film processing10.1016/j.tsf.2009.07.184 ↗
3. Barsoum · 2011 · vol. 41
4. Mechanical properties of Cr2AlC ceramics10.1111/j.1551-2916.2007.01634.x ↗
5. Progress in research and development on MAX phases: a family of layered ternary compounds10.1179/1743280410Y.0000000001 ↗
6. A conceptual study into the potential of M(n+1)AX(n)-phase ceramics for self-healing of crack damage10.1016/j.jeurceramsoc.2014.08.046 ↗
7. Oxidation and crack healing behavior of a fine-grained Cr2AlC ceramic10.1111/jace.12170 ↗
8. Layered machinable and electrically conductive Ti2AlC and Ti3AlC2 ceramics: a review10.1016/S1005-0302(10)60064-3 ↗
9. Towards large area deposition of Cr2AlC on steel10.1016/j.tsf.2005.12.219 ↗
10. Comparative investigation of TiAlC(N), TiCrAlC(N), and CrAlC(N) coatings deposited by sputtering of MAX-phase Ti2−xCrxAlC targets10.1016/j.surfcoat.2009.05.036 ↗
11. Synthesis and oxidation testing of MAX phase composites in the Cr-Ti-Al-C quaternary system10.1111/jace.13962 ↗
12. Microstructure and mechanical properties of a Cr2Al(Si)C solid solution10.1016/j.msea.2010.05.093 ↗
13. Crack healing in Y-doped Cr2AlC-MAX phase coatings10.1080/02670844.2016.1201366 ↗
14. Crack healing behaviour of Cr2AlC MAX phase studied by X-ray tomography10.1016/j.jeurceramsoc.2016.07.018 ↗
15. Reducing the erosive wear rate of Cr2AlC MAX phase ceramic by oxidative healing of local impact damage10.1016/j.wear.2016.03.019 ↗
16. Tribological behavior of select MAX phases against Al2O3 at elevated temperatures10.1016/j.wear.2007.11.018 ↗
17. Ambient and 550 °C tribological behavior of select MAX phases against Ni-based superalloys10.1016/j.wear.2007.03.011 ↗
18. Influence of grain size on high temperature oxidation behavior of Cr2AlC ceramics10.1016/j.ceramint.2012.09.039 ↗
19. Effect of Si additions on the Al2O3 grain refinement upon oxidation of Cr2AlC MAX phase10.1016/j.jeurceramsoc.2016.11.050 ↗
20. Part I. Mechanism of oxidation of Cr2AlC films in temperature range 700–1200 degrees C10.1179/1743294414Y.0000000417 ↗
21. Oxide-scale growth on Cr2AlC ceramic and its consequence for self-healing10.1016/j.scriptamat.2013.04.013 ↗
22. Oxidation of Cr2AlC coatings in the temperature range of 1230 to 1410 °C10.1016/j.surfcoat.2011.03.086 ↗
23. A critical review of the oxidation of Ti2AlC, Ti3AlC2 and Cr2AlC in air10.1080/21663831.2013.806364 ↗
24. Environmental resistance of a Ti2AlC-type MAX phase in a high pressure burner rig10.1016/j.jeurceramsoc.2016.07.038 ↗
25. Environmental resistance of Cr2AlC MAX phase under thermal gradient loading using a burner rig10.1111/jace.15425 ↗
26. Thermal cycling testing of TBCs on Cr2AlC MAX phase substrates10.1016/j.surfcoat.2018.02.035 ↗
27. Oxidative durability of TBCs on Ti2AlC MAX phase substrates10.1016/j.surfcoat.2015.11.018 ↗
28. Oxidation of Al2O3 scale-forming MAX phases in turbine environments10.1007/s11661-017-4346-9 ↗
29. On extracting mechanical properties from nanoindentation at temperatures up to 1000 °C10.1016/j.eml.2017.09.007 ↗
30. High temperature microcompression and nanoindentation in vacuum10.1557/jmr.2011.268 ↗
31. Development of high temperature nanoindentation methodology and its application in the nanoindentation of polycrystalline tungsten in vacuum to 950 °C
32. Effect of sintering method on the microstructure of pure Cr2AlC MAX phase ceramics10.2109/jcersj2.15263 ↗
33. Improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
34. Measurement of hardness and elastic modulus by instrumented indentation: advances in understanding and refinements to methodology10.1557/jmr.2004.19.1.3 ↗
35. Measuring fracture toughness of coatings using focused-ion-beam-machined microbeams10.1557/JMR.2005.0048 ↗
36. Sputtering power effects on growth and mechanical properties of Cr2AlC MAX phase coatings10.3390/met6110265 ↗
37. Calculated elastic properties of M2AlC (M = Ti, V, Cr, Nb and Ta)10.1016/j.ssc.2003.12.008 ↗
38. Deposition of chromium-carbon films by magnetron sputtering of chromium and carbon targets10.1142/S0217984905009043 ↗
39. Effects of deposition parameters on the properties of chromium carbide coatings deposited onto steel by sputtering10.1016/S0921-5093(01)01725-7 ↗
40. A comparative study of Cr7C3, Fe3C and Fe2B in cast iron both from ab initio calculations and experiments10.1088/0022-3727/42/11/115415 ↗
41. Hussainova · 2006 · vol. 12
42. Auerkari · 1996 · vol. 23
43. (Nbx, Zr1−x)4AlC3 MAX phase solid solutions: processing, mechanical properties, and density functional theory calculations10.1021/acs.inorgchem.6b00484 ↗
44. Elastic, thermodynamic and optical behavior of V2AC (A = Al, Ga) MAX phases10.1016/j.rinp.2017.09.043 ↗
45. Phase stability, elastic, electronic, thermal and optical properties of Ti3Al1−xSixC2 (0 < = x < = 1): first principle study10.1016/j.physb.2012.07.007 ↗
46. High strain-rate response and deformation mechanisms in polycrystalline Ti2AlC10.1016/j.msea.2014.01.032 ↗
47. Evidence of dislocation cross-slip in MAX phase deformed at high temperature10.1038/srep06358 ↗
48. Mapping of mechanical properties at microstructural length scale in wc-co cemented carbides: assessment of hardness and elastic modulus by means of high speed massive nanoindentation and statistical analysis10.1016/j.ijrmhm.2018.04.019 ↗
49. Effects of crystal orientation on the crack propagation of sapphire by sequential indentation testing
50. Huang · 2011
51. Critical review of the oxidation of Cr2AlC
52. Ceramic materials for thermal barrier coatings10.1016/S0955-2219(03)00129-8 ↗
53. Theoretical study on the mechanism of anisotropic thermal properties of Ti2AlC and Cr2AlC10.1111/jace.12814 ↗